H01L2224/83896

Bonded die assembly containing a manganese-containing oxide bonding layer and methods for making the same

A method of forming a bonded assembly includes providing a first semiconductor die containing a first substrate, first semiconductor devices, first dielectric material layers overlying the first semiconductor devices, and first metal interconnect structures, providing a second semiconductor die containing a second substrate, second semiconductor devices, second dielectric material layers overlying the second semiconductor devices, and second metal interconnect structures, depositing a manganese layer on a top surface of the first dielectric material layers, disposing the second semiconductor die on the manganese layer such that a surface of the second dielectric material layers contacts the manganese layer, and performing a bonding anneal to bond the first semiconductor die to the second semiconductor die and to convert the manganese layer into a manganese-containing oxide layer, such that the manganese-containing oxide layer is bonded to the first dielectric material layers and the second dielectric material layers.

Hybrid Bonding with Uniform Pattern Density
20220173092 · 2022-06-02 ·

A chip includes a semiconductor substrate, integrated circuits with at least portions in the semiconductor substrate, and a surface dielectric layer over the integrated circuits. A plurality of metal pads is distributed substantially uniformly throughout substantially an entirety of a surface of the chip. The plurality of metal pads has top surfaces level with a top surface of the surface dielectric layer. The plurality of metal pads includes active metal pads and dummy metal pads. The active metal pads are electrically coupled to the integrated circuits. The dummy metal pads are electrically decoupled from the integrated circuits.

Three-dimensional memory devices and fabricating methods thereof

A method for forming a gate structure of a 3D memory device is provided. The method comprises forming an array wafer including a periphery region and a staircase and array region. A process of forming the array wafer comprises forming an etch stop layer on a first substrate in the periphery region, forming an array device on the first substrate in the staircase and array region, and forming at least one first vertical through in the periphery region and in contact with the etch stop layer. The method further comprises forming a CMOS wafer, and bonding the array wafer and the CMOS wafer. The method further comprises forming at least one through substrate contact penetrating the first substrate and the etch stop layer, and in contact with the at least one first vertical through contact.

Semiconductor devices including bonding layer and adsorption layer

A semiconductor device includes a first adsorption layer, a first bonding layer, a second bonding layer, and a second adsorption layer stacked on a first substrate, and a conductive pattern structure penetrating through the first adsorption layer, the first bonding layer, the second bonding layer and the second adsorption layer. The first and second bonding layers are in contact with each other, and each of the first and second adsorption layers includes a low-K dielectric material.

METHOD OF MANUFACTURING DIE STACK STRUCTURE

A method of manufacturing a die stack structure includes the following steps. A first bonding structure is formed over a front side of a first die. The method of forming the first bonding structure includes the following steps. A first bonding dielectric material is formed on a first test pad of the first die. A first blocking layer is formed over the first bonding dielectric material. A second bonding dielectric material and a first dummy metal layer are formed over the first blocking layer. The first dummy metal layer and the first test pad are electrically isolated from each other by the first blocking layer. Thereafter, a second bonding structure is formed over a front side of a second die. The first die and the second die are bonded through the first bonding structure and the second bonding structure.

Three-dimensional memory devices and fabricating methods thereof

A method for forming a gate structure of a 3D memory device is provided. The method comprises forming an array wafer including a periphery region and a staircase and array region. A process of forming the array wafer comprises forming an array well structure in a first substrate in the periphery region, forming an array device on the first substrate in the staircase and array region, and forming at least one vertical through contact in the periphery region and in contact with the array well structure. The method further comprises forming a CMOS wafer, and bonding the array wafer and the CMOS wafer. The method further comprises forming at least one through substrate contact penetrating the first substrate and the array well structure, and in contact with the at least one vertical through contact.

Semiconductor structure and manufacturing method thereof
11342307 · 2022-05-24 · ·

A semiconductor structure includes a first die, a second die, and a first conductive via. The first die includes a first dielectric layer and a first landing pad embedded in the first dielectric layer. The second die includes a second dielectric layer and a second landing pad embedded in the second dielectric layer. The first die is disposed on the second die. The second landing pad has a through-hole. The first conductive via extends from the first landing pad toward the second landing pad and penetrates through the through-hole of the second landing pad.

ELECTRONIC CIRCUIT FOR A HYBRID MOLECULAR BONDING

An electronic circuit including a surface intended to be attached to another electronic circuit by hybrid molecular bonding. The electronic circuit includes an electrically-insulating layer exposed on the surface, and, distributed in the electrically-insulating layer, first electrically-conductive bonding pads exposed on a first portion of the surface, the density of the first bonding pads on the first portion of the surface being smaller than 30%, and at least one electrically-conductive test pad, exposed on a second portion of the surface containing a square having a side length greater than 30 μm. The density of electrically-conductive material of the test pad exposed on the second portion of the surface is in the range from 40% to 80%.

CHEMICAL BONDING METHOD AND JOINED STRUCTURE

The present invention achieves chemical bonding by means of a joined film made of oxides formed on a joined surface. In a vacuum container, amorphous oxide thin films are respectively formed on smooth surfaces of two substrates, and the two substrates overlap such that the amorphous oxide thin films formed on the two substrates come into contact with each other, thereby causing chemical bonding involving an atomic diffusion at a joined interface between the amorphous oxide thin films to join the two substrates.

CHEMICAL MECHANICAL POLISHING FOR HYBRID BONDING

Representative implementations of techniques and methods include chemical mechanical polishing for hybrid bonding. The disclosed methods include depositing and patterning a dielectric layer on a substrate to form openings in the dielectric layer, depositing a barrier layer over the dielectric layer and within a first portion of the openings, and depositing a conductive structure over the barrier layer and within a second portion of the openings not occupied by the barrier layer, at least a portion of the conductive structure in the second portion of the openings coupled or contacting electrical circuitry within the substrate. Additionally, the conductive structure is polished to reveal portions of the barrier layer deposited over the dielectric layer and not in the second portion of the openings. Further, the barrier layer is polished with a selective polish to reveal a bonding surface on or at the dielectric layer.