Patent classifications
H01L2224/81075
Bonding with pre-deoxide process and apparatus for performing the same
A method includes picking up a first package component, removing an oxide layer on an electrical connector of the first package component, placing the first package component on a second package component after the oxide layer is removed, and bonding the first package component to the second package component.
METHOD FOR ASSEMBLING COMPONENTS IMPLEMENTING A PRE-TREATMENT OF THE SOLDER BUMPS ALLOWING AN ASSEMBLY BY FLUXLESS AND RESIDUE-FREE SOLDERING
A method for assembling components implementing includes a pre-treatment of the solder bumps allowing an assembly by fluxless and residue-free soldering. A first component carrying solder bumps is assembled with a second component carrying connectors. Beforehand, a pre-treatment of the components carrying solder bumps is carried out by contacting them with a pre-treatment liquid which makes their subsequent fluxless and residue-free soldering possible.
Semiconductor device with a protection mechanism and associated systems, devices, and methods
A semiconductor device includes a substrate; a die attached over the substrate; and a metal enclosure continuously encircling a space and extending vertically between the substrate and the die.
Bonding with Pre-Deoxide Process and Apparatus for Performing the Same
A method includes picking up a first package component, removing an oxide layer on an electrical connector of the first package component, placing the first package component on a second package component after the oxide layer is removed, and bonding the first package component to the second package component.
Method for producing joined structure
A method for producing a joined structure according to the present invention includes: a reflow step of heating a first member and a solder material while keeping them in contact with each other in a reflow chamber to melt a solder alloy constituting the solder material, the reflow step including: a first reflow step of melting the solder alloy with an atmosphere in the reflow chamber reduced to a first pressure P.sub.1 lower than the atmospheric pressure; and a second reflow step of, after the first reflow step, melting the solder alloy with the atmosphere in the reflow chamber reduced to a second pressure P.sub.2 lower than the first pressure P.sub.1.
Advanced Device Assembly Structures And Methods
A microelectronic assembly includes a first substrate having a surface and a first conductive element and a second substrate having a surface and a second conductive element. The assembly further includes an electrically conductive alloy mass joined to the first and second conductive elements. First and second materials of the alloy mass each have a melting point lower than a melting point of the alloy. A concentration of the first material varies in concentration from a relatively higher amount at a location disposed toward the first conductive element to a relatively lower amount toward the second conductive element, and a concentration of the second material varies in concentration from a relatively higher amount at a location disposed toward the second conductive element to a relatively lower amount toward the first conductive element.
System and method for uniform pressure gang bonding
A uniform pressure gang bonding device and fabrication method are presented using an expandable upper chamber with an elastic surface. Typically, the elastic surface is an elastomer material having a Young's modulus in a range of 40 to 1000 kilo-Pascal (kPA). After depositing a plurality of components overlying a substrate top surface, the substrate is positioned over the lower plate, with the top surface underlying and adjacent (in close proximity) to the elastic surface. The method creates a positive upper chamber medium pressure differential in the expandable upper chamber, causing the elastic surface to deform. For example, the positive upper chamber medium pressure differential may be in the range of 0.05 atmospheres (atm) and 10 atm. Typically, the elastic surface deforms between 0.5 millimeters (mm) and 20 mm, in response to the positive upper chamber medium pressure differential.
LOW PRESSURE SINTERING POWDER
A sintering powder comprising: a first type of metal particles having a mean longest dimension of from 100 nm to 50 μm.
SEMICONDUCTOR DEVICE WITH A PROTECTION MECHANISM AND ASSOCIATED SYSTEMS, DEVICES, AND METHODS
A semiconductor device includes a substrate; a die attached over the substrate; and a metal enclosure continuously encircling a space and extending vertically between the substrate and the die.
METHOD FOR PRODUCING JOINED STRUCTURE
A method for producing a joined structure according to the present invention includes: a reflow step of heating a first member and a solder material while keeping them in contact with each other in a reflow chamber to melt a solder alloy constituting the solder material, the reflow step including: a first reflow step of melting the solder alloy with an atmosphere in the reflow chamber reduced to a first pressure P.sub.1 lower than the atmospheric pressure; and a second reflow step of, after the first reflow step, melting the solder alloy with the atmosphere in the reflow chamber reduced to a second pressure P.sub.2 lower than the first pressure P.sub.1.