C03B2203/24

COMPOSITE OPTICAL FIBRE BASED PLASMA GENERATION DEVICE

A device for generating a plasma and detecting a light signal. The plasma being intended to be generated in the vicinity of a study area of a sample and the light signal originating in the study area. The device including a current generator, an analysis unit, and an electrical and optical waveguide including means for transmitting an electric current configured to generate a plasma at one end of the means for transmitting the electric current in the vicinity of the study zone, means for detecting and transmitting configured to detect and transmit the light signal from the study area to the analysis unit, and an optical cladding portion, the means for transmitting the electric current and the means for detecting and transmitting the light signal being accommodated in the optical cladding portion.

Quasi-single-mode optical fiber with a large effective area

A quasi-single-mode optical fiber with a large effective area is disclosed. The quasi-single-mode fiber has a core with a radius greater than 5 μm, and a cladding section configured to support a fundamental mode and a higher-order mode. The fundamental mode has an effective area greater than 170 μm.sup.2 and an attenuation of no greater than 0.17 dB/km at a wavelength of 1530 nm. The higher-order mode has an attenuation of at least 1.0 dB/km at the wavelength of 1530 nm. The quasi-single-mode optical fiber has a bending loss of less than 0.02 dB/turn for a bend diameter of 60 mm for a wavelength of 1625 nm.

Multi-core optical fiber ribbons and methods for making the same
09796618 · 2017-10-24 · ·

Multi-core optical fiber ribbons and methods for making multi-core optical fiber ribbons are described herein. In one embodiment, a multi-core optical fiber ribbon includes at least two core members formed from silica-based glass and oriented in parallel with one another in a single plane. Adjacent core members have a center-to-center spacing ≧15 microns and a cross-talk between adjacent core members is ≦−25 dB. In this embodiment each core member is single-moded with an index of refraction n.sub.c, and a core diameter d.sub.c. In an alternative embodiment, each core member is multi-moded and the center-to-center spacing between adjacent core members is ≧25 microns. A single cladding layer is formed from silica-based glass and surrounds and is in direct contact with the core members. The single cladding layer is substantially rectangular in cross section with a thickness ≦400 microns and an index of refraction n.sub.cl<n.sub.c.

METHODS OF MAKING AN OPTICAL FIBER, AND OPTICAL FIBER

According to some embodiments a method of processing an optical fiber comprises the steps of: (i) drawing the fiber at a drawing rate of at least 30 m/sec; and (ii) cooling the drawn fiber in a gas at an average cooling rate less than 5000° C./s, such that said cooling reduces the temperature of the fiber from an entering temperature in the range between 1500° C. and 1700° C. to another temperature in the range between 1200° C. and 1400° C., the gas being at a temperature between 800° C. and 1500° C.; and the thermal conductivity κ of the gas being not greater than 1.5×10.sup.−4 cal/cm-s-K for at least one temperature within a range of 800° C. to 1500° C. at one atm (atmosphere) pressure absolute.

OPTICAL FIBER PREFORM, OPTICAL FIBER, AND METHOD OF MANUFACTURING OPTICAL FIBER
20170285259 · 2017-10-05 · ·

An optical fiber preform includes: a core formed of silica glass which does not contain Ge, wherein the core has at least one of characteristics in spectrometry of (1) an absorption peak is present at a wavelength of 240 nm to 255 nm, and (2) a wavelength at which an ultraviolet transmittance is 50% or lower is longer than 170 nm.

Optical fibers and preforms with one step fluorine trench and overclad and methods for making the same

A method is provided that includes: forming a low-index trench region with a first density; forming an inner barrier layer comprising silica around the trench region at a second density greater than the first density; depositing silica-based soot around the first barrier layer to form an overclad region at a third density less than the second density; inserting a core cane into a trench-overclad structure; forming an outer barrier layer comprising silica in an outer portion of the overclad region at a fourth density greater than the third density; flowing a down dopant-containing gas through the trench-overclad structure to dope the trench region with the down dopant, and wherein the barrier layers mitigate diffusion of the down-dopant into the overclad region; and consolidating the trench-overclad and the core cane.

LOW ATTENUATION FIBER WITH STRESS RELIEVING LAYER AND A METHOD OF MAKING SUCH
20170235045 · 2017-08-17 ·

A single mode optical fiber having a core made from silica and less than or equal to about 11 weight % germania and having a maximum relative refractive index Δ.sub.1MAX. The optical fiber also has an inner cladding surrounding the core and having a minimum relative refractive index Δ.sub.2MIN, a first outer cladding surrounding the inner cladding and a second outer cladding surrounding the first outer cladding. The viscosity at 1650° C. of the second outer cladding minus the viscosity at 1650° C. of the first outer cladding is greater than 0.1e.sup.7 Poise, and Δ.sub.1MAX>Δ.sub.2MIN. The single mode optical fiber may also have an outer cladding surrounding the inner cladding made from silica or SiON. The first outer cladding has a maximum relative refractive index Δ.sub.3MAX, and Δ.sub.3MAX>Δ.sub.2MIN.

High chlorine content low attenuation optical fiber

An optical fiber having a core comprising silica and greater than 1.5 wt % chlorine and less than 0.5 wt % F, said core having a refractive index Δ.sub.1MAX, and an inner cladding region having refractive index Δ.sub.2MIN surrounding the core, where Δ.sub.1MAX>Δ.sub.2MIN.

OPTICAL FIBER PREFORM
20220009816 · 2022-01-13 ·

The present invention provides an optical fiber with improved optical properties such as zero dispersion wavelength by suppressing the volatilization of dopant materials such as germanium dioxide and optimizing the refractive index distribution by adjusting the setting position of the core portion burner for deposition in a larger optical fiber preform. An optical fiber preform includes a core portion with a relatively high refractive index and a clad portion with a relatively low refractive index, wherein a position having a value of 45% of a refractive index difference between a center of the core portion and the clad portion is a boundary rcore (mm) between the core portion and the clad portion; and when a radius position r at which a refractive index difference with the clad portion being a maximum value is rside (mm), r.sub.side/rcore is 0.745 to 1.

Method for manufacturing a preform for optical fibers

The present invention relates to a method for manufacturing a preform for optical fibers, which method comprises the sequential steps of: i) deposition of non-vitrified silica layers on the inner surface of a hollow substrate tube; ii) deposition of vitrified silica layers inside the hollow substrate tube on the inner surface of the non-vitrified silica layers deposited in step i); iii) removal of the hollow substrate tube from the vitrified silica layers deposited in step ii) and the non-vitrified silica layers deposited in step i) to obtain a deposited tube; iv) optional collapsing said deposited tube obtained in step iii) to obtain a deposited rod comprising from the periphery to the center at least one inner optical cladding and an optical core; v) preparation of an intermediate layer by the steps of: * deposition of non-vitrified silica layers on the outside surface of the deposited tube obtained in step iii) or deposited rod obtained in step iv) with a flame hydrolysis process in an outer reaction zone using glass-forming precursors, and subsequently; * drying and consolidating said non-vitrified silica layers into a vitrified fluorine-doped silica intermediate cladding layer; and * in case preceding step iv) was omitted collapsing; to provide a solid rod comprising from the periphery to the center the intermediate layer, at least one inner optical cladding and an optical core; wherein a fluorine-comprising gas is used during the deposition and/or drying and/or consolidating and wherein the intermediate layer has a ratio between the outer diameter of the intermediate cladding layer (C) to the outer diameter of the optical core (A) that is at least 3.5; vi) deposition of natural silica on the outside surface of the intermediate cladding layer of the solid rod obtained in step v) by melting natural silica particles in an outer deposition zone to produce an outer cladding whereby a preform is obtained.