Patent classifications
C03B2201/36
APPARATUS FOR OPTICAL FIBER MANUFACTURING PROCESS
An apparatus for optical fiber manufacturing process is provided, including a raw material providing structure, a dopant providing structure, and a preform forming substrate tube. The dopant providing structure is disposed at a downstream side of the raw material providing structure and in communication with the raw material providing structure. The dopant providing structure includes an outer tube, a first inner tube, a first dopant providing container, a second inner tube, and a second dopant providing container. The first inner tube is disposed in the outer tube. The first dopant providing container is disposed in the first inner tube. The second inner tube is disposed in the outer tube at a downstream of the first inner tube. The second dopant providing container is disposed in the second inner tube. The preform forming substrate tube is disposed at a downstream side of the dopant providing structure.
Method and apparatus for producing a glass component
In known methods for producing a glass component, a void-containing intermediate product containing doped or non-doped SiO.sub.2 is inserted into a sheath tube composed of glass, which has a longitudinal axis and an inner bore, and is thermally treated therein. In order to subject the intermediate product to a thermal and/or reactive treatment that is reproducible and uniform in its effect from this starting point, it is proposed in one embodiment that into the sheath tube's inner bore a first gas-permeable gas diffuser is inserted which is displaceable along the sheath tube's longitudinal axis and is pressed against the intermediate product during the thermal treatment.
RADIATION-RESISTANT LASER OPTICAL FIBER PREFORM CORE ROD AND PREPARATION METHOD THEREFOR
A radiation-resistant laser optical fiber preform core rod at least includes one type of activated ion (Yb.sup.3+, Er.sup.3+) and one or more types of co-doped ion (Al.sup.3+, P.sup.5+, Ge.sup.4+, Ce.sup.3+, F.sup.−), and —OD group of 16-118 ppm. Irradiation resistance of core rod glass can be effectively improved by sequentially performing pre-treatments, i.e. deuterium loading, pre-irradiation and thermal annealing on a preform core rod. Electron paramagnetic resonance test shows that, under the same radiation condition, the radiation induced color center concentration in a preform core rod treated by the method above is lower than in an untreated core rod by one or more orders of magnitude. The obtained core rod can be used for preparing a radiation-resistant rare earth-doped silica fiber, and has the advantages of high laser slope efficiency, low background loss, being able to be used stably in a vacuum environment for a long time, for example.
RARE EARTH METAL-DOPED QUARTZ GLASS AND METHOD FOR PRODUCING THE SAME
A method for producing rare earth metal-doped quartz glass includes the steps of (a) providing a blank of the rare earth metal-doped quartz glass, and (b) homogenizing the blank by softening the blank zone by zone in a heating zone and by twisting the softened zone along a rotation axis. Some rare earth metals, however, show a discoloration of the quartz glass, which hints at an unforeseeable and undesired change in the chemical composition or possibly at an inhomogeneous distribution of the dopants. To avoid this drawback and to provide a modified method which ensures the production of rare earth metal-doped quartz glass with reproducible properties, during homogenization according to method step (b), the blank is softened under the action of an oxidizingly acting or a neutral plasma.
Apparatus for optical fiber manufacturing process
An apparatus for optical fiber manufacturing process is provided, including a raw material providing structure, a dopant providing structure, and a preform forming substrate tube. The dopant providing structure is disposed at a downstream side of the raw material providing structure and in communication with the raw material providing structure. The dopant providing structure includes an outer tube, a first inner tube, a first dopant providing container, a second inner tube, and a second dopant providing container. The first inner tube is disposed in the outer tube. The first dopant providing container is disposed in the first inner tube. The second inner tube is disposed in the outer tube at a downstream of the first inner tube. The second dopant providing container is disposed in the second inner tube. The preform forming substrate tube is disposed at a downstream side of the dopant providing structure.
Manufacturing method for optical fiber and manufacturing apparatus for optical fiber
A manufacturing method for an optical fiber, includes: drawing, while heating in a heating furnace, a lower end of an optical fiber preform that is to be an optical fiber having a core consisting of silica glass containing a rare earth element compound. The heating furnace has a temperature profile in which a temperature of the heating furnace increases to a maximum temperature T.sub.max and then decreases from an upstream side of the heating furnace toward a downstream side of the heating furnace. The temperature profile has a changing point at which the temperature decreases more steeply on the downstream side from a position where the maximum temperature T.sub.max is reached. At the maximum temperature, a temperature of the silica glass is higher than or equal to a glass transition temperature and the silica glass is in a single phase.
OPTICAL TUBE WAVEGUIDE LASING MEDIUM AND RELATED METHOD
Laser waveguides, methods and systems for forming a laser waveguide are provided. The waveguide includes an inner cladding layer surrounding a central axis and a glass core surrounding and located outside of the inner cladding layer. The glass core includes a laser-active material. The waveguide includes an outer cladding layer surrounding and located outside of the glass core. The inner cladding, outer cladding and/or core may surround a hollow central channel or bore and may be annular in shape.
Tapered core fiber manufacturing methods
Tapered core fibers are produced using tapered core rods that can be etched or ground so that a fiber cladding has a constant diameter. The tapered core can be an actively doped core, or a passive core. One or more sleeving tubes can be collapsed onto a tapered core rod and exterior portions of the collapsed sleeving tubes can be ground to provide a constant cladding diameter in a fiber drawn from the preform.
SYSTEM AND METHOD FOR OPTICAL FIBER PREFORM PREPARATION VIA HIGH-SURFACE-AREA COATING
The present disclosure relates to a method for forming a glass, ceramic or composite material. The method may involve initially forming a plurality of tubes and then performing a coating operation to coat the plurality of tubes with materials containing metal or metalloid elements, including inorganic compounds, organometallic compounds, or coordination complexes to form coated tubes. The method may further include performing at least one of a thermal operation or a thermochemical operation on the coated tubes to form a solid glass, ceramic, or composite structure with dimensions representing at least one of a rod or fiber.
Photodarkening-resistant ytterbium-doped quartz optical fiber and preparation method therefor
A photodarkening-resistant ytterbium-doped quartz optical fiber and a method for prpearing such a fiber are provided. Glass of a photodarkening-resistant ytterbium-doped quartz optical fiber core rod includes at least Yb.sub.2O.sub.3, Al.sub.2O.sub.3, P.sub.2O.sub.5, SiO.sub.2. The proportions of Yb.sub.2O.sub.3, Al.sub.2O.sub.3, and P.sub.2O.sub.5 in the entire substance are Yb.sub.2O.sub.3: 0.05-0.3 mol %, Al.sub.2O.sub.3: 1-3 mol %, and P.sub.2O.sub.5: 1-5 mol %, respectively. In the preparation method for the photodarkening-resistant ytterbium-doped quartz optical fiber, a sol-gel method and an improved chemical vapor deposition method are combined. By using the molecular-level doping uniformity and the low preparation loss thereof respectively, ytterbium ions, aluminum ions and phosphorus ions are effectively doped in a quartz matrix, thereby effectively solving the problems in the optical fiber of high loss, photodarkening caused by cluster or the like, and a central refractive index dip.