Patent classifications
C01F7/0633
Use of Calcium Fluoride in the Bayer Process
A Bayer process includes contacting bauxite and calcium fluoride with sodium hydroxide and forming a slurry, with the calcium fluoride may provide at least 1 wt. % of the calcium added to the process, and precipitating alumina from the slurry.
Use of Calcium Fluoride in the Bayer Process
A Bayer process includes contacting bauxite and calcium fluoride with sodium hydroxide and forming a slurry, with the calcium fluoride may provide at least 1 wt. % of the calcium added to the process, and precipitating alumina from the slurry.
PURIFICATION OF ORES USING BORONIC ACID-FUNCTIONAL COMPOUNDS
Described herein is a method of adding one or more boronic acid functional compounds to a mineral ore to result in a treated mineral ore. Where the mineral ore is a bauxite ore, and the ore is subsequently processed according to the Bayer process to obtain alumina, adding a boronic acid functional compound to the bauxite ore or a Bayer product followed by processing the treated bauxite ore or treated Bayer product using one or more processes associated with the Bayer process results in an increased yield of alumina product, increased alumina content (purity) in the alumina product obtained, or both when compared to the same bauxite ore or Bayer product subjected to the same process(es) but in the absence of a boronic acid functional compound.
METHODS AND COMPOSITIONS FOR BAUXITE BENEFICIATION
Disclosed herein are methods and compositions for increasing the alumina content of a bauxite ore prior to alumina extraction by an extractive process, such as the Bayer process. By adding a beneficiation agent to an aqueous ore slurry, then applying a gravitational force to separate, or partition, the slurry into a beneficiary and a gangue, a number of quantifiable benefits are observed. These include increased alumina content and reduced silica content in the beneficiary solids as compared to the starting ore. These benefits are in excess of those observed by pre-extraction gravitational separation of ore slurries without the addition of a beneficiation agent. Beneficiation agents include DADMAC polymers, and combinations of DADMAC polymers with dextrans. The beneficiary is collected and applied to an extractive process, such as the Bayer process.
Surfactant based small molecules for reducing aluminosilicate scale in the Bayer process
The invention provides methods and compositions for inhibiting the accumulation of DSP scale in the liquor circuit of Bayer process equipment. The method includes adding one or more GPS-surfactant based small molecules to the liquor fluid circuit. These scale inhibitors reduce DSP scale formation and thereby increase fluid throughput, increase the amount of time Bayer process equipment can be operational and reduce the need for expensive and dangerous acid washes of Bayer process equipment. As a result, the invention provides a significant reduction in the total cost of operating a Bayer process.
Reducing aluminosilicate scale in the Bayer process
The invention provides a method of inhibiting the accumulation of DSP scale in the liquor circuit of Bayer process equipment. The method includes adding one or more particular silane based small molecules to the liquor fluid circuit. These scale inhibitors reduce DSP scale formation and thereby increase fluid throughput, increase the amount of time Bayer process equipment can be operational and reduce the need for expensive and dangerous acid washes of Bayer process equipment. As a result, the invention provides a significant reduction in the total cost of operating a Bayer process.
Purification of ores using boronic acid-functional compounds
Described herein is a method of adding one or more boronic acid functional compounds to a mineral ore to result in a treated mineral ore. Where the mineral ore is a bauxite ore, and the ore is subsequently processed according to the Bayer process to obtain alumina, adding a boronic acid functional compound to the bauxite ore or a Bayer product followed by processing the treated bauxite ore or treated Bayer product using one or more processes associated with the Bayer process results in an increased yield of alumina product, increased alumina content (purity) in the alumina product obtained, or both when compared to the same bauxite ore or Bayer product subjected to the same process(es) but in the absence of a boronic acid functional compound.
Surfactant Based Small Molecules for Reducing Aluminosilicate Scale in the Bayer Process
The invention provides methods and compositions for inhibiting the accumulation of DSP scale in the liquor circuit of Bayer process equipment. The method includes adding one or more GPS-surfactant based small molecules to the liquor fluid circuit. These scale inhibitors reduce DSP scale formation and thereby increase fluid throughput, increase the amount of time Bayer process equipment can be operational and reduce the need for expensive and dangerous acid washes of Bayer process equipment. As a result, the invention provides a significant reduction in the total cost of operating a Bayer process.
Reducing Aluminosilicate Scale in the Bayer Process
The invention provides a method of inhibiting the accumulation of DSP scale in the liquor circuit of Bayer process equipment. The method includes adding one or more particular silane based small molecules to the liquor fluid circuit. These scale inhibitors reduce DSP scale formation and thereby increase fluid throughput, increase the amount of time Bayer process equipment can be operational and reduce the need for expensive and dangerous acid washes of Bayer process equipment. As a result, the invention provides a significant reduction in the total cost of operating a Bayer process.
Use of calcium fluoride in the bayer process
A Bayer process includes contacting bauxite and calcium fluoride with sodium hydroxide and forming a slurry, with the calcium fluoride may provide at least 1 wt. % of the calcium added to the process, and precipitating alumina from the slurry.