Y10S525/903

Semi-IPN polyurethane/polyurea protective films

Briefly, the present disclosure provides a film, tape or outer layer of a composite part comprising: a) at least one layer comprising a crosslinked polymer selected from the group consisting of crosslinked polyurethane, crosslinked polyurea, and crosslinked mixed polyurethane/polyurea polymer; and in some embodiments b) an adhesive layer. In some embodiments the layer additionally comprises a non-crosslinked polymer forming a semi-IPN with the crosslinked polymer. In some embodiments the non-crosslinked polymer may be selected from the group consisting of polyurethane, polyurea, and mixed polyurethane/polyurea polymer. In some embodiments the crosslinked polymer may additionally comprise an acrylate-containing component.

Extended wear ophthalmic lens

A method for making a silicone hydrogel contact lens is provided. In one embodiment, a prepolymer mixture is polymerized in a lens mold in an atmosphere having less than about 10000 ppm oxygen to form a silicone hydrogel contact lens suitable for extended wear as characterized by producing less than 10% corneal swelling after a period of continuous wear of 7 days including normal sleep periods. In one embodiment, the prepolymer mixture comprises at least one oxyperm material containing hydrophilic groups, wherein the at least one oxyperm material is a siloxane-containing macromer or monomer, at least one ionperm material, and a cross-linking agent. In certain embodiments, the polymerization of the prepolymer mixture may be carried out in an atmosphere having less than about 1000 ppm oxygen.