Y10S73/09

Sampler for hot metal

A sampler for taking samples from a molten metal bath, particularly a molten iron includes a sample chamber assembly having a cover plate and a housing. The housing has first and second openings for an inflow conduit and a gas coupler, respectively. The first face has an analysis zone, a ventilation zone, and a distribution zone. A depth of the analysis zone is 0.5 mm to 1.5 mm. The cover plate and the housing are assembled together to form a sample cavity. The sample chamber assembly chills the molten iron received therein to a solidified white structure metal sample. An analysis surface of the sample lies in a first plane. In a flow direction of the molten iron, there are no increases in width of the sample cavity and a ratio of the length to depth of the sample cavity increases.

Sampler and sampling method for molten material

A sampler has a sample chamber for a sample forming from a molten material, at least one lower cooling body, at least one upper cooling body, at least one inner cooling body, and at least one filling part. The sample chamber is surrounded jointly at least by the lower cooling body and the inner cooling body, such that at least the sample chamber can be cooled by at least the lower and inner cooling bodies. The filling part merges into the sample chamber by a filling opening. Between a region of the outer surface of the inner cooling body and a region of the outer surface of the upper cooling body opposite the outer surface of the inner cooling body, the sampler has at least one gap for conducting at least one gas. The volume of the respective cooling bodies is larger than the volume of the gap.

SAMPLER FOR HOT METAL
20180164195 · 2018-06-14 ·

A sampler for taking samples from a molten metal bath, particularly a molten iron includes a sample chamber assembly having a cover plate and a housing. The housing has first and second openings for an inflow conduit and a gas coupler, respectively. The first face has an analysis zone, a ventilation zone, and a distribution zone. A depth of the analysis zone is 0.5 mm to 1.5 mm. The cover plate and the housing are assembled together to form a sample cavity. The sample chamber assembly chills the molten iron received therein to a solidified white structure metal sample. An analysis surface of the sample lies in a first plane. In a flow direction of the molten iron, there are no increases in width of the sample cavity and a ratio of the length to depth of the sample cavity increases.

Sampler and sampling method for molten material

A sampler has a sample chamber for a sample forming from a molten material, at least one lower cooling body, at least one upper cooling body, at least one inner cooling body, and at least one filling part. The sample chamber is surrounded jointly at least by the lower cooling body and the inner cooling body, such that at least the sample chamber can be cooled by at least the lower and inner cooling bodies. The filling part merges into the sample chamber by a filling opening. Between a region of the outer surface of the inner cooling body and a region of the outer surface of the upper cooling body opposite the outer surface of the inner cooling body, the sampler has at least one gap for conducting at least one gas. The volume of the respective cooling bodies is larger than the volume of the gap.