H01M10/058

LITHIUM ION BATTERY MODULE

A lithium-ion battery module includes a housing having a plurality of partitions configured to define a plurality of compartments within a housing. The battery module also includes a lithium-ion cell element provided in each of the compartments of the housing. The battery module further includes a cover coupled to the housing and configured to route electrolyte into each of the compartments. The cover is also configured to seal the compartments of the housing.

LITHIUM ION BATTERY MODULE

A lithium-ion battery module includes a housing having a plurality of partitions configured to define a plurality of compartments within a housing. The battery module also includes a lithium-ion cell element provided in each of the compartments of the housing. The battery module further includes a cover coupled to the housing and configured to route electrolyte into each of the compartments. The cover is also configured to seal the compartments of the housing.

METHOD FOR MANUFACTURING NONAQUEOUS ELECTROLYTE SECONDARY BATTERY

A method for manufacturing a nonaqueous electrolyte secondary battery according to an embodiment of the present invention is a method for manufacturing a nonaqueous electrolyte secondary battery including a positive electrode plate and a negative electrode plate provided with a negative electrode mixture layer containing graphite and a silicon material and includes a step of applying positive electrode mixture slurry containing a lithium-transition metal composite oxide and polyvinylidene fluoride to a positive electrode current collector, a step of forming a positive electrode mixture layer by drying the positive electrode mixture slurry, and a step of heat-treating the positive electrode mixture layer. The temperature of heat treatment is preferably 160° C. to 350° C.

METHOD FOR MANUFACTURING NONAQUEOUS ELECTROLYTE SECONDARY BATTERY

A method for manufacturing a nonaqueous electrolyte secondary battery according to an embodiment of the present invention is a method for manufacturing a nonaqueous electrolyte secondary battery including a positive electrode plate and a negative electrode plate provided with a negative electrode mixture layer containing graphite and a silicon material and includes a step of applying positive electrode mixture slurry containing a lithium-transition metal composite oxide and polyvinylidene fluoride to a positive electrode current collector, a step of forming a positive electrode mixture layer by drying the positive electrode mixture slurry, and a step of heat-treating the positive electrode mixture layer. The temperature of heat treatment is preferably 160° C. to 350° C.

ELECTRIC TOOL POWERED BY A PLURALITY OF BATTERY PACKS AND ADAPTER THEREFOR
20230238806 · 2023-07-27 ·

An electrical apparatus includes first and second battery interfaces disposed on a housing for electrically and mechanically connecting first and second battery packs in series. A controller is disposed within the housing and includes an apparatus microprocessor that receives first and second communication signals respectively outputted from respective microprocessors of the first and second battery packs. A first signal communication path communicates the first communication signal from the first battery pack microprocessor to the apparatus microprocessor by shifting a first voltage range of the first communication signal to a second voltage range that is suitable for inputting into the apparatus microprocessor. A second signal communication path communicates a third communication signal from the apparatus microprocessor to the first battery pack microprocessor by shifting the second voltage range of the third communication signal to a first voltage range that is suitable for inputting into the first battery pack microprocessor.

POROUS CERAMIC SEPARATOR MATERIALS AND FORMATION PROCESSES
20230006242 · 2023-01-05 · ·

Energy storage devices, battery cells, and batteries may include a battery cell component that is formed by a method that includes forming a slurry that includes a ceramic material, a binder, and an ionic dispersant. The ceramic material may be greater than 50% of the slurry by weight. The method may also include applying the slurry to a polymeric material to form a two-layer separator. The slurry may be applied to a thickness of less than or about 10 μm.

POROUS CERAMIC SEPARATOR MATERIALS AND FORMATION PROCESSES
20230006242 · 2023-01-05 · ·

Energy storage devices, battery cells, and batteries may include a battery cell component that is formed by a method that includes forming a slurry that includes a ceramic material, a binder, and an ionic dispersant. The ceramic material may be greater than 50% of the slurry by weight. The method may also include applying the slurry to a polymeric material to form a two-layer separator. The slurry may be applied to a thickness of less than or about 10 μm.

ELECTROCHEMICAL APPARATUS, ELECTRONIC APPARATUS, AND PREPARATION METHOD OF ELECTROCHEMICAL APPARATUS

An electrochemical apparatus includes a positive electrode. The positive electrode includes a current collector, a first material layer, and a second material layer. The second material layer is disposed on at least one surface of the current collector, and the first material layer is disposed between the current collector and the second material layer. The first material layer includes a leveling agent. A difference between the maximum value and the minimum value of thickness of the first material layer is less than or equal to 3 μm. The obtained positive electrode has high uniformity in thickness, and there is strong adhesion between the current collector and the first material layer, and between the second material layer and the first material layer.

ELECTROCHEMICAL APPARATUS, ELECTRONIC APPARATUS, AND PREPARATION METHOD OF ELECTROCHEMICAL APPARATUS

An electrochemical apparatus includes a positive electrode. The positive electrode includes a current collector, a first material layer, and a second material layer. The second material layer is disposed on at least one surface of the current collector, and the first material layer is disposed between the current collector and the second material layer. The first material layer includes a leveling agent. A difference between the maximum value and the minimum value of thickness of the first material layer is less than or equal to 3 μm. The obtained positive electrode has high uniformity in thickness, and there is strong adhesion between the current collector and the first material layer, and between the second material layer and the first material layer.

COMPOSITE ELECTRODE COMPRISING A METAL AND A POLYMER MEMBRANE, MANUFACTURING METHOD AND BATTERY CONTAINING SAME
20230006199 · 2023-01-05 ·

A composite negative electrode based on pure metallic lithium, pure metallic sodium or one of their alloys and a polymer membrane, a method for manufacturing such an electrode, as well as an electrical energy storage system, in particular an electrochemical accumulator such as a secondary (rechargeable) lithium or sodium battery comprising at least one such negative electrode. It is particularly applicable to Lithium-Metal-Polymer or LMP™ batteries.