Patent classifications
C04B2103/603
Concrete compositions and methods for producing same
This present invention relates to compositions to improve concrete using biochemical-producing microbes and/or byproducts synthesized by the microbes. The invention also relates to methods for enhancing the performance of the concrete with said microbial strains and/or their byproducts.
Concrete compositions and methods for producing same
This present invention relates to compositions to improve concrete using biochemical-producing microbes and/or byproducts synthesized by the microbes. The invention also relates to methods for enhancing the performance of the concrete with said microbial strains and/or their byproducts.
ALKALI-SILICA MITIGATION ADMIXTURE, METHODS OF MAKING AND KITS COMPRISING THE SAME
The present invention relates in part to an alkali-silica reaction mitigation admixture comprising an organic or inorganic salt that provides an aluminum, calcium, magnesium, or iron cation. The present invention also relates to a method of mitigating the alkali-silica reaction in a concrete product. The invention is further related to kits comprising the alkali-silica mitigation admixture and an instruction booklet.
CONCRETE FORMULATION FOR SEALING AND PLUGGING OIL OR GAS WELLS FOR ABANDONMENT
An improved oil or gas well cement for penetrating, sealing and plugging wells to be abandoned. The cement fill includes (a) a cement component including a calcium sulfoaluminate cement and a Portland cement having a ratio by weight of Portland cement to calcium sulfoaluminate cement ranging from 1/19 to ⅕ and (b) an aggregate component with gradation spanning 1,200 microns to 5 microns. Further an improved oil or gas well microcellular cement for penetrating sealing and completely filling wells to be abandoned that includes (a) a cement component including a calcium sulfoaluminate cement and a Portland cement having a ratio by weight of Portland cement to calcium sulfoaluminate cement ranging from 1/19 to ⅕ and (b) an aggregate component with gradation spanning 200 microns to 5 microns and (c) a foaming agent.
Liquid coloring suspension and colored cementitious composition
A colored cementitious composition is provided that is composed of hydraulic cement and a liquid coloring suspension. The liquid coloring suspension for cementitious compositions contains polycarboxylate dispersant, pigment, and a polysaccharide thixotropic additive. The liquid coloring suspension has improved viscosity consistency, improved shelf-life, anti-settling and anti-sludging properties, and decreased polycarboxylate dispersant requirements.
Liquid coloring suspension and colored cementitious composition
A colored cementitious composition is provided that is composed of hydraulic cement and a liquid coloring suspension. The liquid coloring suspension for cementitious compositions contains polycarboxylate dispersant, pigment, and a polysaccharide thixotropic additive. The liquid coloring suspension has improved viscosity consistency, improved shelf-life, anti-settling and anti-sludging properties, and decreased polycarboxylate dispersant requirements.
CEMENTITIOUS COMPOSITIONS WITH ACCELERATED CURING AT LOW TEMPERATURES
A cementitious composition with accelerated curing at low temperatures particularly at temperatures <5° C., especially at temperatures <0° C. The cementitious composition consists of 2 components with a first component A including at least one ordinary Portland cement, at least one cement selected from calcium aluminate cement and/or calcium sulfoaluminate cement, a powder P, selected from the group consisting of carbonates or hydrogen carbonates of alkali and/or alkaline earth metals, optionally aggregates, optionally other additives and a second component B comprising at least one accelerator, an anti-freeze agent, water, and optionally other additives. The composition shows increased development of compressive strength, maintain good workability, and have particularly low shrinkage, also when cured at temperatures <5° C., especially <0° C., and as low as −10° C.
CEMENTITIOUS COMPOSITIONS WITH ACCELERATED CURING AT LOW TEMPERATURES
A cementitious composition with accelerated curing at low temperatures particularly at temperatures <5° C., especially at temperatures <0° C. The cementitious composition consists of 2 components with a first component A including at least one ordinary Portland cement, at least one cement selected from calcium aluminate cement and/or calcium sulfoaluminate cement, a powder P, selected from the group consisting of carbonates or hydrogen carbonates of alkali and/or alkaline earth metals, optionally aggregates, optionally other additives and a second component B comprising at least one accelerator, an anti-freeze agent, water, and optionally other additives. The composition shows increased development of compressive strength, maintain good workability, and have particularly low shrinkage, also when cured at temperatures <5° C., especially <0° C., and as low as −10° C.
IMPROVED GEOPOLYMER CEMENT
The present invention provides a geopolymer cement, comprising: a geopolymer binder; and a setting control composition comprising: a viscosity control agent, a polymeric binder, and a retarding additive. The invention also relates to a geopolymer concrete comprising the geopolymer cement of the invention and aggregate material. The invention further relates to a method for controlling open time in a geopolymer composition, wherein a sufficient quantity of the setting control composition is added such that the open time is between 30 and 120 minutes. The present invention provides particular uses in construction of walls, flooring, and roofing, especially lightweight prefabricated panels intended to be used as structural, insulating or cladding elements.
IMPROVED GEOPOLYMER CEMENT
The present invention provides a geopolymer cement, comprising: a geopolymer binder; and a setting control composition comprising: a viscosity control agent, a polymeric binder, and a retarding additive. The invention also relates to a geopolymer concrete comprising the geopolymer cement of the invention and aggregate material. The invention further relates to a method for controlling open time in a geopolymer composition, wherein a sufficient quantity of the setting control composition is added such that the open time is between 30 and 120 minutes. The present invention provides particular uses in construction of walls, flooring, and roofing, especially lightweight prefabricated panels intended to be used as structural, insulating or cladding elements.