Patent classifications
H01L21/3003
Hydrogenated graphene with surface doping and bandgap tunability
A graphene compound made from the method of preparing graphene flakes or chemical vapor deposition grown graphene films on a SiO.sub.2/Si substrate; exposing the graphene flakes or the chemical vapor deposition grown graphene film to hydrogen plasma; performing hydrogenation of the graphene; wherein the hydrogenated graphene has a majority carrier type; creating a bandgap from the hydrogenation of the graphene; applying an electric field to the hydrogenated graphene; and tuning the bandgap.
Tuning threshold voltage through meta stable plasma treatment
A method includes forming a first high-k dielectric layer over a first semiconductor region, forming a second high-k dielectric layer over a second semiconductor region, forming a first metal layer comprising a first portion over the first high-k dielectric layer and a second portion over the second high-k dielectric layer, forming an etching mask over the second portion of the first metal layer, and etching the first portion of the first metal layer. The etching mask protects the second portion of the first metal layer. The etching mask is ashed using meta stable plasma. A second metal layer is then formed over the first high-k dielectric layer.
Advanced hydrogenation of silicon solar cells
A method of hydrogenation of a silicon photovoltaic junction device is provided, the silicon photovoltaic junction device comprising p-type silicon semiconductor material and n-type silicon semiconductor material forming at least one p-n junction. The method comprises: i) ensuring that any silicon surface phosphorus diffused layers through which hydrogen must diffuse have peak doping concentrations of 1×10.sup.20 atoms/cm.sup.3 or less and silicon surface boron diffused layers through which hydrogen must diffuse have peak doping concentrations of 1×10.sup.19 atoms/cm.sup.3 or less; ii) Providing one or more hydrogen sources accessible by each surface of the device; and iii) Heating the device, or a local region of the device to at least 40° C. while simultaneously illuminating at least some and/or advantageously all of the device with at least one light source whereby the cumulative power of all the incident photons with sufficient energy to generate electron hole pairs within the silicon (in other words photons with energy levels above the bandgap of silicon of 1.12 eV) is at least 20 mW/cm.sup.2.
CONTACT FORMATION ON GERMANIUM-CONTAINING SUBSTRATES USING HYDROGENATED SILICON
A method and structure is provided in which germanium or a germanium tin alloy can be used as a channel material in either planar or non-planar architectures, with a functional gate structure formed utilizing either a gate first or gate last process. After formation of the functional gate structure, and contact openings within a middle-of-the-line (MOL) dielectric material, a hydrogenated silicon layer is formed that includes hydrogenated crystalline silicon regions disposed over the germanium or a germanium tin alloy, and hydrogenated amorphous silicon regions disposed over dielectric material. The hydrogenated amorphous silicon regions can be removed selective to the hydrogenated crystalline silicon regions, and thereafter a contact structure is formed on the hydrogenated crystalline silicon regions.
SEMICONDUCTOR DEVICE AND METHOD FOR FABRICATING THE SAME
A semiconductor device includes: a dielectric structure in which etch stop structures and low-k layers are alternately stacked over a substrate; and a metal interconnection electrically connected to the substrate in the dielectric structure, wherein each one of the etch stop structures includes: a first etch stop layer including a hydrogen blocking material; and a second etch stop layer formed over the first etch stop layer.
Method of manufacturing the thin film
The invention disclosed a method of manufacturing the thin film, which belongs to the technological field of SOI wafer manufacture. By growing a layer of dielectric material (silicon oxide) on the provided high-resistivity silicon wafer, then to grow a layer of amorphous silicon on the dielectric material, to transfer a layer of silicon oxide to the amorphous silicon, to make the mono crystalline silicon exist on the oxidation layer, so that a SOI wafer with a layer of amorphous silicon is manufactured. The process above is completed in specific process conditions. The manufactured thin film, e.g. SOI wafer with amorphous silicon layer, is used main for RF apparatus.
SEMICONDUCTOR DEVICE HAVING GERMANIUM LAYER AS CHANNEL REGION AND METHOD FOR MANUFACTURING THE SAME
A semiconductor device having a channel region that is formed in a germanium layer and has a first conductive type, and a source region and a drain region that are formed in the germanium layer and have a second conductive type different from the first conductive type, wherein an oxygen concentration in the channel region is less than an oxygen concentration in a junction interface between at least one of the source region and the drain region and a region that surrounds the at least one of the source region and the drain region and has the first conductive type.
SEMICONDUCTOR DEVICE AND METHOD OF MANUFACTURING THE SAME
A method of manufacturing a semiconductor device includes forming a stack in which first material layers and second material layers are alternately stacked, forming a channel structure passing through the stack, forming openings by removing the first material layers, forming an amorphous blocking layer in the openings, and performing a first heat treatment process to supply deuterium through the openings and substitute hydrogen in the channel structure with the deuterium.
METHOD FOR MANUFACTURING NONVOLATILE MEMORY THIN FILM DEVICE BY USING NEUTRAL PARTICLE BEAM GENERATION APPARATUS
The present invention relates to a method for manufacturing a nonvolatile memory thin film device by using a neutral particle beam generation apparatus. The present invention solves the problem that substrates such as glass and a plastic film may not be used for manufacturing the memory thin film device due to the high temperature heat treatment process for a long time, in the existing method for manufacturing the thin film device having the nonvolatile memory function by forming the mobile proton layer.
Apparatus and systems for substrate processing for lowering contact resistance
Methods, apparatuses, and systems for substrate processing for lowering contact resistance in at least contact pads of a semiconductor device are provided herein. In some embodiments, a method of substrate processing for lowering contact resistance of contact pads includes: circulating a cooling fluid in at least one channel of a pedestal; and exposing a backside of the substrate located on the pedestal to a cooling gas to cool a substrate located on the pedestal to a temperature of less than 70 degrees Celsius. In some embodiments in accordance with the present principles, the method can further include distributing a hydrogen gas or hydrogen gas combination over the substrate.