C08F222/06
MALEIMIDE COPOLYMER, METHOD FOR PRODUCING SAME, RESIN COMPOSITION AND INJECTION MOLDED BODY
A maleimide based copolymer, manufacturing method thereof, and a resin composition using the maleimide based copolymer is provided. The maleimide based copolymer includes 40 to 60 mass % of aromatic vinyl monomer unit, 5 to 20 mass % of vinyl cyanide monomer unit, 35 to 50 mass % of maleimide monomer unit, and 0 to 10 mass % of monomer copolymerizable with these monomer units. The maleimide based copolymer has a glass transition temperature of 165° C. or higher and a melt mass flow rate of 25 to 80 g/10 min measured at 265° C. with 98 N load. By using such maleimide based copolymer, flowability can be improved without decreasing heat resistance providing ability.
MALEIMIDE COPOLYMER, METHOD FOR PRODUCING SAME, RESIN COMPOSITION AND INJECTION MOLDED BODY
A maleimide based copolymer, manufacturing method thereof, and a resin composition using the maleimide based copolymer is provided. The maleimide based copolymer includes 40 to 60 mass % of aromatic vinyl monomer unit, 5 to 20 mass % of vinyl cyanide monomer unit, 35 to 50 mass % of maleimide monomer unit, and 0 to 10 mass % of monomer copolymerizable with these monomer units. The maleimide based copolymer has a glass transition temperature of 165° C. or higher and a melt mass flow rate of 25 to 80 g/10 min measured at 265° C. with 98 N load. By using such maleimide based copolymer, flowability can be improved without decreasing heat resistance providing ability.
Polypropylene resin composition and monolayer and multilayer film
A propylene polymer satisfying (a) below, a soft propylene copolymer satisfying (b) below, and a polyolefin containing a structural unit derived from an unsaturated carboxylic acid and/or a derivative thereof, wherein (a) a melting point is 100° C. or more, and (b) an MFR is in the range of 0.01 to 100 g/10 min, at least one of the following requirements (b-1) and (b-2) is satisfied: (b-1) a syndiotactic triad fraction s 60% or more, and (b-2) a structural unit derived from propylene is 55 to 90 mol % and a structural unit derived from at least one olefin having 2 to 20 carbon atoms (excluding propylene) is contained at 10 to 45 mol % (with provisos), and the relation between an intrinsic viscosity [η] (dL/g) and the MFR satisfies the relation: 1.50×MFR.sup.−0.20≤[η]≤2.65×MFR.sup.−0.20.
Polypropylene resin composition and monolayer and multilayer film
A propylene polymer satisfying (a) below, a soft propylene copolymer satisfying (b) below, and a polyolefin containing a structural unit derived from an unsaturated carboxylic acid and/or a derivative thereof, wherein (a) a melting point is 100° C. or more, and (b) an MFR is in the range of 0.01 to 100 g/10 min, at least one of the following requirements (b-1) and (b-2) is satisfied: (b-1) a syndiotactic triad fraction s 60% or more, and (b-2) a structural unit derived from propylene is 55 to 90 mol % and a structural unit derived from at least one olefin having 2 to 20 carbon atoms (excluding propylene) is contained at 10 to 45 mol % (with provisos), and the relation between an intrinsic viscosity [η] (dL/g) and the MFR satisfies the relation: 1.50×MFR.sup.−0.20≤[η]≤2.65×MFR.sup.−0.20.
Thermoplastic resin composition including maleimide-based heat-resistant copolymer and molded product using same
This disclosure relates to a thermoplastic resin composition comprising (A) 60 to 85 wt % of a (meth)acrylic resin, (B) 10 to 30 wt % of an acrylic graft copolymer, and (C) 5 to 10 wt % of a maleimide-based heat-resistant copolymer and a molded product using the same.
Thermoplastic resin composition including maleimide-based heat-resistant copolymer and molded product using same
This disclosure relates to a thermoplastic resin composition comprising (A) 60 to 85 wt % of a (meth)acrylic resin, (B) 10 to 30 wt % of an acrylic graft copolymer, and (C) 5 to 10 wt % of a maleimide-based heat-resistant copolymer and a molded product using the same.
POLYAMIDE COMPOSITION
A polyamide composition excellent in balance between fluidity during molding and, for example, surface appearance, bleed-out resistance, impact resistance and rigidity in the form of a molded article, and also relates to a polyamide composition a polyamide (A), an ethylene/α-olefin copolymer (B) satisfying requirements (b-1) to (b-3), and 0.1 to 20.0 mass % of an ethylene/α-olefin copolymer (C) satisfying the requirements (c-1) to (c-5), provided that (A)+(B)+(C)=100 mass %.
POLYAMIDE COMPOSITION
A polyamide composition excellent in balance between fluidity during molding and, for example, surface appearance, bleed-out resistance, impact resistance and rigidity in the form of a molded article, and also relates to a polyamide composition a polyamide (A), an ethylene/α-olefin copolymer (B) satisfying requirements (b-1) to (b-3), and 0.1 to 20.0 mass % of an ethylene/α-olefin copolymer (C) satisfying the requirements (c-1) to (c-5), provided that (A)+(B)+(C)=100 mass %.
Unsaturated Polyester Resin Compositions and Methods for Preparation Thereof
The invention relates to an unsaturated polyester resin composition comprising: —a (meth)acrylate compound; and, —a polyester formed from at least: —reagent a) comprising itaconic acid and/or itaconic anhydride; —reagent b) comprising maleic acid, maleic anhydride, and/or fumaric acid; —reagent c) comprising dicyclopentadiene (DCPD); and, —reagent d) comprising at least one di- or poly-functional alcohol, preferably at least one diol; wherein the combined weight of reagent a) (i.e. the combined weight of itaconic acid and/or itaconic anhydride) is at least 10 wt. %, preferably at least 20 wt. %, of the total weight of di-acids and anhydrides used in the unsaturated polyester resin composition. The invention further relates to use of said unsaturated polyester resin for structural parts and for gel-coats. The invention also provides methods for preparing said unsaturated polyester resin composition.
Unsaturated Polyester Resin Compositions and Methods for Preparation Thereof
The invention relates to an unsaturated polyester resin composition comprising: —a (meth)acrylate compound; and, —a polyester formed from at least: —reagent a) comprising itaconic acid and/or itaconic anhydride; —reagent b) comprising maleic acid, maleic anhydride, and/or fumaric acid; —reagent c) comprising dicyclopentadiene (DCPD); and, —reagent d) comprising at least one di- or poly-functional alcohol, preferably at least one diol; wherein the combined weight of reagent a) (i.e. the combined weight of itaconic acid and/or itaconic anhydride) is at least 10 wt. %, preferably at least 20 wt. %, of the total weight of di-acids and anhydrides used in the unsaturated polyester resin composition. The invention further relates to use of said unsaturated polyester resin for structural parts and for gel-coats. The invention also provides methods for preparing said unsaturated polyester resin composition.