C04B2237/341

Manufacturing method for a member for a semiconductor manufacturing device and member for a semiconductor manufacturing device

In a manufacturing method for a member for a semiconductor manufacturing device, a metal terminal and a ceramic member are joined by using a paste that contains a resin and a metal particle(s), and a metal fine particle(s) that has/have a particle size(s) of 100 nm or less in the metal particle(s) account(s) for 1% by mass or more of 100% by mass of the metal particle(s). A member for a semiconductor manufacturing device includes a metal terminal, a ceramic member, and a joining part that connects the metal terminal and the ceramic member. The joining part contains a metal particle(s).

POROUS FLOW RESTRICTOR AND METHODS OF MANUFACTURE THEREOF
20230160404 · 2023-05-25 ·

Disclosed herein is a dual density disc comprising a dense outer tube comprising a metal oxide having a purity of greater than 92%; and a porous core comprising a metal oxide of a lower density than a density of the dense outer tube; wherein the porous core has a metal oxide purity of greater than 99%; where the dense outer tube has an inner tapered surface.

High optical power light conversion device using a phosphor element with solder attachment

A light generator comprises a light conversion device and a light source arranged to apply a light beam to the light conversion element. The light conversion device includes an optoceramic or other solid phosphor element comprising one or more phosphors embedded in a ceramic, glass, or other host, a metal heat sink, and a solder bond attaching the optoceramic phosphor element to the metal heat sink. The optoceramic phosphor element does not undergo cracking in response to the light source applying a light beam of beam energy effective to heat the optoceramic phosphor element to the phosphor quenching point.

THREE-DIMENSIONAL SHAPED ARTICLE PRODUCTION METHOD
20230111896 · 2023-04-13 ·

A three-dimensional shaped article production method for producing a three-dimensional shaped article by stacking layers to form a stacked body includes a first layer formation step of forming a first layer on a support by supplying a first composition containing first particles and a binder, a second layer formation step of forming a second layer composed of one layer or a plurality of layers on the first layer by supplying a second composition containing second particles and a binder, and a separation step of separating the second layer from the support through the first layer, wherein after the separation step, a sintering step of sintering the second layer is performed.

Thermal Insulation
20230108233 · 2023-04-06 · ·

The present invention relates to inorganic fibres having a composition comprising: 61.0 to 70.8 wt % SiO.sub.2; 28.0 to 39.0 wt % CaO; 0.10 to 0.85 wt % MgO other components, if any, providing the balance up to 100 wt %,

The sum of SiO.sub.2 and CaO is greater than or equal to 98.8 wt % and the other components comprise less than 0.70 wt % Al.sub.2O.sub.3, if any.

HIGH TEMPERATURE COMPOSITES AND METHODS FOR PREPARING HIGH TEMPERATURE COMPOSITES

A method for making a carbon carbon, carbon ceramic matrix, or carbon silica composite, comprising melt processing a resin comprising a polyaryletherketone (PAEK) and at least one reinforcing additive to make a precursor part, pyrolyzing the precursor part to make a pyrolyzed part, infusing a liquid second resin into the pyrolyzed part to make an infused part, and pyrolyzing the infused part. Other methods comprise processing aligned reinforcing additives and a resin comprising a PAEK to make an aligned reinforcing additives PAEK, aligned 1-2 dimensional flake material, or aligned 1-2 dimensional platelet material, to create a fabric, prepreg or tape comprising the aligned reinforcing additives and impregnated PAEK. Other methods comprise impregnating continuous fiber tape or fabric with a resin comprising PAEK and at least one reinforcing additive or co-weaving a continuous fiber or fabric with a PAEK fiber comprising PAEK and at least one reinforcing additive.

JOINT SURFACE COATINGS FOR CERAMIC COMPONENTS
20170368803 · 2017-12-28 ·

An example article may include a component, a substrate including a first ceramic, a joining layer between the component and the substrate, and a joint surface coating between the substrate and the joining layer. The joint surface coating may include a diffusion barrier layer including a second ceramic material, and a compliance layer including at least one of a metal or a metalloid. An example technique may include holding a first joining surface of a coated component adjacent a second joining surface of a second component. The example technique may further include heating at least one of the coated component, the second component, and a braze material, and brazing the coated component by allowing the braze material to flow in a region between the first joining surface and the second joining surface.

Electronic component

An electronic component that has fewer cracks during production is provided. The electronic component includes an outer electrode on a multilayer body, which includes an inner glass layer, a magnetic material layer on top and bottom surfaces of the inner glass layer, and an outer glass layer on top and bottom surfaces of the magnetic material layer. The insulating layers of the inner glass layer and the outer glass layers contain a dielectric glass material that contains a glass material containing at least K, B, and Si, quartz, and alumina. The glass material content of each insulating layer of the inner glass layer ranges from approximately 60%-65% by weight, the quartz content of each insulating layer of the inner glass layer ranges from approximately 34%-37% by weight, and the alumina content of each insulating layer of the inner glass layer ranges from approximately 0.5%-4% by weight.

JOINING MATERIAL WITH SILICON CARBIDE PARTICLES AND REACTIVE ADDITIVES

In some examples, a method including forming a layer of a slurry composition between a first ceramic or CMC part and a second ceramic or CMC part. The slurry composition includes a carrier material; and a plurality of solid particles in the carrier material. The plurality of solid particles includes first silicon carbide (SiC) particles defining a first average particle size, second SiC particles defining a second average particles size that is less than the first average particles size, and reactive additive particles. The method includes heating the layer of slurry composition to react the plurality of reactive additive particles to fuse the plurality of first SiC particles and the plurality of second SiC particles together with the reactive additive particles, wherein the fused layer of the slurry composition forms a joint layer that joins the first ceramic or CMC part to the second ceramic or CMC part.

Method for manufacturing optical element and optical element

A method for manufacturing an optical element is a method for manufacturing an optical element in which laser light is transmitted, reciprocated, or reflected, and the method includes a first step of obtaining a bonded element formed by subjecting a first element part and a second element part, both being transparent to laser light, to surface activated bonding with a non-crystalline layer interposed therebetween; and after the first step, a second step of crystallizing at least a portion of the non-crystalline layer by raising the temperature of the bonded element. In the second step, the temperature of the bonded element is raised to a predetermined temperature that is lower than the melting points of the first element part and the second element part.