WATERPROOF CORRUGATED PAPER
20220204708 · 2022-06-30
Assignee
Inventors
Cpc classification
B32B2264/303
PERFORMING OPERATIONS; TRANSPORTING
B32B3/28
PERFORMING OPERATIONS; TRANSPORTING
B32B27/18
PERFORMING OPERATIONS; TRANSPORTING
C08K11/00
CHEMISTRY; METALLURGY
D21H27/40
TEXTILES; PAPER
B32B2255/10
PERFORMING OPERATIONS; TRANSPORTING
B32B7/14
PERFORMING OPERATIONS; TRANSPORTING
B32B2250/242
PERFORMING OPERATIONS; TRANSPORTING
C08K2201/005
CHEMISTRY; METALLURGY
B32B7/12
PERFORMING OPERATIONS; TRANSPORTING
B32B27/20
PERFORMING OPERATIONS; TRANSPORTING
B32B2264/104
PERFORMING OPERATIONS; TRANSPORTING
B32B2264/12
PERFORMING OPERATIONS; TRANSPORTING
International classification
C08J5/12
CHEMISTRY; METALLURGY
B32B27/20
PERFORMING OPERATIONS; TRANSPORTING
B32B3/28
PERFORMING OPERATIONS; TRANSPORTING
B32B7/14
PERFORMING OPERATIONS; TRANSPORTING
Abstract
A waterproof corrugated paper includes a stone paper medium, a stone glue, and at least two stone liner papers. The stone paper medium includes a first fluting surface and a second fluting surface. The stone glue is applied to wave crests of the first fluting surface and wave crests of the second fluting surface. The at least two stone liner papers are respectively attached to the first fluting surface and the second fluting surface by the stone glue applied to the wave crests of the first and second fluting surfaces, thereby allowing the stone paper medium to be located between the at least two stone liner papers. The stone paper medium, the stone glue, and the stone liner papers includes a linear polyolefin plastic material and an inorganic material. The waterproof corrugated paper provided by the present invention is waterproof and frost-resistant, which is adapted to package cooled or frozen food.
Claims
1. A waterproof corrugated paper, comprising: a stone paper medium which is fluted shaped, wherein the stone paper medium has a first fluting surface and a second fluting surface which face opposite directions; the stone paper medium has a thickness is in a range of 0.10 mm-0.25 mm, the wave height is in a range of 0.6 mm-6.0 mm; a stone glue merely applied to a plurality of wave crests of the first fluting surface and a plurality of wave crests of the second fluting surface; and at least two stone liner papers which are respectively attached to the first fluting surface and the second fluting surface with the stone glue on the plurality of wave crests of the first fluting surface and on the plurality of wave crests of the second fluting surface, so that the stone paper medium is located between the at least two stone liner papers; wherein the stone paper medium, the stone glue, and the at least two stone liner papers comprise a linear polyolefin plastic material and an inorganic material; wherein the stone glue comprises the linear polyolefin plastic material accounts for 30 wt %-70 wt % of a weight of the stone glue, and the inorganic material accounts for 30 wt %-70 wt % of the weight of the stone glue; the stone paper medium comprises the linear polyolefin plastic material accounts for 15 wt %-40 wt % of a weight of the stone paper medium, and the inorganic material accounts for 60 wt %-85 wt % of the weight of the stone paper medium; each of the at least two stone liner papers comprises the linear polyolefin plastic material accounts for 15 wt %-40 wt % of a weight of the stone liner paper, and the inorganic material accounts for 60 wt %-85 wt % of the weight of the stone liner paper.
2. The waterproof corrugated paper as claimed in claim 1, a horizontal distance on the stone paper medium is defined as a distance between one of a plurality wave crests and one of a plurality of troughs which is adjacent to the one of the plurality of wave crests of the stone paper medium; the stone paper medium has a flute number (Fno) which is defined by an unit distance divided by the horizontal distance; the unit distance is 30 cm; the horizontal distance is between 1.0 mm and 5.0 mm; the flute number (Fno) is between 60 and 300; a ratio of the wave height to the horizontal distance is in a range from 0.9 to 1.8.
3. The waterproof corrugated paper as claimed in claim 1, wherein a number of the stone paper medium is two, and a number of the at least two stone liner papers is three; each of the two stone paper mediums is located between two of the three stone liner papers; the plurality of wave crests of the first fluting surface of each of the two stone paper mediums is attached to one of the three stone liner papers with the stone glue, and the plurality of wave crests of the second fluting surface is attached to another one of the three stone liner papers with the stone glue.
4. The waterproof corrugated paper as claimed in claim 1, wherein the linear polyolefin plastic material comprises a polyolefin composition.
5. The waterproof corrugated paper as claimed in claim 4, wherein the polyolefin composition comprises a crystalline material; the crystalline material is selected from a group consisting of polyethylene (PE), high density polyethylene (HDPE), metallocene linear low density polyethylene (MLLDPE), and a combination thereof.
6. The waterproof corrugated paper as claimed in claim 1, wherein the stone glue comprises the linear polyolefin plastic material accounts for 30 wt %-50 wt % of a weight of the stone glue, and the inorganic material accounts for 50 wt %-70 wt % of the weight of the stone glue.
7. The waterproof corrugated paper as claimed in claim 1, wherein the inorganic material is an inorganic powder with a grain size of 2-10 micrometers (μm).
8. The waterproof corrugated paper as claimed in claim 1, wherein the stone paper medium further comprises an additive, and the additive accounts for smaller than 2 wt % of the weight of the stone paper medium.
9. The waterproof corrugated paper as claimed in claim 8, wherein the additive is selected from a group consisting of a processing additive, a slip agent, a toughening agent, or a combination thereof.
10. The waterproof corrugated paper as claimed in claim 1, wherein the at least two stone liner paper further comprises an additive, and the additive accounts for smaller than 2 wt % of the weight of the stone liner paper.
11. The waterproof corrugated paper as claimed in claim 10, wherein the additive is selected from a group consisting of a processing additive, a slip agent, a toughening agent, or a combination thereof.
Description
BRIEF DESCRIPTION OF THE SEVERAL VIEWS OF THE DRAWINGS
[0011] The present invention will be best understood by referring to the following detailed description of some illustrative embodiments in conjunction with the accompanying drawings, in which
[0012]
[0013]
[0014]
[0015]
[0016]
[0017]
DETAILED DESCRIPTION OF THE INVENTION
[0018] Referring to
[0019] The stone glue includes a linear polyolefin plastic material and an inorganic material, wherein the linear polyolefin plastic material is 30 wt %-70 wt % based on the stone glue, and the inorganic material is 30 wt %-70 wt % based on the stone glue. In the first embodiment, the linear polyolefin plastic material is preferably 30 wt %-50 wt % based on the stone glue, and the inorganic material is preferably 50 wt %-70 wt % based on the stone glue. In the current embodiment, a sum of weight percentages of the linear polyolefin plastic material and the inorganic material is equal to 100 wt % of the stone glue.
[0020] In the first embodiment, the linear polyolefin plastic material includes a polyolefin composition which includes a crystalline material, wherein the crystalline material includes polyethylene (PE), high density polyethylene (HDPE), metallocene linear low density polyethylene (MLLDPE), or a combination thereof. In the first embodiment, the inorganic material could be white or other inorganic materials without heavy metal, wherein the inorganic material is an inorganic powder made by grinding a natural stone, and a main ingredient of the inorganic material is calcium carbonate (CaCO.sub.3), calcium oxide (CaO), calcium hydroxide Ca(OH).sub.2, silicon dioxide (SiO.sub.2), or a combination thereof at micron-level. The inorganic material is the inorganic powder with a grain size of 2-10 micrometers (μm).
[0021] In the first embodiment, the stone paper medium 12 and the stone liner paper 14 are respectively one material layer, wherein the plurality of material layers includes the inorganic material, the linear polyolefin plastic material, and an additive, which are mixed and pressurized together. In the current embodiment, the inorganic material accounts for 60 wt %-85 wt % of a weight of each of the material layers; the linear polyolefin plastic material accounts for 15 wt %-40 wt % of the weight of each of the material layers; the additive could be additionally added on the required demand. When the additive is needed, the additive accounts for smaller than 2 wt % of the weight of each of the material layers. In the current embodiment, a sum of weight percentages of the inorganic material, the linear polyolefin plastic material, and the additive is equal to 100 wt % of each of the material layers. In the current embodiment, the inorganic material could be, but not limited to, calcium carbonate (CaCO.sub.3), calcium oxide (CaO), calcium hydroxide Ca(OH).sub.2, silicon dioxide (SiO.sub.2), or a combination thereof; the linear polyolefin plastic material could be, but not limited to, high density polyethylene (HDPE); the additive could be, but not limited to, a processing additive, a slip agent, a toughening agent, or a combination thereof, wherein the slip agent could be, but not limited to, zinc stearate, magnesium stearate, or a combination thereof.
[0022] It's worthy to mention that, in practice, the stone paper medium 12 and the stone liner paper 14 could respectively be “Disposable (Degradable) Environmental-friendly Paper with Five Layers” claimed in Taiwan invention patent No. 1535913 of TAIWAN LUNG MENG ADVANCED COMPOSITE MATERIALS CO., LTD. and “Environmental-friendly Paper manufactured by manufacturing method thereof” claimed in Taiwan invention patent No. 379272 of TAIWAN LUNG MENG ADVANCED COMPOSITE MATERIALS CO., LTD.
[0023] Referring to
[0024] The waterproof corrugated paper 1B of the second embodiment includes a layer of the stone paper medium 12 and two layers of the stone liner paper 14, wherein the stone paper medium 12 has the first fluting surface 121 and a second fluting surface 123 which face opposite directions. One of the two layers of the stone liner papers 14 is attached to the wave crests 122 of the first fluting surface 121 by using the stone glue (not shown), and the other one of the layers of the stone liner papers 14 is attached to a plurality of wave crests 124 of the second fluting surface 123 by using the stone glue (not shown), thereby to form the waterproof corrugated paper 1B which is a single wall type.
[0025] In
[0026] It's worthy to mention that a horizontal distance don the stone paper medium 12 is defined between one of the wave crests (i.e. the wave crests 124 of the second fluting surface 123) and one of a plurality of troughs (i.e. one of the wave crests 122 of the first fluting surface 121) which is adjacent to the one of the wave crests. The stone paper medium 12 has a flute number (Fno) which is defined by an unit distance divided by the horizontal distance d. In the second embodiment, the unit distance is 30 cm; the horizontal distance d is between 1.0 mm and 5.0 mm; the flute number (Fno) is between 60 and 300. A ratio (H/d) of the wave height H to the horizontal distance d is in a range from 0.9 to 1.8. Generally, the smaller the flute number (Fno) is, the smaller the average compressive strength (FCR value) of the waterproof corrugated paper 1B is; the greater the flute number (Fno) is, the greater the average compressive strength (FCR value) of the waterproof corrugated paper 1B is. However, in the second embodiment, when the flute number (Fno) is smaller than 60, the flute number (Fno) of the stone paper medium 12 is not enough to provide sufficient strength of the structural support, so that the average compressive strength (FCR value) of the waterproof corrugated paper 1B is too small to use. When the flute number (Fno) is larger than 120, the average compressive strength (FCR value) of the waterproof corrugated paper 1B becomes greater, but the flute number (Fno) of the stone paper medium 12 is too great that the density of the waterproof corrugated paper 1B is too great, which doesn't have practically applied value but increase the cost of material and manufacture. On the other hand, the greater the ratio (H/d) of the wave height H to the horizontal distance d is, the smaller the average compressive strength (FCR value) of the stone paper medium 12; the smaller the ratio (H/d) of the wave height H to the horizontal distance d is, the greater the average compressive strength (FCR value) of the stone paper medium 12 is. However, in the second embodiment, when the ratio (H/d) of the wave height H to the horizontal distance d is larger than 1.8, the flute number (Fno) of the stone paper medium 12 is not enough to provide sufficient strength of the structural support, so that the average compressive strength (FCR value) of the waterproof corrugated paper 1B is too small to use. When the ratio (H/d) of the wave height H to the horizontal distance d is smaller than 0.9, the average compressive strength (FCR value) of the waterproof corrugated paper 1B becomes greater, but the flute number (Fno) of the stone paper medium 12 is too great that the density of the waterproof corrugated paper 1B is too great, which doesn't have practically applied value but increase the cost of material and manufacture.
[0027] Additionally, the average compressive strength (FCR value) of the waterproof corrugated paper 1B is directly proportional to a thickness of each of the two stone liner papers 14. If the thickness of each of the two stone liner papers 14 is larger, the average compressive strength (FCR value) of the waterproof corrugated paper 1B is greater. On the contrary, if the thickness of each of the two stone liner papers 14 is smaller, the average compressive strength (FCR value) of the waterproof corrugated paper 1B is smaller.
[0028] The average compressive strength (FCR value) of the waterproof corrugated paper 1B is directly proportional to a hardness of the stone paper medium 12. In other words, the harder the stone paper medium 12 is, the greater the average compressive strength (FCR value) of the waterproof corrugated paper 1B is. On the contrary, the softer the stone paper medium 12 is, the smaller the average compressive strength (FCR value) of the waterproof corrugated paper 1B is. The hardness of the stone paper medium 12 is related to the composition of the stone paper medium 12, wherein if a proportion of the inorganic material of the stone paper medium 12 is greater, the stone paper medium 12 is softer. If the proportion of the inorganic material of the stone paper medium 12 is smaller, the stone paper medium 12 is harder. For example, a hardness of the stone paper medium 12 with 80 w/w % of the inorganic material is smaller than that of the stone paper medium 12 with 50 w/w % of the inorganic material. Besides, the hardness of the stone paper medium 12 is related to the thickness t of the stone paper medium 12. The larger the thickness t of the stone paper medium 12 is, the harder the stone paper medium 12 is; the smaller the thickness t of the stone paper medium 12 is, the softer the stone paper medium 12 is. In an embodiment, the stone paper medium 12 with desired thickness t could be produced by adjusting the proportion of the inorganic material in the stone paper medium 12, thereby to obtain an average compressive strength (FCR value) which is preferable.
[0029] Referring to
[0030] The waterproof corrugated paper 1C of the third embodiment includes two layers of the stone paper medium 12 and three layers of the stone liner papers 14, wherein the two stone paper mediums 12 are respectively arranged between two of the three stone liner papers 14. The plurality of wave crests 122 of the first fluting surface 121 of each of the two stone paper mediums 12 are attached to one of the three stone liner papers 14 by using the stone glue, and the plurality of wave crests 124 of the second fluting surface 123 of each of the two stone paper mediums 12 are attached to another one of the three stone liner papers 14 by using the stone glue.
[0031] Referring to
[0032] The manufacturing method of the waterproof corrugated paper 1A includes at least following steps: [0033] Step S01: the stone paper medium 12 is provided; [0034] Step S02: the corrugated synchronized roller 26 is utilized to make the stone paper medium 12 wave-shaped and to have the first fluting surface 121; [0035] Step S03: the stone glue 16 is provided, wherein the stone glue 16 includes the linear polyolefin plastic material and the inorganic material; [0036] Step S04: a glue roll set 28 is utilized to apply the stone glue 16 to the plurality of wave crests 122 of the first fluting surface 121 of the stone paper medium 12; [0037] Step S05: the stone liner paper 14 is attached to the plurality of wave crests 122 of the first fluting surface 121 of the stone paper medium 12.
[0038] In the current embodiment, the stone glue 16 includes the linear polyolefin plastic material and the inorganic material, wherein the linear polyolefin plastic material is 30 wt %-70 wt % based on the stone glue, and the inorganic material is 30 wt %-70 wt % based on the stone glue. In the current embodiment, the plastic is preferably 30 wt %-50 wt % based on the stone glue, and the inorganic material is preferably 50 wt %-70 wt % based on the stone glue. In the current embodiment, a sum of weight percentages of the linear polyolefin plastic material and the inorganic material is equal to 100 wt % of the stone glue.
[0039] In
[0040] In the first embodiment, the stone paper medium 12 and the stone liner paper 14 are respectively one material layer, wherein the material layers include the inorganic material, the linear polyolefin plastic material, and the additive, which are mixed and pressurized together. In the current embodiment, the inorganic material accounts for 60 wt %-85 wt % of a weight of each of the material layers; the linear polyolefin plastic material accounts for 15 wt %-40 wt % of the weight of each of the material layers; the additive could be additionally added on the required demand. When the additive is needed, the additive accounts for smaller than 2 wt % of the weight of each of the material layers. In the current embodiment, the sum of weight percentages of the inorganic material, the linear polyolefin plastic material, and the additive is equal to 100 wt % of each of the material layers. In the current embodiment, the inorganic material could be, but not limited to, calcium carbonate (CaCO.sub.3), calcium oxide (CaO), calcium hydroxide Ca(OH).sub.2, silicon dioxide (SiO.sub.2), or a combination thereof; the linear polyolefin plastic material could be, but not limited to, high density polyethylene (HDPE); the additive could be, but not limited to, a processing additive, a slip agent, a toughening agent, or a combination thereof, wherein the slip agent could be, but not limited to, zinc stearate, magnesium stearate, or a combination thereof.
[0041] It's worthy to mention that, in practice, the stone paper medium 12 and the stone liner paper 14 could respectively be “Disposable (Degradable) Environmental-friendly Paper with Five Layers” claimed in Taiwan invention patent No. 1535913 of TAIWAN LUNG MENG ADVANCED COMPOSITE MATERIALS CO., LTD. and “Environmental-friendly Paper manufactured by manufacturing method thereof” claimed in Taiwan invention patent No. 379272 of TAIWAN LUNG MENG ADVANCED COMPOSITE MATERIALS CO., LTD.
[0042] In the
[0043] Referring to
[0044] In
[0045] When the first roller 282, the second roller 284, the third roller 286, the first gear 262, and the second gear 264 rotate, the stone glue 16 is transmitted through the first roller 282, the second roller 284, and the third roller 286 to the second gear 264 of the corrugated synchronized roller 26 to make the plurality of wave crests 122 of the stone paper medium 12 be applied with the stone glue 16.
[0046] The second gear 264 of the corrugated synchronized roller 26 is adjacent to the pinch roller 20, and both of the stone paper medium 12 in corrugated shape and the stone liner paper 14 pass between the corrugated synchronized roller 26 and the pinch roller 20 at the same time. In the current embodiment, the stone paper medium 12 applied with the stone glue 16 could be tightly adhered to the stone liner paper 14 by the pinch roller 20. In the current embodiment, a minimum distance between the pinch roller 20 and the second gear 264 is smaller than or equal to a total thickness of the waterproof corrugated paper which is a sum of the wave height H of the stone paper medium 12 and a thickness of the stone liner paper 14. In the current embodiment, the total thickness of the waterproof corrugated paper is between 0.6 mm and 6.0 mm.
[0047] In the current embodiment, the waterproof corrugated paper 1A of the first embodiment, the waterproof corrugated paper 1B of the second embodiment, and the waterproof corrugated paper 1C of the third embodiment are adapted to package seafood, vegetables, and fruits, but not limited thereto. The waterproof corrugated papers 1A, 1B, 1C provided by the embodiments according to the present invention could be applied to package any kind of stuff. The waterproof corrugated papers 1A, 1B, 1C provided by the embodiments could be used to package the frozen seafood and meat or to package the vegetables and fruits which are cooled down by spraying 5-13 degrees Celsius water. For example, the waterproof corrugated papers 1A, 1B, 1C could be further processed to produce waterproof corrugated paper boxes, waterproof corrugated paper bags, or waterproof corrugated paper rings to be used as a packaging material.
[0048] With the aforementioned design, the main ingredient of the waterproof corrugated paper includes the inorganic powder made by grinding natural stone and a little of linear polyolefin plastic material for binding, so that it could completely avoid using wood pulp. Besides, comparing to the conventional corrugated paper made of the wood pulp paper, the waterproof corrugated paper provided by the present invention has significantly waterproof and frost resistant ability. Even if the waterproof corrugated paper is frozen and unfrozen repeatedly, the waterproof corrugated paper could maintain a good strength and still could be easily transported without being broken. Therefore, the waterproof corrugated paper provided by the present invention could be applied to package the products which need to be cooled or be frozen, such as vegetables, fruits, fish, meat, and so on. The waterproof corrugated paper provided by the present invention could tolerate a low temperature lower than or equal to minus 40 degrees Celsius. Additionally, the waterproof corrugated paper doesn't absorb water(moisture), and the characteristic of the Calcium Carbonate (CaCO.sub.3) could avoid the growth of mold or bacteria, so that the waterproof corrugated paper ensures the hygiene of the packaged food without adding an additional antibacterial and antifungal agent. Furthermore, since the additional antibacterial and antifungal agent doesn't need to be added, there is no food safety issue. When the package contains the containers having liquid (e.g. water, drinks or condiments), once the liquid leaks out, the conventional corrugated paper made of wood pulp paper absorbs the liquid easily, causing the corrugated paper broken, so that the containers in the package is possibly dropped from the package; even the corrugated paper made of the wood pulp papers located under the leaky container could be broken due to absorbing liquid. At this time, the mold and bacteria could easily grow on the corrugated paper made of the wood pulp papers which absorbs water. In contrast to the conventional corrugated paper made of the wood pulp papers, the waterproof corrugated paper provided by the present invention would not be broken due to absorbing water, so that the packaged containers would not drop, thereby to protect the completeness of other container having liquid and to keep the waterproof corrugated paper boxes being stacked in a good state. Besides, the waterproof corrugated paper provided by the present invention doesn't absorb water, so that the mold or bacteria couldn't grow on the waterproof corrugated paper. Additionally, no matter the inorganic material is one of calcium carbonate (CaCO.sub.3), calcium oxide (CaO), calcium hydroxide Ca(OH).sub.2, silicon dioxide (SiO.sub.2), or a combination thereof, the ability of waterproof and the oil resistance of the waterproof paper could be enhanced.
[0049] Moreover, the waterproof corrugated paper provided by the present invention could be recycled after undergoing a simple sanitizing process, thereby to reach a goal of reducing waste. It is worthy to mention that comparing to the conventional corrugated paper made of the wood pulp papers, the waterproof corrugated paper provided by the present invention could significantly reduce the production cost, so that the usage of the conventional corrugated box made of the wood pulp papers could be reduced, thereby to reduce deforestation. Additionally, the waterproof corrugated paper provided by the present invention is made from natural stone powder, which is easily be decomposed in the natural environment. Therefore, a goal of environmental sustainability and environmental protection could be achieved.
[0050] It must be pointed out that the embodiment described above is only a preferred embodiment of the present invention. All equivalent structures and methods which employ the concepts disclosed in this specification and the appended claims should fall within the scope of the present invention.