C01F7/021
Method for producing metal oxide-containing particles, and method for producing aggregates of metal oxide colloidal particles
A method for producing particles containing a metal oxide is provided, and the method includes: feeding a metal oxide sol having a pH of 7 or higher and containing metal oxide colloidal particles as dispersoids and water as a dispersion medium, into a liquid containing a solvent having a solubility in 20 C. water of 0.05 g/100 ml or more and having a relative permittivity of 30 or lower (protic solvent) or of 40 or lower (aprotic solvent) at 20 C., and thereby forming aggregates of the metal oxide colloidal particles in the liquid; and subjecting the aggregates to a treatment such as drying and heating, and thereby converting the aggregates into particles that are insoluble in water. By appropriately selecting the solvent, particles can be obtained in the form of flakes, fibers, spheres, and the like.
LASER-COLORED SAPPHIRE MATERIAL
A colored sapphire material and methods for coloring sapphire material using lasers are disclosed. The method for coloring the sapphire material may include positioning the sapphire material over an opaque substrate material, exposing the opaque substrate material to a laser beam passing through the sapphire material to impact the substrate material, and inducing a chemical change in a portion of the sapphire material exposed to the laser beam. The method may also include creating a visible color in the portion of the sapphire material as a result of the chemical change. The colored sapphire material may include a first transparent portion, and a second, colored portion substantially surrounded by the first portion. The second, colored portion may have a chemical composition different than that of the first portion.
TREATMENT METHOD FOR MODIFYING THE REFLECTED COLOUR OF A SAPPHIRE MATERIAL SURFACE
A treatment method for modifying the reflected colour of a sapphire material surface comprising bombardment by a single- and/or multi-charged gas ion beam so as to modify the reflected colour of the treated sapphire material surface, wherein the ions are selected from ions of the elements from the list consisting of helium (He), neon (Ne), argon (Ar), krypton (Kr), xenon (Xe), boron (B), carbon (C), nitrogen (N), oxygen (O), fluorine (F), silicon (Si), phosphorus (P) and sulphur (S).
TRANSPARENT CERAMIC WITH COMPLEX GEOMETRY
A ceramic product includes a transparent ceramic panel having a non-planar geometry including a bend having a slippage plane, an increased haze, a non-uniform thickness, or a combination thereof. A method includes providing a transparent ceramic panel, heating the panel, bending the panel to conform to a non-planar geometry.
SINGLE- AND/OR MULTI-CHARGED GAS ION BEAM TREATMENT METHOD FOR PRODUCING AN ANTI-GLARE SAPPHIRE MATERIAL
A treatment method of a sapphire material, said method comprising bombardment of a surface of the sapphire material, said surface facing a medium different from the sapphire material, by a single- and/or multi-charged gas ion beam so as to produce an ion implanted layer in the sapphire material, wherein the ions are selected from ions of the elements from the list consisting of helium (He), neon (Ne), argon (Ar), krypton (Kr), xenon (Xe), boron (B), carbon (C), nitrogen (N), oxygen (O), fluorine (F), silicon (Si), phosphorus (P) and sulphur (S). Use of said method to obtain a capacitive touch panel having a high transmission in the visible range.
Method of surface modification of alumina
A method of surface modification of an alumina carrier. The method includes: 1) dissolving a soluble kazoe in deionized water to yield a kazoe aqueous solution; 2) submerging an alumina carrier in the kazoe aqueous solution and drying the alumina carrier in a vacuum environment; 3) placing the dried alumina carrier in a reactor, adding silicon tetrachloride and Grignard reagent dropwise to the reactor, sealing the reactor and heating it to a constant temperature, and maintaining the constant temperature for between 3 and 18 hours, where a volume ratio of the added silicon tetrachloride and the alumina carrier is between 0.5:1 and 5:1, the constant temperature is controlled to be between 160 and 350 C.; and 4) cooling the reactor, filtering, washing, and drying the alumina carrier in the vacuum environment.
Burner for producing inorganic spheroidized particles, apparatus for producing inorganic spheroidized particles, and method for producing inorganic spheroidized particles
One object of the present invention is to provide a burner for producing inorganic spheroidized particles which can efficiently melt and spheroidize even organic powder with a large particle size distribution. The present invention provides a burner for producing inorganic spheroidized particles, including; a raw material powder supply path configured to supply inorganic powder as raw material powder; a first fuel gas supply path (3A) configured to supply a first fuel gas; and a first combustion-supporting gas supply path (4A) configured to supply a first combustion-supporting gas; wherein the raw material powder supply path includes: a first supply path (2A) configured to extend in an axial direction of the burner (1); a first collision wall (2D) configured to be located at the top of the first supply path (2A); a plurality of second supply paths (2B) configured to be branched from the top of the first supply path (2A), and extend radially from the center of the burner (1); one or more dispersion chambers (2C) configured to be located at the top of the second supply path (2B), and have a space in which the cross-sectional area is larger than the cross-sectional area in the second supply path (2B); and one or more raw material ejection holes (2a) configured to communicate with the dispersion chamber (2C).
Burner for producing inorganic spheroidized particles, apparatus for producing inorganic spheroidized particles, and method for producing inorganic spheroidized particles
One object of the present invention is to provide a burner for producing inorganic spheroidized particles which can efficiently melt and spheroidize even organic powder with a large particle size distribution. The present invention provides a burner for producing inorganic spheroidized particles, including; a raw material powder supply path configured to supply inorganic powder as raw material powder; a first fuel gas supply path (3A) configured to supply a first fuel gas; and a first combustion-supporting gas supply path (4A) configured to supply a first combustion-supporting gas; wherein the raw material powder supply path includes: a first supply path (2A) configured to extend in an axial direction of the burner (1); a first collision wall (2D) configured to be located at the top of the first supply path (2A); a plurality of second supply paths (2B) configured to be branched from the top of the first supply path (2A), and extend radially from the center of the burner (1); one or more dispersion chambers (2C) configured to be located at the top of the second supply path (2B), and have a space in which the cross-sectional area is larger than the cross-sectional area in the second supply path (2B); and one or more raw material ejection holes (2a) configured to communicate with the dispersion chamber (2C).
Method for Processing Packaging Material
The subject of the present invention is a method for processing metallized packaging materials, especially beverage cartons, or blister packaging.
According to the invention, the aluminum is dissolved with the aid of acid and separated from the plastic. The metal-containing acid solution then undergoes pyrohydrolytic treatment and the acid is thus recovered. The aluminum can be recovered as valuable aluminum oxide.
LASER-COLORED SAPPHIRE MATERIAL
A colored sapphire material and methods for coloring sapphire material using lasers are disclosed. The method for coloring the sapphire material may include positioning the sapphire material over an opaque substrate material, exposing the opaque substrate material to a laser beam passing through the sapphire material to impact the substrate material, and inducing a chemical change in a portion of the sapphire material exposed to the laser beam. The method may also include creating a visible color in the portion of the sapphire material as a result of the chemical change. The colored sapphire material may include a first transparent portion, and a second, colored portion substantially surrounded by the first portion. The second, colored portion may have a chemical composition different than that of the first portion.