Methods for temporarily bonding a device wafer to a carrier wafer, and related assemblies
09716023 ยท 2017-07-25
Assignee
Inventors
Cpc classification
B32B2405/00
PERFORMING OPERATIONS; TRANSPORTING
B32B5/142
PERFORMING OPERATIONS; TRANSPORTING
B32B37/1292
PERFORMING OPERATIONS; TRANSPORTING
H01L2221/6834
ELECTRICITY
H01L2221/68318
ELECTRICITY
B32B7/12
PERFORMING OPERATIONS; TRANSPORTING
H01L2221/68381
ELECTRICITY
International classification
B32B37/00
PERFORMING OPERATIONS; TRANSPORTING
B32B37/12
PERFORMING OPERATIONS; TRANSPORTING
C09J5/04
CHEMISTRY; METALLURGY
B29C65/00
PERFORMING OPERATIONS; TRANSPORTING
B32B5/14
PERFORMING OPERATIONS; TRANSPORTING
B32B7/14
PERFORMING OPERATIONS; TRANSPORTING
H01L21/46
ELECTRICITY
H01L21/30
ELECTRICITY
Abstract
A method of bonding a device wafer to a carrier wafer includes disposing a first adhesive over a central portion of a carrier wafer, the first adhesive having a first glass transition temperature, disposing a second adhesive over a peripheral portion of the carrier wafer, the second adhesive having a second glass transition temperature greater than the first glass transition temperature, and bonding the first adhesive to an active front side of the device wafer and the second adhesive to a peripheral portion of the front side of the device wafer. Related assemblies may be used in such methods.
Claims
1. A method of bonding a device wafer to a carrier wafer, comprising: disposing a first thermoplastic adhesive having a first glass transition temperature of less than or equal to about 200 C. over a central portion of a carrier wafer; disposing a second thermoplastic adhesive having a second glass transition temperature of at least about fifteen degrees Celsius (15 C.) greater and less than about twenty-five degrees Celsius (25 C.) greater than the first glass transition temperature over a peripheral portion of the carrier wafer; and bonding the first thermoplastic adhesive to at least a portion of a front side of a device wafer and the second thermoplastic adhesive to a peripheral portion of the front side of the device wafer.
2. The method of claim 1, wherein disposing the first thermoplastic adhesive over the central portion of the carrier wafer comprises disposing the first thermoplastic adhesive over substantially the entire surface of the carrier wafer and at least partially removing the first thermoplastic adhesive from the peripheral portion of the carrier wafer.
3. The method of claim 2, wherein at least partially removing the first thermoplastic adhesive from the peripheral portion of the carrier wafer comprises removing the first thermoplastic adhesive from an area extending from a periphery of the carrier wafer up to about twenty (20) mm radially inward.
4. The method of claim 2, wherein at least partially removing the first thermoplastic adhesive from the peripheral portion of the carrier wafer comprises applying a solvent to the first thermoplastic adhesive disposed over the peripheral portion of the carrier wafer.
5. The method of claim 2, wherein disposing the second thermoplastic adhesive over the peripheral portion of the carrier wafer comprises disposing the second thermoplastic adhesive over the area of the peripheral portion of the carrier wafer from which the first thermoplastic adhesive is removed.
6. The method of claim 5, further comprising removing an outer peripheral portion of the second thermoplastic adhesive with a solvent.
7. The method of claim 1, wherein disposing the first thermoplastic adhesive over the central portion of the carrier wafer and disposing the second thermoplastic adhesive over the peripheral portion of the carrier wafer comprise disposing the second thermoplastic adhesive over the peripheral portion of the carrier wafer and subsequently disposing the first thermoplastic adhesive over the central portion of the carrier wafer and at least a portion of the second thermoplastic adhesive.
8. The method of claim 7, further comprising removing a portion of the second thermoplastic adhesive and the first thermoplastic adhesive from an outermost area of the peripheral portion of the carrier wafer.
9. The method of claim 1, wherein bonding the first thermoplastic adhesive to the at least a portion of the front side of the device wafer and the second thermoplastic adhesive to the peripheral portion of the front side of the device wafer comprises heating the first thermoplastic adhesive and the second thermoplastic adhesive and pressing the front side of the device wafer onto the heated first adhesive and second adhesive.
10. The method of claim 9, wherein heating the first thermoplastic adhesive and the second thermoplastic adhesive comprises heating the first thermoplastic adhesive and the second thermoplastic adhesive to at least about one hundred fifty degrees Celsius (150 C.).
11. The method of claim 1, further comprising reducing a thickness of the device wafer by removing material from a backside of the device wafer.
12. The method of claim 1, wherein bonding the second thermoplastic adhesive to the peripheral portion of the front side of the device wafer further comprises bonding the second adhesive to a lateral side surface of the device wafer adjacent to and surrounding the active surface.
13. A method of bonding a device wafer to a carrier wafer, comprising: disposing a first adhesive having a first glass transition temperature over substantially an entire surface of a carrier wafer and removing the first adhesive from an area extending from a periphery of the carrier wafer more than about twenty (20) mm radially inward to leave the first adhesive over a central portion of the carrier wafer; disposing a second adhesive having a second glass transition temperature greater than the first glass transition temperature over a peripheral portion of the carrier wafer; and bonding the first adhesive to a central portion of a front side of a device wafer and the second adhesive to a peripheral portion of the front side of the device wafer.
14. A method of bonding a device wafer to a carrier wafer, comprising: disposing a first adhesive having a first glass transition temperature over a central portion of a carrier wafer; disposing a second adhesive having a second glass transition temperature greater than the first glass transition temperature over a peripheral portion of the carrier wafer, comprising disposing the second adhesive over the peripheral portion of the carrier wafer to leave a gap between the second adhesive and the first adhesive; and bonding the first adhesive to at least a portion of a front side of a device wafer and the second adhesive to a peripheral portion of the front side of the device wafer.
15. A method of bonding a device wafer to a carrier wafer, comprising: disposing a first adhesive having a first glass transition temperature over a central portion of a carrier wafer; disposing a second adhesive having a second glass transition temperature greater than the first glass transition temperature over a peripheral portion of the carrier wafer; and bonding the first adhesive to at least a portion of a front side of a device wafer and the second adhesive to a peripheral portion of the front side of the device wafer, comprising: heating the first adhesive and the second adhesive; and pressing the front side of the device wafer onto the heated first adhesive and second adhesive, comprising pressing the device wafer and the carrier wafer together with between about eight (8) kN and thirty (30) kN of force.
16. A method of bonding a device wafer to a carrier wafer, comprising: disposing a first adhesive with a first glass transition temperature over a carrier wafer; removing the first adhesive from a peripheral portion of the carrier wafer; disposing a second adhesive with a second glass transition temperature higher than the first glass transition temperature over the peripheral portion of the carrier wafer and out of contact with the first adhesive; and bonding the first adhesive to a central portion of a device wafer and the second adhesive to a peripheral portion of the device wafer.
17. A method of bonding a device wafer to a carrier wafer, comprising: disposing a first adhesive having a first glass transition temperature over a portion of a carrier wafer; disposing a second adhesive having a second glass transition temperature over a portion of the carrier wafer; and bonding the first adhesive to a central portion of an active surface of a device wafer and bonding the second adhesive to a lateral side surface of the device wafer adjacent to and surrounding the active surface of the device wafer and to a peripheral portion of the active surface of the device wafer extending radially inward from the lateral side surface of the device wafer.
18. The method of claim 17, wherein bonding the second adhesive to the peripheral portion of the active surface of the device wafer comprises bonding the second adhesive to the peripheral portion of the active surface of the device wafer extending between about four (4) mm and about twenty (20) mm radially inward from the lateral side surface of the device wafer surrounding the active surface.
Description
BRIEF DESCRIPTION OF THE DRAWINGS
(1)
(2)
(3)
(4)
(5)
DETAILED DESCRIPTION
(6) The illustrations included herewith are not meant to be actual views of any particular methods or devices, but are merely idealized representations that are employed to describe embodiments described herein. Elements and features common between figures may retain the same numerical designation except that, for ease of following the description, for the most part, reference numerals begin with the number of the drawing on which the elements are introduced or most fully discussed.
(7) The following description provides specific details, such as material types, material thicknesses, and processing conditions in order to provide a thorough description of embodiments described herein. However, a person of ordinary skill in the art will understand that the embodiments disclosed herein may be practiced without employing these specific details. Indeed, the embodiments may be practiced in conjunction with conventional fabrication techniques employed in the semiconductor industry.
(8) With reference now to
(9) The second adhesive 208 may be a thermoplastic material with a T.sub.g higher than the T.sub.g of the first adhesive material 204. For example, the second adhesive 208 may have a T.sub.g of about fifteen degrees Celsius (15 C.), or more, higher than the T.sub.g of the first adhesive 204. As a non-limiting example, the T.sub.g of the second adhesive 208 may be between about fifteen degrees Celsius (15 C.) and about twenty-five degrees Celsius (25 C.) greater than the T.sub.g of the first adhesive 204. Suitable materials for the second adhesive 208 may include, without limitation, 9001A, available from Brewer Science, Inc., TA7000M available from Shin Etsu, Tokyo, Japan, or other adhesive materials having the desired characteristics.
(10) Since the second adhesive 208 has a higher T.sub.g than the first adhesive 204, the second adhesive 208 may be used to function as a dam around an outer periphery of the carrier wafer 200, preventing flow and seepage of the first adhesive 204 from an interface between a device wafer and carrier wafer 200 under elevated temperatures encountered during processing of a device wafer bonded to carrier wafer 200.
(11) The first adhesive 204 may be chosen in part based on a desired device feature density and topography of a device wafer to which the carrier wafer 200 is intended to be bonded. For example, a relatively lower viscosity adhesive may be suitable for a device wafer with a relatively higher feature density or higher topography, as the relatively lower viscosity adhesive may more easily wet and fill the fine features of the semiconductor device wafer.
(12) The first adhesive 204 and the second adhesive 208 may be disposed to a thickness of, for example, between about fifty (50) microns and about one hundred fifty (150) microns. As a further non-limiting example, the first adhesive 204 and the second adhesive 208 may be disposed to a thickness of between about ninety (90) microns and about one hundred (100) microns. The first adhesive 204 may be formed on the carrier wafer 200 by conventional techniques, such as by spin coating, dry film lamination, or spray coating. The second adhesive 208 may be formed on the outer periphery of the carrier wafer 200 by conventional techniques, such as spraying, dispensing from a tip dispensing device, e.g., a syringe, or by other methods.
(13) The carrier wafer 200 may have a substantially circular shape. As a non-limiting example, the carrier wafer 200 may have a diameter of about three hundred (300) mm and an initial thickness of about six hundred fifty (650) microns.
(14) Now referring to
(15) A portion of the first adhesive 310 may be removed from the peripheral portion 306 of the carrier wafer 300, as shown in
(16) Alternatively, the first adhesive 310 may be disposed over the central portion 304 of the carrier wafer 300 such that the peripheral portion 306 remains uncoated with the first adhesive 310. For example, a spin coating process may be tailored by adjusting, e.g., adhesive volume and spin parameters, to dispose the first adhesive 310 over the central portion 304 of the carrier wafer 300 while leaving the peripheral portion 306 uncoated, substantially as depicted in
(17) Referring now to
(18) The second adhesive 314 may be placed to leave a gap 320 between the first adhesive 310 and the second adhesive 314, i.e., such that the first adhesive 310 and the second adhesive 314 do not contact one another. A width w of the gap 320 may be selected based on the size of the secondary bead 316, the thickness of the first adhesive 310, or other factors, and will be discussed further below in connection with
(19) A portion of the second adhesive 314 may be removed from the peripheral portion 306 of the carrier wafer 300. For example, as shown in
(20) Following removal of a portion of the second adhesive 314, the carrier wafer 300 may be heated, e.g., baked, to remove undesirable residual solvents, e.g., solvents that may have been used to facilitate application of the adhesives, and/or solvents used to remove portions of the first adhesive 310 and the second adhesive 314. Baking time and temperature may depend on the type and amount of the residual solvents.
(21) Referring now to
(22) The device wafer 324 may be bonded to the carrier wafer 300 under heat and pressure. For example, the device wafer 324 may be concentrically aligned with the carrier wafer 300 by conventional techniques, and the device wafer 324 and the carrier wafer 300 may be placed in a mechanical press and pressed together under elevated temperature conditions, such as at a temperature about equal to the T.sub.g of the second adhesive 314 but higher than the T.sub.g of the first adhesive 310. As a non-limiting example, the temperature may be raised to at least about one hundred fifty degrees Celsius (150 C.), and the device wafer 324 and the carrier wafer 300 may be pressed together under at least about eight (8) kN up to about thirty (30) kN of force for about two (2) minutes. Bonding conditions of time, temperature, and force may be optimized for viscous interface conditions that depend upon melt viscosity of the first adhesive 310 and the second adhesive 314 at the bond temperature and the density and topology of the device architecture. As the device wafer 324 and the carrier wafer 300 are pressed together under the elevated temperature conditions, the first adhesive 310 melts and flows to fill and protect the topography of active surface 326 of device wafer 324 while bonding the active surface 326 to carrier wafer 300, while the second adhesive 314 may soften without excessive flow (i.e., seepage), bonding the carrier wafer 300 to the peripheral area 328 of the device wafer 324 and in some embodiments to lateral surface 336 extending from active surface 326 to peripheral area 328. Under these conditions, the adhesive material within the secondary bead 316 (
(23) Referring now to
(24) Referring now to
(25) When backside processing of the device wafer 324 is complete, the device wafer 324 may be debonded from the carrier wafer 300 by heating to a temperature above the T.sub.g of the first adhesive 310 where the shear modulus of the first adhesive 310 is less than or equal to about 1e5 Pa. to reduce the adhesive bond between device wafer 324 and carrier wafer 300. A mechanical shear force may be applied substantially parallel to the bonding surface 302 and the active surface 326 of the device wafer 324 to slide the carrier wafer 300 and the device wafer 324 apart. Because the remaining small portion 334 of second adhesive 314 only bonds to a small area at the periphery of carrier wafer 300 and the active surface 326 of the device wafer 324, the cumulative bonding strength (i.e., the total bonding strength over the entire bonding area) of the second adhesive 314 may be negligible compared to the cumulative bonding strength of the heated, melted first adhesive 310. Thus, the force and temperature utilized to debond the device wafer 324 from the carrier wafer 300 using methods of the present disclosure may be similar to that utilized for debonding when only a single adhesive is used, e.g., a process flow similar to that described above in connection with
(26) The higher T.sub.g of the second adhesive material 314 relative to the first adhesive material 310 may enable the second adhesive material 314 to maintain its integrity during backside processing acts that involve relatively high temperature (e.g., in excess of about 200 C.) thermal cycles. The portion 334 of the second adhesive 314 may prevent the first adhesive 310 from flowing from between the carrier wafer 300 and the device wafer 324 under elevated temperatures during backside processing. Eliminating the flow may protect the active surface 326 of the device wafer 324 from adhesive squeeze out (i.e., seepage) and contamination during thinning and backside processing acts.
(27) Moreover, adhesive forces between the second adhesive 314, the device wafer 324, and the bonding surface 302 of the carrier wafer 300 may prevent heat-induced warping in the device wafer 324 from causing a peripheral edge of the device wafer 324 to lift away from the bonding surface 302 of the carrier wafer 300. During the thinning and backside processing, the second adhesive 314 may provide sufficient adhesion between the device wafer 324 and the carrier wafer 300 at temperatures that reduce the adhesive strength of first adhesive 310 to reduce or prevent such warping. The disclosed methods may provide increases in thickness uniformity of the thinned device wafer 324, prevent crack formation in the device wafer 324, and increase yields by a reduction in edge die loss.
(28) The disclosure includes a method of bonding a device wafer to a carrier wafer, the method comprising disposing a first adhesive having a glass transition temperature over a central portion of a carrier wafer. A second adhesive having a glass transition temperature greater than the first glass transition temperature is disposed over a peripheral portion of the carrier wafer. The first adhesive is bonded to at least a portion of a front side of a device wafer and the second adhesive is bonded to a peripheral portion of the front side of the device wafer and to a portion of an active surface of the device wafer.
(29) The disclosure also includes a method of bonding a device wafer to a carrier wafer, the method comprising disposing a first adhesive with a first glass transition temperature over the carrier wafer. The first adhesive is removed from a peripheral portion of the carrier wafer, and a second adhesive with a second glass transition temperature higher than the first glass transition temperature is disposed over the peripheral portion of the carrier wafer. The first adhesive is bonded to a central portion of a device wafer and the second adhesive is bonded to a peripheral portion of the device wafer.
(30) Referring now to
(31) Referring now to
(32) Referring now to
(33) As shown in
(34) As shown in
(35) The disclosure includes a method of bonding a device wafer to a carrier wafer, the method comprising disposing an adhesive having a first glass transition temperature over a peripheral area of the carrier wafer. Another adhesive having a second glass transition temperature lower than the first glass transition temperature is disposed over the carrier wafer and the adhesive having a first glass transition temperature. A portion of the adhesive having a first glass transition temperature and a portion of the another adhesive having a second glass transition temperature is removed from the peripheral area of the carrier wafer. The adhesive having a first glass transition temperature and the another adhesive having a second glass transition temperature are bonded to a device wafer.
(36) The area of the carrier wafer over which the second adhesive is disposed may be chosen to provide a particular desired bond strength at the periphery of the device wafer. In some embodiments, the second adhesive may be disposed over an area of the carrier wafer such that a greater portion of the second adhesive is disposed between the active surface of the front side of the device wafer and the carrier wafer compared to the embodiments of
(37) Referring now to
(38) As shown in
(39) In the embodiment of
(40) Further, first adhesive 310 may be optimized to provide interface properties between a device wafer and a carrier wafer with respect to topography and conductive elements (e.g., solder bumps) combined with favorable debonding parameters such as debonding temperature and device wafer slide speed.
(41) Superior adhesion of the device wafer to the carrier wafer by using a two (inner and outer) zone adhesive bonding approach device may eliminate wafer edge chipping, device wafer delamination, crack formation, and loss of die. Overall thickness uniformity of the thinned device wafer is increased, increasing yield by reducing edge die loss. Other processing steps may also be simplified since the incoming device wafer/carrier wafer stack is flat. As a non-limiting example, abrasive processing, such as CMP processing, and device wafer backside plating each benefit from flat, well-adhered device wafer/carrier wafer stacks.
(42) The disclosure includes a method of bonding a device wafer to a carrier wafer, the method comprising disposing a first adhesive having a first glass transition temperature over a portion of the carrier wafer. A second adhesive having a second glass transition temperature is disposed over a portion of the carrier wafer. The first adhesive is bonded to a central portion of an active surface of a device wafer, and the second adhesive is bonded to a peripheral portion of the active surface of the device wafer.
(43) The disclosure also includes an assembly including a carrier wafer and a device wafer having an active surface facing the carrier wafer. A first thermoplastic adhesive material is between the carrier wafer and the device wafer. A second thermoplastic material exhibiting a higher glass transition temperature than a glass transition temperature exhibited by the first thermoplastic adhesive material peripherally surrounds the first adhesive material between the carrier wafer and the device wafer.
(44) While certain illustrative embodiments have been described in connection with the figures, those of ordinary skill in the art will recognize and appreciate that embodiments encompassed by the disclosure are not limited to those embodiments explicitly shown and described herein. Rather, many additions, deletions, and modifications to the embodiments described herein may be made without departing from the scope of embodiments encompassed by the disclosure, such as those hereinafter claimed, including legal equivalents. In addition, features from one disclosed embodiment may be combined with features of another disclosed embodiment while still being encompassed within the scope of the disclosure.