A62D3/36

COMPOSITES FOR CHEMICAL SEQUESTRATION DECONTAMINATION

Materials for decontamination of compounds having a phosphorous-sulfur bond or a phosphorous-oxygen bond. A porous polymer, such as poly(dicyclopentadiene), contains particles of zirconium hydroxide. The polymer optionally has hydroperoxide groups.

Method and system for neutralizing asbestos
11534644 · 2022-12-27 ·

A system for asbestos neutralization, that includes a neutralization unit having a module configured for sorting of asbestos waste, an asbestos waste grinder; a concentrated sulfuric acid tank, a vat containing a hot diluted acid solution, for which temperature is between 70° C. and 100° C., in which grinded asbestos waste containing asbestos is dipped, the solution is configured for neutralizing asbestos contained in the grinded asbestos waste, a filtration unit to separate, at the end of the neutralization reaction, a solid inert waste from a liquid phase of the diluted acid solution, a regeneration unit for the diluted acid solution, which adjusts the hydrogen potential of the extracted liquid phase by adding concentrated sulfuric acid from the tank, and means for transferring the regenerated solution into the vat.

Method and system for neutralizing asbestos
11534644 · 2022-12-27 ·

A system for asbestos neutralization, that includes a neutralization unit having a module configured for sorting of asbestos waste, an asbestos waste grinder; a concentrated sulfuric acid tank, a vat containing a hot diluted acid solution, for which temperature is between 70° C. and 100° C., in which grinded asbestos waste containing asbestos is dipped, the solution is configured for neutralizing asbestos contained in the grinded asbestos waste, a filtration unit to separate, at the end of the neutralization reaction, a solid inert waste from a liquid phase of the diluted acid solution, a regeneration unit for the diluted acid solution, which adjusts the hydrogen potential of the extracted liquid phase by adding concentrated sulfuric acid from the tank, and means for transferring the regenerated solution into the vat.

Method for detoxifying chromium slag by using high sulfur coal

The present invention discloses a method for detoxifying chromium slag by using high sulfur coal. The method includes: sieving chromium slag into coarse-grained chromium slag and fine-grained chromium slag, air-drying and crushing both the coarse-grained chromium slag and the fine-grained chromium slag; separately mixing the crushed coarse-grained chromium slag and fine-grained chromium slag with the crushed high sulfur coal uniformly; adjusting pH values of a coarse-grained slag mixture and a fine-grained slag mixture to 8.0-11.0 and moisture content thereof to 12%-18%; conducting reduction on the treated coarse-grained slag mixture and fine-grained slag mixture, where the reduction temperature of the fine-grained slag mixture is 500-700° C., the reduction time of the fine-grained slag mixture is 10-30 min, the reduction temperature of the coarse-grained slag mixture is 800-1000° C., the reduction time of the coarse-grained slag mixture is 10-30 min; after the reduction, conducting water quenching, and discharging the product.

Method for detoxifying chromium slag by using high sulfur coal

The present invention discloses a method for detoxifying chromium slag by using high sulfur coal. The method includes: sieving chromium slag into coarse-grained chromium slag and fine-grained chromium slag, air-drying and crushing both the coarse-grained chromium slag and the fine-grained chromium slag; separately mixing the crushed coarse-grained chromium slag and fine-grained chromium slag with the crushed high sulfur coal uniformly; adjusting pH values of a coarse-grained slag mixture and a fine-grained slag mixture to 8.0-11.0 and moisture content thereof to 12%-18%; conducting reduction on the treated coarse-grained slag mixture and fine-grained slag mixture, where the reduction temperature of the fine-grained slag mixture is 500-700° C., the reduction time of the fine-grained slag mixture is 10-30 min, the reduction temperature of the coarse-grained slag mixture is 800-1000° C., the reduction time of the coarse-grained slag mixture is 10-30 min; after the reduction, conducting water quenching, and discharging the product.

Protective technology with reactive solid sorbent for oxidative decontamination of toxic materials

A solid particulate reactive sorbent for decontaminating toxic chemical and biological agents and its method of making. The reactive sorbent comprising a plurality of aggregates formed from linked hydrophilic nanoparticles and individual nanoparticles that bind at least one detoxifier, such that the sorbent absorbs the agents, allowing the detoxifier to oxidize and decontaminate the agents for removal. More preferably, the hydrophilic nanoparticles comprise fumed silica and the detoxifier comprises hydrogen peroxide.

METHOD AND REAGENT SYSTEM FOR REMEDIATING MINE WASTE AND OTHER SOLID WASTE CONTAMINATED WITH HEAVY METALS
20220348463 · 2022-11-03 ·

A reagent system for treating heavy metal-contaminated materials is provided and includes an oxidizer, a soluble phosphate, and an alkaline hydroxide source, such as a caustic soda or lime. A method of treating mine waste bearing one or more heavy metals is also provided and includes the step of admixing a reagent system with heavy metal-containing material to preferentially reduce the leachability of heavy metals and form precipitates and complexes of low metal solubility that remain stable within the host solid matrix for long durations in acidic and abrasive conditions.

METHOD AND REAGENT SYSTEM FOR REMEDIATING MINE WASTE AND OTHER SOLID WASTE CONTAMINATED WITH HEAVY METALS
20220348463 · 2022-11-03 ·

A reagent system for treating heavy metal-contaminated materials is provided and includes an oxidizer, a soluble phosphate, and an alkaline hydroxide source, such as a caustic soda or lime. A method of treating mine waste bearing one or more heavy metals is also provided and includes the step of admixing a reagent system with heavy metal-containing material to preferentially reduce the leachability of heavy metals and form precipitates and complexes of low metal solubility that remain stable within the host solid matrix for long durations in acidic and abrasive conditions.

METHOD AND SYSTEM FOR NEUTRALIZING ASBESTOS
20170304666 · 2017-10-26 ·

The invention relates to a system for neutralizing asbestos, said system comprising a mobile neutralization unit (200) comprising: an asbestos waste sorting module (225), an asbestos grinder (255) and a hot acid bath (250) for rendering asbestos inert.

Preferably, the asbestos waste sorting module comprises: a window with glove boxes; and a conveyor for transporting the asbestos waste in front of the window.

In embodiments, the system comprises a means for containing the atmosphere within the mobile neutralization unit and/or the hot acid bath (250) of the mobile neutralization unit (200) comprises sulfuric acid.

METHOD AND SYSTEM FOR NEUTRALIZING ASBESTOS
20170304666 · 2017-10-26 ·

The invention relates to a system for neutralizing asbestos, said system comprising a mobile neutralization unit (200) comprising: an asbestos waste sorting module (225), an asbestos grinder (255) and a hot acid bath (250) for rendering asbestos inert.

Preferably, the asbestos waste sorting module comprises: a window with glove boxes; and a conveyor for transporting the asbestos waste in front of the window.