Y10T428/12986
High strength steel sheet
High strength steel sheet having a tensile strength of 800 MPa or more comprising a middle part in sheet thickness and a soft surface layer arranged at one side or both sides of the middle part in sheet thickness, wherein each soft surface layer has a thickness of more than 10 μm and 30% or less of the sheet thickness, the soft surface layer has an average Vickers hardness of 0.60 time or less the average Vickers hardness of the sheet thickness ½ position, and the soft surface layer has a nano-hardness standard deviation of 0.8 or less is provided.
DAMPING METHOD INCLUDING A FACE-CENTERED CUBIC FERROMAGNETIC DAMPING MATERIAL, AND COMPONENTS HAVING SAME
A method to increase the damping of a substrate using a face-centered cubic ferromagnetic damping material.
Highly luminescent color-selective nanocrystalline materials
A nanocrystal capable of light emission includes a nanoparticle having photoluminescence having quantum yields of greater than 30%.
BMG parts having greater than critical casting thickness and method for making the same
The embodiments described herein relate to BMG articles with high bulk having all dimensions greater than the critical dimension. Exemplary BMG article can include at least one bulk component and/or one or more fixation elements configured on surface of the bulk component or inserted into the bulk component. Other embodiments relate to methods of making the BMG articles by thermo-plastic-formation of BMG alloy materials.
Joint structure
A joint structure includes: a first same-type metal member; a second same-type metal member that can be mutually welded with the first same-type metal member; and a different-type member that has a penetrating portion, is interposed between the first same-type metal member and the second same-type metal member. In the plate thickness direction of an emission region in which a laser beam is emitted toward the penetrating portion, the plate thickness at the emission region of the first same-type metal member positioned on the side on which the laser beam is emitted is a predetermined thickness corresponding to a first gap. The first same-type metal member and the second same-type metal member are fused and bonded together via the penetrating portion, and the different-type member is compressed and fixed, such that the different-type member is fixed to the first same-type metal member and the second same-type metal member.
Slide member, bicycle component using slide member, and fishing tackle component using slide member
A slide member is provided with a base material, a plated slide layer and an intermediate plated layer. The plated slide layer contains a solid lubricant. The intermediate plated layer is disposed between the base material and the plated slide layer, the intermediate plated layer increasing cohesion of the base material and the plated slide layer. The plated slide layer has a content of the solid lubricant in a range from 30 to 70 vol %, inclusive.
ENVIRONMENTAL BARRIER COATING
An article includes a substrate and a barrier layer on the substrate. The barrier layer includes a matrix, diffusive particles dispersed in the matrix, and gettering particles dispersed in the matrix. The gettering particles include at least one alloyed metal silicide. A composite material and a method of fabricating an article are also disclosed.
Steel sheet and method of manufacturing same
Steel sheet for cans high in strength and excellent in formability and appearance comprising C: 0.0010 to 0.0035%, Si: 0.050% or less, Mn: 0.10 to 0.50%, P: 0.040% or less, S: 0.040% or less, Al: less than 0.005%, N: 0.0050% or less and a balance of Fe and unavoidable impurities, wherein an average value of a ratio of length of crystal grains in a sheet thickness direction to length in a sheet width direction is 0.70 or more, a yield strength is 500 MPa or more, and, in a range of 0 to 90° of the rolling direction, a minimum value of an r-value is 1.50 or more, an average value of the r-value is 1.70 or more, and a difference of the maximum value and minimum value of the r-value is 0.50 or less.
JOINT STRUCTURE
A joint structure includes: a first same-type metal member; a second same-type metal member that can be mutually welded with the first same-type metal member; and a different-type member that has a penetrating portion, is interposed between the first same-type metal member and the second same-type metal member. In the plate thickness direction of an emission region in which a laser beam is emitted toward the penetrating portion, the plate thickness at the emission region of the first same-type metal member positioned on the side on which the laser beam is emitted is a predetermined thickness corresponding to a first gap. The first same-type metal member and the second same-type metal member are fused and bonded together via the penetrating portion, and the different-type member is compressed and fixed, such that the different-type member is fixed to the first same-type metal member and the second same-type metal member.
HIGH STRENGTH STEEL SHEET
High strength steel sheet having a tensile strength of 800 MPa or more comprising a middle part in sheet thickness and a soft surface layer arranged at one side or both sides of the middle part in sheet thickness, wherein each soft surface layer has a thickness of more than 10 m and 30% or less of the sheet thickness, the soft surface layer has an average Vickers hardness of 0.60 time or less the average Vickers hardness of the sheet thickness position, and the soft surface layer has a nano-hardness standard deviation of 0.8 or less is provided.