B32B2038/166
MANUFACTURING PROCEDURE FOR CEILING TRIMS FOR VEHICLES
A manufacturing procedure for ceiling trims for vehicles, the structure of which comprises at least one first coating sheet and at least one second coating sheet that extend along one of the sides of the first sheet, joined via a layer of heat-stable polyurethane adhesive, comprising a step of applying a gas-phase catalyst on such sheets through a thermoforming mould that starts before the mould is completely closed and ends before the mould is completely opened. As a result of said application of a gas-phase catalyst we prevent the use of demoulding agents to facilitate extraction of the ceiling trim formed inside the mould.
WORKPIECE BONDING METHOD
Provided is a workpiece bonding method that makes it possible to achieve a joining state with a high strength and to obtain a good repeatability of the joining state.
A workpiece bonding method according to the present invention is a workpiece bonding method for bonding two workpieces to each other, each of the two workpieces being composed of a material selected from the group consisting of synthetic resin, glass, silicon wafer, crystal and sapphire, the workpiece bonding method including: a surface activation step of activating a bonded surface of at least one of the workpieces; and a laminating step of laminating the two workpieces such that respective bonded surfaces contact with each other, and a pretreatment step of removing moisture from the bonded surface of the workpiece that is to be subjected to the surface activation step is performed before the surface activation step is performed.
Scent sampler and air freshener
A scent sampler and air freshener has a wafer of an absorbent resilient material infused with a liquid containing a scent. The wafer is encapsulated in a chamber formed between two panels of sheet material with edges sealed together to form an envelope. An opening in one of the panels enables scent from the liquid to be emitted to the ambient atmosphere. The rate of emission can be increased by squeezing the panels to compress the wafer. The interior surfaces of the panels can be coated with a barrier film to prevent leakage of the liquid from contaminating the sheet material.
Lightweight thermal shield
A method of making a lightweight thermal shield that includes obtaining a mold having a shaped support screen with a molding surface configured to allow the passage of air and moisture therethrough, and with the mold being adapted for drawing a vacuum from behind the support screen. The method also includes applying a wet insulation material onto the molding surface of the support screen and drawing a vacuum to withdraw moisture through the support screen and consolidate a layer of insulation material on top the molding surface. The method further includes removing the consolidated layer of insulation material from off the molding surface, installing the consolidated layer of insulation material into an outer shell layer, and drying the consolidated layer of insulation material within the outer shell layer to form a lightweight core insulation layer.
METHOD FOR MAKING A COATED FABRIC
A method for making a coated fabric includes the steps of: applying a coating solution of a resin in an organic solvent to a roller-conveyed non-stretchable and releasable substrate web to form a coating layer; laminating a roller-conveyed base fabric to the coating layer to form a laminate; guiding the laminate to pass through at least one tank containing water to immerse the laminate in water such that the coating layer is solidified and the organic solvent contained in the coating layer is replaced by water; and removing water from the coating layer by drying to leave micropores in the coating layer.
METHOD OF MANUFACTURING A TIMBER COMPOSITE, THE TIMBER COMPOSITE OBTAINED AND DECORATIVE PANELS COMPRISING SUCH TIMBER COMPOSITE
A decorative panel including a substrate material and a decorative top layer, wherein the decorative top layer includes at least one timber layer with a wood structure, wherein the timber layer is a compressed timber layer with naturally occurring vessels throughout a thickness of the wood structure, the vessels being collapsed.
Method for Upgrading and Embossing Leather
A method for making an upgraded and embossed laminar supporting element, in particular leather, by applying several layers on the surface of the leather, including an aqueous base coat and a lacquer coat and partially removing water and/or solvent from said layers followed by embossing and optionally further drying.
Method of manufacturing a timber composite, the timber composite obtained and decorative panels comprising such timber composite
A decorative panel including a substrate material and a decorative top layer. The decorative top layer is formed by at least one timber layer penetrated with a cured adhesive, and the timber layer has a wood structure with collapsed vessels having opposed walls, the opposed walls being glued together permanently by the cured adhesive.
METHOD OF MANUFACTURING A TIMBER COMPOSITE, THE TIMBER COMPOSITE OBTAINED AND DECORATIVE PANELS COMPRISING SUCH TIMBER COMPOSITE
A decorative panel including a substrate material and decorative top layer, wherein the decorative top layer includes at least one timber layer, wherein the timber layer is a compressed timber layer with a permanent increased density as compared to an original timber layer, wherein the decorative panel is a square or rectangular floor panel which, at, at least one pair of opposite edges, or at both pairs, includes mechanical coupling allowing to couple two of such floor panels to each other such that a locking is created in a vertical direction perpendicular to a plane of the coupled panels, as well as in a horizontal direction perpendicular to a coupled edge and in the plane of the coupled panels, the mechanical coupling being in the substrate material.
Flour binder for gypsum board, and related methods, product, and slurries
Disclosed is an acid-modified flour and a method of making the acid-modified flour. The acid-modified flour is desirably prepared using a dry milling process. A starting flour is combined with a strong acid to form a mixture. The mixture is heated. A neutralizer is added to increase the pH of the mixture. If desired, the mixture can be dried and any agglomerates can be removed. The acid-modified flour can be used as a binder in a slurry for preparing one or more gypsum layers in a gypsum board.