B23K35/0255

Systems and methods for low-manganese welding alloys

Systems and methods for low-manganese welding alloys are disclosed. An example arc welding consumable may comprise: less than 0.4 wt % manganese; strengthening agents selected from the group consisting of nickel, cobalt, copper, carbon, molybdenum, chromium, vanadium, silicon, and boron; and grain control agents selected from the group consisting of niobium, tantalum, titanium, zirconium, and boron. The grain control agents may comprise greater than 0.06 wt % and less than 0.6 wt % of the welding consumable. The resulting weld deposit may comprise a tensile strength greater than or equal to 70 ksi, a yield strength greater than or equal to 58 ksi, a ductility (as measured by percent elongation) of at least 22%, and a Charpy V-notch toughness greater than or equal to 20 ft-lbs at −20° F. The welding consumable may provide a manganese fume generation rate less than 0.01 grams per minute during the arc welding operation.

FLUID-COOLED CONTACT TIP ASSEMBLY FOR METAL WELDING
20180014397 · 2018-01-11 ·

Provided is a fluid-cooled contact tip assembly that can be used in methods and systems for manufacturing objects by solid freeform fabrication, especially titanium and titanium alloy objects, where the deposition rate is increased by increasing the flow rate of electric charge through the metal wire.

Method for the manufacturing of liquid metal embrittlement resistant zinc coated steel sheet

The present invention relates to a method for the manufacture of a coated steel sheet comprising the following successive steps: A. the coating of the steel sheet with a first coating consisting of nickel and having a thickness between 600 nm and 1400 nm, the steel sheet having the following composition in weight: 0.10<C<0.40%, 1.5<Mn<3.0%, 0.7<Si<3.0%, 0.05<Al<1.0%, 0.75<(Si+Al)<3.0%, and on a purely optional basis, one or more elements such as Nb≤0.5%, B≤0.010%, Cr≤1.0%, Mo≤0.50%, Ni≤1.0%, Ti≤0.5%, the remainder of the composition making up of iron and inevitable impurities resulting from the elaboration, B. the recrystallization annealing at a temperature between 820 to 1200° C., C. the coating with a second coating based on zinc not comprising nickel.

LAMINATE INCLUDING ALUMINUM SHEETS
20230015873 · 2023-01-19 · ·

A laminate structure and method of forming is provided. The laminate structure includes a first metal sheet having a first thickness, a second metal sheet having a second thickness, and an adhesive core having an adhesive thickness. The adhesive core is disposed between and bonded to the first and second metal sheets. The first and second metal sheets are made of an aluminum based material and the adhesive core is made of an adhesive material also described as a viscoelastic adhesive material. The laminate structure is configured such that a ratio of the sum of the first and second thickness to the adhesive thickness is greater than either to one (8:1). The laminate structure including the viscoelastic adhesive core is characterized by a composite loss factor at 1,000 Hertz which is continuously greater than 0.1 within a temperature range of 25 degrees Celsius to 50 degrees Celsius.

Laminated molding and method of manufacturing laminated molding

An additively manufactured object formed by depositing weld bead layers, each of the weld bead layers being obtained by melting and solidifying a filler metal made of a mild steel, the additively manufactured object includes a plurality of the weld bead layers having a ferrite phase with an average grain diameter of 11 μm or less in a part except for a surface oxide film.

SYSTEM AND METHOD OF MANUFACTURING A RESISTANCE SPOT WELD OF WORKPIECES
20220355410 · 2022-11-10 ·

A system for increasing joint strength and reducing embrittlement in a resistance spot weld of metal workpieces is disclosed. The system comprises a stackup of first and second metal workpieces, and an interface member disposed between the first and second metal workpieces. The interface member comprises a peripheral wall defining a hollow inner portion. The peripheral wall has a first open end extending to a second open end. The first open end is in contact with the first metal workpiece defining a first weld portion thereon. The second open end is in contact with the second metal workpiece defining a second weld portion thereon. The system further comprises a first electrode configured to contact the first metal workpiece to heat the peripheral wall at the first weld portion and join the first metal workpiece with the first open end of the peripheral wall. The system further comprises a second electrode configured to contact the second metal workpiece to heat the peripheral wall at the second weld portion and join the second metal workpiece with the second open end of the peripheral wall to define a weld joint. The system further comprises a power source configured to power the first and second electrodes and a controller configured to control the power to the first and second electrodes to heat the peripheral wall.

Suppressors and their methods of manufacture
11493297 · 2022-11-08 · ·

A suppressor having a body and a first connector half coupled to the body, wherein the first connector half includes a first component that includes at least one channel and a first surface; and wherein the body provides a second surface, wherein a gap between the first surface and the second surface defines at least one track; wherein the gun includes a second connector half comprising at least one protrusion, wherein the protrusion and channel have corresponding shapes that allow the protrusion to be inserted through the channel and into alignment with the track, wherein the first component may be rotated with respect to the protrusion and the body to bring the protrusion out of alignment with the channel so that the first and second surfaces clamp the protrusion to thereby secure the first connector half and second connector half with respect to each other.

Additive manufacturing of metal matrix composite feedstock

A feedstock for an additive manufacturing process includes a pre-ceramic polymer intermixed with a base material. A method of additive manufacturing includes melting and pyrolizing a feedstock containing metal and a pre-ceramic polymer. An article of manufacture includes an additive manufacturing component including a pyrolized feedstock.

Laminate including weldable regions

A laminate sheet including a weldable margin is formed by laminating metal sheets having a core layer disposed therebetween. The core layer is formed of a core material which includes one or more of a viscoelastic, adhesive and acoustic material. The core layer is selectively distributed such that the laminate sheet includes an adhered region providing a laminate structure, and a non-adhered region including a weldable margin. The non-adhered region is adjacent an edge of the core layer and is characterized by a gap between the first and second metal sheets and by an absence of the core layer in the gap. The non-adhered region defines a weldable margin adjacent a core edge configured such that a weld is formable in the weldable margin without heat affecting the core layer. The laminate sheet can be joined by fasteners installed in the non-adhered region.

Exothermic reaction welding molds, weld-metal containing cartridges for such molds, and methods of use

Exothermic welding molds, weld-metal containing cartridges for such molds, and methods of use are provided. The mold, cartridges, and methods can provide interaction between the cartridge's disk member with the mold, which allows the housing member to be withdrawn from the mold while leaving the disk member and weld-metal in place. The interaction can be a rotational restraint alone, a vertical restraint alone, or combinations thereof. Alternately, the interaction can be an outward pressure on the housing member and/or disk member, a shear force on the housing member and/or disk member, or combinations thereof. The outward pressure on the housing member and/or disk member can alternately be provided without interaction between the disk member and the mold, but rather by the simple application of an internal pressure to the cartridge. The internal pressure can be applied by squeezing the walls of the cartridge and/or by depressing a pusher member.