Homogenization and heat-treatment of cast metals
A method of casting a metal ingot with a microstructure that facilitates further working, such as hot and cold rolling. The metal is cast in a direct chill casting mold, or the equivalent, that directs a spray of coolant liquid onto the outer surface of the ingot to achieve rapid cooling. The coolant is removed from the surface at a location where the emerging embryonic ingot is still not completely solid, such that the latent heat of solidification and the sensible heat of the molten core raises the temperature of the adjacent solid shell to a convergence temperature that is above a transition temperature for in-situ homogenization of the metal. A further conventional homogenization step is then not required. The invention also relates to the heat-treatment of such ingots prior to hot working.
Process and apparatus for minimizing the potential for explosions in the direct chill casting of lithium alloys
An apparatus and a system including a casting pit; a mold including a reservoir and a cavity; a coolant feed operable to introduce a coolant to a periphery of a metal emerging from the mold cavity; an array of water vapor exhaust ports about at least the top periphery of the casting pit; a mechanism to introduce an inert fluid into the coolant feed. A method for a direct chill casting including, after detecting a bleed out, exhausting generated gas from the casting pit at a flow volume rate that is enhanced relative to a flow volume rate prior to detecting bleed out or run out; introducing an inert gas into the casting pit; and introducing an inert fluid into a coolant feed to the casting mold.
PROCESS AND APPARATUS FOR MINIMIZING THE POTENTIAL FOR EXPLOSIONS IN THE DIRECT CHILL CASTING OF LITHIUM ALLOYS
An apparatus and a system including a casting pit; a mold including a reservoir and a cavity; a coolant feed operable to introduce a coolant to a periphery of a metal emerging from the mold cavity; an array of water vapor exhaust ports about at least the top periphery of the casting pit; a mechanism to introduce an inert fluid into the coolant feed. A method for a direct chill casting including, after detecting a bleed out, exhausting generated gas from the casting pit at a flow volume rate that is enhanced relative to a flow volume rate prior to detecting bleed out or run out; introducing an inert gas into the casting pit; and introducing an inert fluid into a coolant feed to the casting mold.
Process and apparatus for minimizing the potential for explosions in the direct chill casting of lithium alloys
An apparatus and a system including a casting pit; a mold including a reservoir and a cavity; a coolant feed operable to introduce a coolant to a periphery of a metal emerging from the mold cavity; an array of water vapor exhaust ports about at least the top periphery of the casting pit; a mechanism to introduce an inert fluid into the coolant feed. A method for a direct chill casting including, after detecting a bleed out, exhausting generated gas from the casting pit at a flow volume rate that is enhanced relative to a flow volume rate prior to detecting bleed out or run out; introducing an inert gas into the casting pit; and introducing an inert fluid into a coolant feed to the casting mold.
Process and apparatus for direct chill casting
A system comprising at least one furnace including a melt containing vessel; an intermediate casting product station coupled to the at least one furnace and operable to receive a molten metal from the at least one furnace, the intermediate casting product station including a casting pit, at least one moveable platen disposed in the casting pit, an array of exhaust ports about at least a top periphery of the casting pit, and an array of gas introduction ports about at least the top periphery of the casting pit; and an inert gas source operable to supply an inert gas to the array of gas introduction ports.
PROCESS AND APPARATUS FOR MINIMIZING THE POTENTIAL FOR EXPLOSIONS IN THE DIRECT CHILL CASTING OF LITHIUM ALLOYS
An apparatus and a system including a casting pit; a mold including a reservoir and a cavity; a coolant feed operable to introduce a coolant to a periphery of a metal emerging from the mold cavity; an array of water vapor exhaust ports about at least the top periphery of the casting pit; a mechanism to introduce an inert fluid into the coolant feed. A method for a direct chill casting including, after detecting a bleed out, exhausting generated gas from the casting pit at a flow volume rate that is enhanced relative to a flow volume rate prior to detecting bleed out or run out; introducing an inert gas into the casting pit; and introducing an inert fluid into a coolant feed to the casting mold.
Process and apparatus for minimizing the potential for explosions in the direct chill casting of aluminum lithium alloys
An apparatus and a system including a casting pit; a mold including a reservoir and a cavity; a coolant feed operable to introduce a coolant to a periphery of a metal emerging from the mold cavity; an array of water vapor exhaust ports about at least the top periphery of the casting pit; a mechanism to introduce an inert fluid into the coolant feed. A method for a direct chill casting including, after detecting a bleed out, exhausting generated gas from the casting pit at a flow volume rate that is enhanced relative to a flow volume rate prior to detecting bleed out or run out; introducing an inert gas into the casting pit; and introducing an inert fluid into a coolant feed to the casting mold.