TWO-COMPONENT AEROSOL CAN
20200399051 · 2020-12-24
Assignee
Inventors
Cpc classification
C08G18/7671
CHEMISTRY; METALLURGY
C08J2203/12
CHEMISTRY; METALLURGY
C08J2203/142
CHEMISTRY; METALLURGY
C08G18/10
CHEMISTRY; METALLURGY
B65D83/66
PERFORMING OPERATIONS; TRANSPORTING
C08J9/142
CHEMISTRY; METALLURGY
B65D83/687
PERFORMING OPERATIONS; TRANSPORTING
C08G2190/00
CHEMISTRY; METALLURGY
B65D83/752
PERFORMING OPERATIONS; TRANSPORTING
C08J2203/14
CHEMISTRY; METALLURGY
C08G18/10
CHEMISTRY; METALLURGY
International classification
Abstract
A two-component aerosol can for dispensing sealing and assembly foams based on isocyanates, having an outer pressure container which holds a prepolymer component and a propellant gas, the outer pressure container being in communication with a first valve device and with a first channel; an inner container which holds a curing component and a propellant gas, the inner container being in communication with a second valve device and with a second channel; and a spray head which comprises a device for simultaneously actuating the first and second valve devices; and a spray tube into which the first and second channels jointly open
Claims
1. A two-component aerosol can for dispensing sealing and assembly foams based on isocyanates, having an outer pressure container which holds a prepolymer component and a propellant gas, the outer pressure container being in communication with a first valve device and with a first channel, an inner container which holds a curing component and a propellant gas, the inner container being in communication with a second valve device and with a second channel, and a spray head which comprises a device for simultaneously actuating the first and second valve devices, and also a spray tube into which the first and second channels jointly open, wherein the second valve device or the second channel comprises a throttle element which tailors the dispensing rate of the curing component to that of the prepolymer component, the curing component being not sufficient to satisfy the isocyanate groups of the prepolymer component, such that in the mixture of prepolymer component and curing component dispensed there is an isocyanate excess of more than 3 wt %, based on the weight of the mixture.
2. The aerosol can as claimed in claim 1, wherein the throttle element is integrated in the second channel.
3. The aerosol can as claimed in claim 1, wherein the excess of isocyanate groups is 5 to 13 wt %.
4. The aerosol can as claimed in claim 3, wherein the isocyanate excess in the mixture is 8 to 12 wt %.
5. The aerosol can as claimed in claim 1, wherein the outer pressure container and the inner container hold the same propellant gas.
6. The aerosol can as claimed in claim 5, wherein the propellant gas is 1,1-difluoroethane (R152a), tetrafluoroethane (R134a), propane, butane, dimethyl ether, or a mixture of at least two of these propellant gases.
7. The aerosol can as claimed in claim 1, wherein the spray head comprises a forced mixer.
8. The aerosol can as claimed in claim 7, wherein the spray tube is designed as a forced mixer.
9. A method for pressure-resistance sealing using a two-component aerosol can for dispensing sealing and assembly foams based on isocyanates, the method comprising: providing an aerosol can comprising: an outer pressure container which holds a prepolymer component and a propellant gas, the outer pressure container being in communication with a first valve device and with a first channel, an inner container which holds a curing component and a propellant gas, the inner container being in communication with a second valve device and with a second channel, and a spray head which comprises a device for simultaneously actuating the first and second valve devices, and also a spray tube into which the first and second channels jointly open, wherein the second valve device or the second channel comprises a throttle element which tailors the dispensing rate of the curing component to that of the prepolymer component, the curing component being not sufficient to satisfy the isocyanate groups of the prepolymer component, such that in the mixture of prepolymer component and curing component dispensed there is an isocyanate excess of more than 3 wt %, based on the weight of the mixture, and using the aerosol can to perform pressure-resistant sealing of joints and openings with sealing foam against passage of water.
10. A method for pressure-resistance sealing as claimed in claim 9, wherein the joints and openings withstand an overpressure of at least 1.5 bar.
11. A method for pressure-resistance sealing as claimed in claim 9, wherein the sealing performed on empty pipes for cable laying.
12. A method for pressure-resistance sealing as claimed in claim 9, wherein the sealing is performed on pipes against ingress or egress of water.
Description
[0012] By isocyanate excess is meant the weight fraction of the isocyanate group as a proportion of the weight of the mixture dispensed.
[0013] The prepolymers employed in the aerosol can of the invention are those with a customary basis, as are prepared, for example, from MDI (diphenylmethane diisocyanate) and polyether polyol. Important in this case is the excess of free NCO groups, which is for example in the range from 15 to 20 wt %, based on the prepolymer. The prepolymer is held in the outer pressure container of the aerosol can and is admixed with propellant gas, as for example with 1,1-difluoroethane (R152a), 1,1,2,2-tetrafluoroethane (R134a), propane, butane or dimethyl ether. It is also possible to use propellant gas mixtures, for instance propane/butane/dimethyl ether, optionally with addition of R152a and/or R134a. The outer pressure container, furthermore, may hold customary adjuvants, examples being foam stabilizers, flame retardants, catalysts, and the like.
[0014] The curing component is located in the inner container and comprises a polyol, as for instance glycol or diethylene glycol. Additionally present is a customary catalyst which brings about crosslinking with the prepolymer, and also propellant gas. It may be useful to add a dye to the curing component, which in the dispensed product indicates the activation of the inner container.
[0015] The inner container preferably holds the same propellant gas as the outer pressure container and, accordingly, has the same pressure. Where the inner container consists of a polyolefin, as is preferred, there is also automatically an exchange of propellant gas and a pressure compensation through the wall.
[0016] The outer pressure container is in communication via a first valve with the first channel in the spray head of the aerosol can, and the first channel opens into a spray tube.
[0017] The inner container is in communication via a separate second valve with the second channel in the spray head of the aerosol can. The two valves here are located in a valve plate which is gastightly arranged in the dome of the can. The inner container here is gastightly mounted on the underside of the valve plate, below the second valve. Reference is made, by way of example, to EP 0 111 089. The arrangement of both valves in the valve plate permits simultaneous triggering.
[0018] The spray head at the same time contains a device for simultaneous actuation of the two valves. For this purpose the spray head is mounted in a vertically movable way on the valve plate and is able to press the valves in for triggering, with the aid of the channels which are arranged in the valve head and which engage around the upper edge of the stent of each valve. The two channels open into a spray tube, in which the two components are combined. The valves, in a known way, have a vertically movable stem which when pressed opens up the valve passage.
[0019] For reasons of cost and in order to enable uniform opening, the first and second valves are identical in design. However, since the dispensing rate for the curing component must be lower than that of the prepolymer componentthe quantitative ratio of prepolymer component to curing component is in the range from 15:1 up to 5:1 and more particularly is about 10:1there is a throttle element located in the dispensing pathway of the curing component, advantageously in the second channel. The throttle function may be served, for example, by a smaller cross section of the second channel, a narrowing in the second channel, a pin which partially closes the exit in the second valve, or else a longer passage of the second channel in comparison to the first channel. In that case the two components are only mixed in the spray tube, which, for the purpose of producing a homogeneous mixture, may be equipped with a forced mixing element, for instance a static mixer. Forced mixers suitable for this purpose are known per se. Adequate mixing, however, may also be achieved without forced mixers.
[0020] A residual content of isocyanate in the dispensed mixture is essential to the invention. This residual content ought to be more than 3 wt %, based on the mixture including propellant gas, and more particularly 5 to 13 wt %. An isocyanate excess of 10 to 12 wt % is preferred.
[0021] The effect of the excess of free isocyanate in the mixture dispensed, under the influence of moisture, more particularly of atmospheric moisture, is a post-expansion of the foam, causing it to conform particularly well to the walls in joints and openings. In the case of reactive surfaces, there is reactive attachment of the sealing foam. In the case of smooth surfaces not offering any good hold, the use of a primer may be useful. For this reason, the sealing and assembly foam generated in the invention can be employed particularly well for the sealings of joints and openings. Watertight closures are developed, with a pressure resistance of more than 1.5 bar.
[0022] The foam may be deployed, for example, for the water-resistant sealing of pipes (especially disused pipes in buildings), of leadthroughs, shaft rings, well caps, and also door and window connection joints. One preferred application is the closure of empty pipes which are installed and laid (in newbuilds, for example) for the purpose of converting cable looms and the like.
[0023] In the testing method, pipe closures with sealing foams dispensed in accordance with the invention were tested at 1.5 bar. The closures proved to be airtight and watertight for much more than 120 hours.