B81C2201/0166

Low-stress low-hydrogen LPCVD silicon nitride

A microelectronic device contains a high performance silicon nitride layer which is stoichiometric within 2 atomic percent, has a low stress of 600 MPa to 1000 MPa, and has a low hydrogen content, less than 5 atomic percent, formed by an LPCVD process. The LPCVD process uses ammonia and dichlorosilane gases in a ratio of 4 to 6, at a pressure of 150 millitorr to 250 millitorr, and at a temperature of 800 C. to 820 C.

LOW-STRESS LOW-HYDROGEN LPCVD SILICON NITRIDE
20170133472 · 2017-05-11 ·

A microelectronic device contains a high performance silicon nitride layer which is stoichiometric within 2 atomic percent, has a low stress of 600 MPa to 1000 MPa, and has a low hydrogen content, less than 5 atomic percent, formed by an LPCVD process. The LPCVD process uses ammonia and dichlorosilane gases in a ratio of 4 to 6, at a pressure of 150 millitorr to 250 millitorr, and at a temperature of 800 C. to 820 C.

Low-stress low-hydrogen LPCVD silicon nitride

A microelectronic device contains a high performance silicon nitride layer which is stoichiometric within 2 atomic percent, has a low stress of 600 MPa to 1000 MPa, and has a low hydrogen content, less than 5 atomic percent, formed by an LPCVD process. The LPCVD process uses ammonia and dichlorosilane gases in a ratio of 4 to 6, at a pressure of 150 millitorr to 250 millitorr, and at a temperature of 800 C. to 820 C.