H01L2224/32501

Solder alloy and junction structure using same

A solder alloy, includes: about 3 wt % to about 15 wt % of Sb; about 0.01 wt % to about 1.5 wt % of Te; and about 0.005 wt % to about 1 wt % of at least one element selected from the group consisting of Zn, Co, and Cr; and a balance of Sn.

Member for semiconductor device

A member for semiconductor device includes a metal portion configured to be bonded to another member by solder, and a treated coating covering a surface of the metal portion, the treated coating including a treatment agent. The treated coating vaporizes at a temperature lower than or equal to a solidus temperature of the solder.

Metal Bumps and Method Forming Same

A method of forming an integrated circuit structure includes forming a patterned passivation layer over a metal pad, with a top surface of the metal pad revealed through a first opening in the patterned passivation layer, and applying a polymer layer over the patterned passivation layer. The polymer layer is substantially free from N-Methyl-2-pyrrolidone (NMP), and comprises aliphatic amide as a solvent. The method further includes performing a light-exposure process on the polymer layer, performing a development process on the polymer layer to form a second opening in the polymer layer, wherein the top surface of the metal pad is revealed to the second opening, baking the polymer, and forming a conductive region having a via portion extending into the second opening.

Semiconductor package and method

In an embodiment, a device includes: a first redistribution structure including a first dielectric layer; a die adhered to a first side of the first redistribution structure; an encapsulant laterally encapsulating the die, the encapsulant being bonded to the first dielectric layer with first covalent bonds; a through via extending through the encapsulant; and first conductive connectors electrically connected to a second side of the first redistribution structure, a subset of the first conductive connectors overlapping an interface of the encapsulant and the die.

Metal bumps and method forming same

A method of forming an integrated circuit structure includes forming a patterned passivation layer over a metal pad, with a top surface of the metal pad revealed through a first opening in the patterned passivation layer, and applying a polymer layer over the patterned passivation layer. The polymer layer is substantially free from N-Methyl-2-pyrrolidone (NMP), and comprises aliphatic amide as a solvent. The method further includes performing a light-exposure process on the polymer layer, performing a development process on the polymer layer to form a second opening in the polymer layer, wherein the top surface of the metal pad is revealed to the second opening, baking the polymer, and forming a conductive region having a via portion extending into the second opening.

SEMICONDUCTOR DEVICES

A semiconductor device includes a first adsorption layer, a first bonding layer, a second bonding layer, and a second adsorption layer stacked on a first substrate, and a conductive pattern structure penetrating through the first adsorption layer, the first bonding layer, the second bonding layer and the second adsorption layer. The first and second bonding layers are in contact with each other, and each of the first and second adsorption layers includes a low-K dielectric material.

Power Semiconductor Device and Manufacturing Method

A power semiconductor device is proposed. The power semiconductor device includes a semiconductor substrate. The power semiconductor device further includes an electrically conducting first layer. At least part of the electrically conducting first layer includes pores. The power semiconductor device further includes an electrically conducting second layer. The electrically conducting second layer is arranged between the semiconductor substrate and the electrically conducting first layer. The pores are at least partially filled with a phase change material.

Chip Structure, Wafer Structure And Method For Manufacturing The Same

A chip structure, a wafer structure and a method for manufacturing the same are provided in the present disclosure. A first chip and a second chip are bonded by bonding layers of a dielectric material. Top wiring layers are led out through bonding via holes from a back surface of a bonded chip. The bonding via holes are used for bonding and are surrounded by the bonding layers. A top wiring layer of a third chip is led out through bonding pads formed in a bonding layer. The bonding via holes are aligned with and bonded to the bonding pads to achieve bonding of the three chips. The top wiring layer of the third chip is led out from the back surface of the third chip through a lead-out pad.

Multi-layered composite bonding materials and power electronics assemblies incorporating the same

A multilayer composite bonding material for transient liquid phase bonding a semiconductor device to a metal substrate includes thermal stress compensation layers sandwiched between a pair of bonding layers. The thermal stress compensation layers may include a core layer with a first stiffness sandwiched between a pair of outer layers with a second stiffness that is different than the first stiffness such that a graded stiffness extends across a thickness of the thermal stress compensation layers. The thermal stress compensation layers have a melting point above a sintering temperature and the bonding layers have a melting point below the sintering temperature. The graded stiffness across the thickness of the thermal stress compensation layers compensates for thermal contraction mismatch between the semiconductor device and the metal substrate during cooling from the sintering temperature to ambient temperature.

SEMICONDUCTOR APPARATUS WITH HIGH-STABILITY BONDING LAYER AND PRODUCTION METHOD THEREOF

In an embodiment, a semiconductor apparatus comprises: a semiconductor chip, a substrate, and a bonding layer located between the semiconductor chip and the substrate that bonds the semiconductor chip and the substrate, wherein the bonding layer comprises sintered metal that comprises a plurality of voids, and wherein at least a portion of the plurality of voids are filled with a specific material having fluidity at a temperature higher than a preset temperature and is curable after being heated and melted.