H01L2224/48507
Cu ALLOY CORE BONDING WIRE WITH Pd COATING FOR SEMICONDUCTOR DEVICE
A bonding wire for a semiconductor device includes a Cu alloy core material and a Pd coating layer formed on a surface thereof, and the boding wire contains one or more elements of As, Te, Sn, Sb, Bi and Se in a total amount of 0.1 to 100 ppm by mass. The bonding longevity of a ball bonded part can increase in a high-temperature and high-humidity environment, improving the bonding reliability. When the Cu alloy core material further contains one or more of Ni, Zn, Rh, In, Ir, Pt, Ga and Ge in an amount, for each, of 0.011 to 1.2% by mass, it is able to increase the reliability of a ball bonded part in a high-temperature environment of 170 C. or more. When an alloy skin layer containing Au and Pd is further formed on a surface of the Pd coating layer, wedge bondability improves.
Semiconductor device and method for fabricating the same
A method for fabricating a semiconductor device includes providing a semiconductor die, arranging an electrical connector over the semiconductor die, the electrical connector including a conductive core, an absorbing feature arranged on a first side of the conductive core, and a solder layer arranged on a second side of the conductive core, opposite the first side and facing the semiconductor die, and soldering the electrical connector onto the semiconductor die by heating the solder layer with a laser, wherein the laser irradiates the absorbing feature and absorbed energy is transferred from the absorbing feature through the conductive core to the solder layer.
SEMICONDUCTOR PACKAGE SUBSTRATE WITH A SMOOTH GROOVE ABOUT A PERIMETER OF A SEMICONDUCTOR DIE
A semiconductor package includes a metallic pad and leads spaced from the metallic pad by a gap, the metallic pad including a roughened surface. The semiconductor package further includes a semiconductor die including bond pads, and an adhesive between the roughened surface of the metallic pad and the semiconductor die, therein bonding the semiconductor die to the metallic pad, wherein the adhesive includes a resin. The metallic pad further includes a groove surrounding the semiconductor die on the roughened surface, the groove having a surface roughness less than a surface roughness of the roughened surface of the metallic pad.
Cu alloy core bonding wire with Pd coating for semiconductor device
A bonding wire for a semiconductor device includes a Cu alloy core material and a Pd coating layer formed on a surface thereof, and the boding wire contains one or more elements of As, Te, Sn, Sb, Bi and Se in a total amount of 0.1 to 100 ppm by mass. The bonding longevity of a ball bonded part can increase in a high-temperature and high-humidity environment, improving the bonding reliability. When the Cu alloy core material further contains one or more of Ni, Zn, Rh, In, Ir, Pt, Ga and Ge in an amount, for each, of 0.011 to 1.2% by mass, it is able to increase the reliability of a ball bonded part in a high-temperature environment of 170 C. or more. When an alloy skin layer containing Au and Pd is further formed on a surface of the Pd coating layer, wedge bondability improves.
Bonding wire for semiconductor device
There is provided a bonding wire for a semiconductor device including a coating layer having Pd as a main component on a surface of a Cu alloy core material and a skin alloy layer containing Au and Pd on a surface of the coating layer, the bonding wire further improving 2nd bondability on a Pd-plated lead frame and achieving excellent ball bondability even in a high-humidity heating condition. The bonding wire for a semiconductor device including the coating layer having Pd as a main component on the surface of the Cu alloy core material and the skin alloy layer containing Au and Pd on the surface of the coating layer has a Cu concentration of 1 to 10 at % at an outermost surface thereof and has the core material containing either or both of Pd and Pt in a total amount of 0.1 to 3.0% by mass, thereby achieving improvement in the 2nd bondability and excellent ball bondability in the high-humidity heating condition. Furthermore, a maximum concentration of Au in the skin alloy layer is preferably 15 at % to 75 at %.
Chip package and method of forming a chip package with a metal contact structure and protective layer, and method of forming an electrical contact
In various embodiments, a chip package is provided. The chip package may include a chip, a metal contact structure including a non-noble metal and electrically contacting the chip, a packaging material, and a protective layer including or essentially consisting of a portion formed at an interface between a portion of the metal contact structure and the packaging material, wherein the protective layer may include a noble metal, wherein the portion of the protective layer may include a plurality of regions free from the noble metal, and wherein the regions free from the noble metal may provide an interface between the packaging material and the non-noble metal of the metal contact structure.
BONDING WIRE FOR SEMICONDUCTOR DEVICE
The present invention provides a bonding wire for a semiconductor device suitable for cutting-edge high-density LSIs and on-vehicle LSIs by improving the formation rate of CuAl IMC in ball bonds. A bonding wire for a semiconductor device contains Pt of 0.1 mass % to 1.3 mass %, at least one dopant selected from a first dopant group consisting of In, Ga, and Ge, for a total of 0.05 mass % to 1.25 mass %, and a balance being made up of Cu and incidental impurities.
Silver bonding wire for semiconductor device containing indium, gallium, and/or cadmium
The present invention provides a bonding wire which can satisfy bonding reliability, spring performance, and chip damage performance required in high-density packaging. A bonding wire contains one or more of In, Ga, and Cd for a total of 0.05 to 5 at %, and a balance being made up of Ag and incidental impurities.
Cu ALLOY CORE BONDING WIRE WITH Pd COATING FOR SEMICONDUCTOR DEVICE
A bonding wire for a semiconductor device includes a Cu alloy core material and a Pd coating layer formed on a surface thereof, and the boding wire contains one or more elements of As, Te, Sn, Sb, Bi and Se in a total amount of 0.1 to 100 ppm by mass. The bonding longevity of a ball bonded part can increase in a high-temperature and high-humidity environment, improving the bonding reliability. When the Cu alloy core material further contains one or more of Ni, Zn, Rh, In, Ir, Pt, Ga and Ge in an amount, for each, of 0.011 to 1.2% by mass, it is able to increase the reliability of a ball bonded part in a high-temperature environment of 170 C. or more. When an alloy skin layer containing Au and Pd is further formed on a surface of the Pd coating layer, wedge bondability improves.
Power Semiconductor Chip, Method for Producing a Power Semiconductor Chip, and Power Semiconductor Device
A power semiconductor chip having: a semiconductor component body; a multilayer metallization arranged on the semiconductor component body; and a nickel layer arranged over the semiconductor component body. The invention further relates to a method for producing a power semiconductor chip and to a power semiconductor device. The invention provides a power semiconductor chip which has a metallization to which a copper wire, provided without a thick metallic coating, can be reliably bonded without damage to the power semiconductor chip during bonding.