Patent classifications
C08J9/32
Epoxy based reinforcing patches having improved damping loss factor
A reinforcing sheet including one or more layers of a reinforcing material, and a thermosetting adhesive associated with the reinforcing material, wherein the thermosetting adhesive includes a curing agent, and an epoxy-modified dimerized fatty acid combined with an epoxy terminated polyurethane interpenetrating network.
Process for forming polylactide expanded bead foam
Expanded poly(lactide) (PLA) beads are made by pressurizing PLA beads with carbon dioxide at approximately room temperature, heating the beads under pressure to 90 to 160 C to saturate and partially crystallize the beads, and then depressurizing and cooling the beads. The PLA beads contain a blend of PLLA and PDLA in certain ratios. The beads are useful for making expanded bead foam.
AROMATIC POLYESTER POLYETHER POLYURETHANE PANELS AND USEFUL MATERIALS COMPRISING SAME
This abstract is intended as a scanning tool for purposes of searching in the particular art and is not intended to be limiting of the present disclosure. The disclosure provides aromatic polyester polyether polyols and compositions comprising such polyols. The disclosed aromatic polyester polyether polyols and compositions including same are the products of the transesterification reaction of polyethylene terephthalate (“PET”) and an ethoxylated triol, namely glycerin or trimethylolpropane, wherein the degree of ethoxylation is from 1 to 9 moles. At least some of the PET used to generate the aromatic polyester polyether polyols is derived from recycled PET. The disclosed aromatic polyester polyether polyols have utility in preparing polyurethane materials, for example.
AROMATIC POLYESTER POLYETHER POLYURETHANE PANELS AND USEFUL MATERIALS COMPRISING SAME
This abstract is intended as a scanning tool for purposes of searching in the particular art and is not intended to be limiting of the present disclosure. The disclosure provides aromatic polyester polyether polyols and compositions comprising such polyols. The disclosed aromatic polyester polyether polyols and compositions including same are the products of the transesterification reaction of polyethylene terephthalate (“PET”) and an ethoxylated triol, namely glycerin or trimethylolpropane, wherein the degree of ethoxylation is from 1 to 9 moles. At least some of the PET used to generate the aromatic polyester polyether polyols is derived from recycled PET. The disclosed aromatic polyester polyether polyols have utility in preparing polyurethane materials, for example.
Polymer matrix composites comprising dielectric particles and methods of making the same
A polymer matrix composite comprising a porous polymeric network; and a plurality of dielectric particles distributed within the polymeric network structure; wherein the dielectric particles are present in a range from 5 to 98 weight percent, based on the total weight of the dielectric particles and the polymer (excluding the solvent); and wherein the polymer matrix composite has a dielectric constant in a range from 1.05 to 80; and methods for making the same. Polymer matrix composites comprising dielectric particles are useful, for example, as electric field insulators.
Super absorbent polymer and method for preparing same
The present invention relates to a super absorbent polymer. The super absorbent polymer contains polymer particles formed of large pores in a certain amount or more, and thus can exhibit large surface area and excellent initial absorption capacity. Therefore, when the super absorbent polymer is used, it can provide a sanitary material such as a diaper or a sanitary napkin which can quickly absorb body fluids and impart a dry and soft touch feeling.
Microwave and electromagnetic heated foaming method, mold and foaming material thereof
Present invention is related to a microwave and electromagnetic heated foaming method, mold and foaming material thereof. The microwave and electromagnetic heated foaming method comprises steps of adding a foam material into a mold, simultaneously applying a microwave and electromagnetic energy toward the mold under a normal or low pressure, and the microwave and electromagnetic energy made the foam material into molded foam body. The mold of the present invention has a microwave penetrating part and an electromagnetic heating part. The microwave penetrating part has an extruded bottom that is corresponded to a dented top of the electromagnetic heat penetrating part. By utilizing the microwave and electromagnetic energy, the present invention is about to provide an efficient way for processing the foaming material compared to the conventional infrared or electrical heated tube heating and achieve the foam method that can be executed under normal or low pressure.
FOAMABLE POLYOLEFIN COMPOSITION PROVIDING INCREASED FLEXIBILITY
The invention relates to a foamable polymer composition comprising a polyolefin polymer which polyolefin polymer does not bear silane moieties and comprises 20 to 99.99 wt. % linear low density polyethylene, and a blowing agent in an amount of 0.01 to 3 wt. % based on the total foamable polymer composition, wherein the blowing agent consists of citric acid and/or derivatives of citric acid or mixtures thereof. Further the invention relates to a foamable polymer composition comprising a polyolefin polymer, and a blowing agent in an amount of 0.01 to 3 wt. % based on the total foamable polymer composition, wherein the blowing agent consists of expandable polymeric microspheres, and the composition does not comprise fluororesin. Further the invention relates to a foamed polymer composition obtained by foaming this foamable polymer composition. Further the invention relates to the use of the foamable composition or the foamed polymer composition for a layer of a cable and a cable comprising at least one layer which comprises the
FOAMABLE POLYOLEFIN COMPOSITION PROVIDING INCREASED FLEXIBILITY
The invention relates to a foamable polymer composition comprising a polyolefin polymer which polyolefin polymer does not bear silane moieties and comprises 20 to 99.99 wt. % linear low density polyethylene, and a blowing agent in an amount of 0.01 to 3 wt. % based on the total foamable polymer composition, wherein the blowing agent consists of citric acid and/or derivatives of citric acid or mixtures thereof. Further the invention relates to a foamable polymer composition comprising a polyolefin polymer, and a blowing agent in an amount of 0.01 to 3 wt. % based on the total foamable polymer composition, wherein the blowing agent consists of expandable polymeric microspheres, and the composition does not comprise fluororesin. Further the invention relates to a foamed polymer composition obtained by foaming this foamable polymer composition. Further the invention relates to the use of the foamable composition or the foamed polymer composition for a layer of a cable and a cable comprising at least one layer which comprises the
Porous polyurethane polishing pad and preparation method thereof
Embodiments relate to a porous polyurethane polishing pad for use in a chemical mechanical planarization (CMP) process of semiconductors and a process for producing the same. In the porous polyurethane polishing pad, it is possible to control the size and distribution of pores, whereby the polishing performance (i.e., polishing rate) of the polishing pad can be adjusted, by way of employing thermally expanded microcapsules as a solid phase foaming agent and an inert gas as a gas phase foaming agent.