B29C65/026

Low permeability and high strength woven fabric and methods of making the same
11634841 · 2023-04-25 · ·

A method for producing a woven fabric comprises weaving fibers in a warp direction and a weft direction to form a fabric having a top surface and a bottom surface, wherein the warp fibers and weft fibers each comprises one or more filaments of a synthetic polymer having substantially uniform cross-sectional composition. At least a portion of the filaments in the fibers on the top and/or bottom surface of the fabric are then fused together in the presence of a heat transfer liquid or vapor added during the fusing step or added in a prior step of the fabric production process and retained by the filaments. The fusing step produces a treated fabric having a tensile strength in both the warp and weft directions of 1000 N or greater and having, in the absence of any coating, a static air permeability (SAP) of 3 l/dm.sup.2/min or lower.

Method for the production of a pacifier teat
10875253 · 2020-12-29 · ·

Method for the production of a pacifier teat and pacifier teat with a suction section forming a cavity, to which suction section a shaft adjoins, wherein an elastic hollow body having suction section and the shaft is pre-formed in an injection or in a dipping process and opposite wall sections of the pre-formed hollow body are connected with each other in the region of the shaft.

LOW PERMEABILITY AND HIGH STRENGTH WOVEN FABRIC AND METHODS OF MAKING THE SAME
20200063298 · 2020-02-27 · ·

A method for producing a woven fabric comprises weaving fibers in a warp direction and a weft direction to form a fabric having a top surface and a bottom surface, wherein the warp fibers and weft fibers each comprises one or more filaments of a synthetic polymer having substantially uniform cross-sectional composition. At least a portion of the filaments in the fibers on the top and/or bottom surface of the fabric are then fused together in the presence of a heat transfer liquid or vapor added during the fusing step or added in a prior step of the fabric production process and retained by the filaments. The fusing step produces a treated fabric having a tensile strength in both the warp and weft directions of 1000 N or greater and having, in the absence of any coating, a static air permeability (SAP) of 3 l/dm.sup.2/min or lower.

SYSTEM AND METHOD OF CONSTRUCTING A THERMOPLASTIC COMPONENT

Systems and methods of constructing a thermoplastic component include joining a thermoplastic skin to a thermoplastic core by introducing heat at an interface of each of the thermoplastic skin and the thermoplastic core to at least partially melt the thermoplastic skin to a thermoplastic core at the interfaces, applying pressure to at least one of the thermoplastic skin and the thermoplastic core to sandwich the elements, and cooling the interfaces below the melting point of each of the thermoplastic skin and the thermoplastic core to consolidate the thermoplastic skin and the thermoplastic core into a unitary thermoplastic component. An optional thermoplastic film may be disposed between the thermoplastic skin and the thermoplastic core. The thermoplastic skin may be joined to the thermoplastic core to form an intermediate thermoplastic component prior to joining the thermoplastic skin to the intermediate component.

Method for adhering parts and device for implementing said method

A method is provided of bonding together at least two parts. The method includes assembling together at least two parts and at least one adhesive layer, the adhesive being configured so that its adhesive power increases on heating as a result of it polymerizing, at least one of the parts being made of composite material or of metal, the adhesive layer being present, after assembly, between the parts, the assembled together parts and the adhesive being present in a chamber defined by a wall, the wall having an inside face situated facing a first part present between the adhesive layer and the wall, the first part being intended to be bonded to a second part and only a fraction of the second part being present inside the chamber; and applying a liquid against the wall on its side opposite from the chamber.

METHOD FOR ADHERING PARTS AND DEVICE FOR IMPLEMENTING SAID METHOD
20170001366 · 2017-01-05 · ·

A method is provided of bonding together at least two parts. The method includes assembling together at least two parts and at least one adhesive layer, the adhesive being configured so that its adhesive power increases on heating as a result of it polymerizing, at least one of the parts being made of composite material or of metal, the adhesive layer being present, after assembly, between the parts, the assembled together parts and the adhesive being present in a chamber defined by a wall, the wall having an inside face situated facing a first part present between the adhesive layer and the wall, the first part being intended to be bonded to a second part and only a fraction of the second part being present inside the chamber; and applying a liquid against the wall on its side opposite from the chamber.