C08F222/103
LIGHT-CURING RESIN COMPOSITION, THREE-DIMENSIONAL OBJECT CONTAINING THE SAME, AND MANUFACTURING METHOD OF THREE-DIMENSIONAL OBJECT
A light-curing resin composition, a three-dimensional object containing the same, and a manufacturing method of the three-dimensional object are provided. The light-curing resin composition includes a photoinitiator, an acrylic oligomer, an acrylic monomer, and expandable particles with hollow spherical shell structures. The acrylic monomer is a monofunctional monomer, a difunctional monomer, or a combination thereof.
Pattern-forming composition, film, infrared cut filter, infrared transmitting filter, solid image pickup element, infrared sensor, and camera module
Provided is a pattern-forming composition, including: an infrared absorbing colorant; and at least one compound selected from the group consisting of a resin having a glass transition temperature of 150° C. to 300° C. and a precursor of a resin having a glass transition temperature of 150° C. to 300° C.
Pattern-forming composition, film, infrared cut filter, infrared transmitting filter, solid image pickup element, infrared sensor, and camera module
Provided is a pattern-forming composition, including: an infrared absorbing colorant; and at least one compound selected from the group consisting of a resin having a glass transition temperature of 150° C. to 300° C. and a precursor of a resin having a glass transition temperature of 150° C. to 300° C.
Composite film with anti-reflective coating
A composite film may include a first transparent substrate and a first anti-reflective coating overlying a first surface of the first transparent substrate. The first anti-reflective coating may include a first UV curable acrylate binder, a photo initiator component, and silica nanoparticles dispersed within the first anti-reflective coating. The first anti-reflective coating may further include a ratio AC1.sub.SiO2/AC1.sub.B of at least about 0.01 and not greater than about 1.3. The composite film may further have a VLT of at least about 93.0% and a haze value of not greater than about 3%.
Composite film with anti-reflective coating
A composite film may include a first transparent substrate and a first anti-reflective coating overlying a first surface of the first transparent substrate. The first anti-reflective coating may include a first UV curable acrylate binder, a photo initiator component, and silica nanoparticles dispersed within the first anti-reflective coating. The first anti-reflective coating may further include a ratio AC1.sub.SiO2/AC1.sub.B of at least about 0.01 and not greater than about 1.3. The composite film may further have a VLT of at least about 93.0% and a haze value of not greater than about 3%.
Composition for model materials, optically shaped article, and method for producing optically shaped articles
A composition for model materials (4a) is used for shaping an optically shaped article by an inkjet optical shaping method, comprises a monofunctional monomer (A) and an oligomer (B) as a photocurable component, further, comprises no polyfunctional monomer (C) as a photocurable component, or comprises a polyfunctional monomer (C) as a photocurable component at 3.0 parts by weight based on 100 parts by weight of a whole composition for model materials, the oligomer (B) has a hydroxyl group or an amino group, and a total molar fraction of the hydroxyl group and the amino group in a total amount of the photocurable components is less than 5.0%. The composition for model materials (4a) can afford an optically shaped article that has flexibility, and does not crack even when it is bent.
Composition for model materials, optically shaped article, and method for producing optically shaped articles
A composition for model materials (4a) is used for shaping an optically shaped article by an inkjet optical shaping method, comprises a monofunctional monomer (A) and an oligomer (B) as a photocurable component, further, comprises no polyfunctional monomer (C) as a photocurable component, or comprises a polyfunctional monomer (C) as a photocurable component at 3.0 parts by weight based on 100 parts by weight of a whole composition for model materials, the oligomer (B) has a hydroxyl group or an amino group, and a total molar fraction of the hydroxyl group and the amino group in a total amount of the photocurable components is less than 5.0%. The composition for model materials (4a) can afford an optically shaped article that has flexibility, and does not crack even when it is bent.
Method of making 3D printed objects using two distinct light sources
This invention relates to the field of 3D printing used to make a 3D object where a 3D printed object is formed using electromagnetic radiation emitted from a visual display screen or emissive pixel array screen illuminated by radiation sources with effectively non-overlapping wavelength emission spectra with the effect of creating two different polymerised properties in the object.
Method of making 3D printed objects using two distinct light sources
This invention relates to the field of 3D printing used to make a 3D object where a 3D printed object is formed using electromagnetic radiation emitted from a visual display screen or emissive pixel array screen illuminated by radiation sources with effectively non-overlapping wavelength emission spectra with the effect of creating two different polymerised properties in the object.
FILM AND ELECTRONIC DEVICE COMPRISING SAME
Provided are a film and an electric device comprising the same. The film comprises at least one modified polyolefin resin layer. A resin forming the modified polyolefin resin layer comprises 1-100% of modified polyolefin resin. A main chain in the modified polyolefin resin is an ethylene-α-olefin copolymer. A grafted branched chain in the modified polyolefin resin is selected from a compound formed by a vinyl monomer comprising one or more of anhydride group, hydroxyl, ester group, carbonyl, acylamino, pyridyl, epoxy, pyrrolidonyl and glycidyl. A molecular weight of the grafted branched chain is 150-8000 g/mol. The film prepared from the modified POE layer with the main chain and the grafted branched chain has excellent anti-PID performance. The layers have a better adhesive property without a laminated interface therebetween. The co-extruded film further has an excellent water vapor barrier property, a relatively high insulating property and a relatively high light transmittance.