C01B39/52

Carbon-based clathrate compounds

The present invention provides carbon-based clathrate compounds, including a carbon-based clathrate compound that includes a clathrate lattice with atoms of at least one element selected from the group consisting of carbon and boron as a host cage structure; guest atoms encapsulated within the clathrate lattice; and, substitution atoms that may be substituted for at least one portion of the carbon and boron atoms that constitute the clathrate lattice. In one embodiment, the invention provides a carbon-based clathrate compound of the formula LaB.sub.3C.sub.3.

SHEET-LIKE PARTICLES OF ZEOLITE AND METHOD FOR PRODUCING SAME

The invention provides a method for producing sheet-like particles of zeolite that cannot be obtained by a top-down method, and provides sheet-like particles of zeolite having an 8-membered oxygen ring structure obtained by the method. A thickness of the sheet-like particles is 1 nm to 100 nm, and an aspect ratio (maximum width/thickness in particles) of the sheet-like particles is 100 or more.

CARBON-BASED CLATHRATE COMPOUNDS
20230147042 · 2023-05-11 · ·

The present invention provides carbon-based clathrate compounds, including a carbon-based clathrate compound that includes a clathrate lattice with atoms of at least one element selected from the group consisting of carbon and boron as a host cage structure; guest atoms encapsulated within the clathrate lattice; and, substitution atoms that may be substituted for at least one portion of the carbon and boron atoms that constitute the clathrate lattice. In one embodiment, the invention provides a carbon-based clathrate compound of the formula LaB.sub.3C.sub.3.

ZEOLITE AND PREPARATION METHOD THEREFOR
20220033269 · 2022-02-03 ·

Disclosed is a method of producing zeolite that includes obtaining a lithium residue including aluminosilicate from lithium ore including lithium oxide; washing the lithium residue to adjust the pH of the lithium residue; adjusting a molar ratio of silicon to aluminum (Si/Al) included in the lithium residue; preparing a hydrogel by adding an alkali material to the lithium residue; and preparing crystals by crystallizing the lithium residue in the form of a hydrogel.

PROCESS FOR THE PREPARATION OF ZEOLITES ENCAPSULATING TRANSITION METAL NANOPARTICLES FROM LAYERED SILICATE PRECURSORS
20210370277 · 2021-12-02 · ·

The present invention relates to a process for the production of a transition metal containing zeolite comprising expanding a layered silicate with a swelling agent and introducing the transition metal into the interlayer expanded silicate prior to calcination thereof for obtaining the transition metal containing zeolite. The present invention further relates to a zeolite containing transition metal nanoparticles as obtainable or obtained according to the inventive process, as well as to a zeolite containing nanoparticles per se. Finally the present invention relates to the use of a zeolite containing transition metal nanoparticles as obtainable or obtained according to the inventive process, as well as to the use of a zeolite containing nanoparticles per se.

Platinum encapsulated zeolite hydrocracking catalyst and methods of making same
11745170 · 2023-09-05 · ·

Embodiments of the present disclosure are directed to hydrocracking catalysts and methods of making same. The hydrocracking catalyst comprises a platinum encapsulated zeolite having a crystallinity greater than 20% determined by X-ray powder diffraction analysis.

Platinum encapsulated zeolite hydrocracking catalyst and methods of making same
11745170 · 2023-09-05 · ·

Embodiments of the present disclosure are directed to hydrocracking catalysts and methods of making same. The hydrocracking catalyst comprises a platinum encapsulated zeolite having a crystallinity greater than 20% determined by X-ray powder diffraction analysis.

Amphiphobic porous materials

A variety of amphiphobic porous materials are provided. The materials can include a variety of porous frameworks that have an outer surface functionalized by a plurality of perfluoroalkyl moieties. By careful selection of appropriate perfluoralkyl moieties, hydrophobic properties can be imparted to the exterior surface of the porous materials without significantly impacting the wetting properties of the porous interior. This can be used to create a variety of highly amphiphobic porous materials. Methods of making and using the amphiphobic porous materials are also provided.

PLATINUM ENCAPSULATED ZEOLITE HYDROCRACKING CATALYST AND METHODS OF MAKING SAME
20210237042 · 2021-08-05 · ·

Embodiments of the present disclosure are directed to hydrocracking catalysts and methods of making same. The hydrocracking catalyst comprises a platinum encapsulated zeolite having a crystallinity greater than 20% determined by X-ray powder diffraction analysis.

PLATINUM ENCAPSULATED ZEOLITE HYDROCRACKING CATALYST AND METHODS OF MAKING SAME
20210237042 · 2021-08-05 · ·

Embodiments of the present disclosure are directed to hydrocracking catalysts and methods of making same. The hydrocracking catalyst comprises a platinum encapsulated zeolite having a crystallinity greater than 20% determined by X-ray powder diffraction analysis.