C09J123/04

AQUEOUS DISPERSION AND LAMINATE
20220411675 · 2022-12-29 ·

An object of the present invention is to provide an aqueous dispersion with which a coating film having small dynamic frictional resistance can be formed immediately after coating. The present invention includes an aqueous dispersion containing a polyolefin (A), as unsaturated carboxylic acid polymer (B), an amide-based wax (C), and water.

AQUEOUS DISPERSION AND LAMINATE
20220411675 · 2022-12-29 ·

An object of the present invention is to provide an aqueous dispersion with which a coating film having small dynamic frictional resistance can be formed immediately after coating. The present invention includes an aqueous dispersion containing a polyolefin (A), as unsaturated carboxylic acid polymer (B), an amide-based wax (C), and water.

Protective film

A protective film 10 of the present invention includes a base material layer and a pressure sensitive adhesive layer, and is used by being attached to a resin substrate 21 at the time of performing heat bending on the resin substrate 21. The pressure sensitive adhesive layer contains a polyolefin having a melting point of lower than 125° C. The base material layer has a first layer which contains a polyolefin having a melting point of 150° C. or higher, and a second layer which contains an adhesive resin. In a case of heating the protective film 100 having such a configuration, in a state of being interposed between two attaching substrates which are formed of polycarbonate, at 145° C. for 30 minutes, peeling off one attaching substrate on the side of the pressure sensitive adhesive layer at 25° C., and then viewing a surface of the one attaching substrate in a plan view, a residual ratio of an area where the pressure sensitive adhesive layer remains is 5% or less.

Protective film

A protective film 10 of the present invention includes a base material layer and a pressure sensitive adhesive layer, and is used by being attached to a resin substrate 21 at the time of performing heat bending on the resin substrate 21. The pressure sensitive adhesive layer contains a polyolefin having a melting point of lower than 125° C. The base material layer has a first layer which contains a polyolefin having a melting point of 150° C. or higher, and a second layer which contains an adhesive resin. In a case of heating the protective film 100 having such a configuration, in a state of being interposed between two attaching substrates which are formed of polycarbonate, at 145° C. for 30 minutes, peeling off one attaching substrate on the side of the pressure sensitive adhesive layer at 25° C., and then viewing a surface of the one attaching substrate in a plan view, a residual ratio of an area where the pressure sensitive adhesive layer remains is 5% or less.

Protective film

A protective film 10 of the present invention includes a base material layer and a pressure sensitive adhesive layer, and is used by being attached to a resin substrate 21 at the time of performing heat bending on the resin substrate 21. The pressure sensitive adhesive layer contains a polyolefin having a melting point of lower than 125° C. The base material layer has a first layer which contains a polyolefin having a melting point of 150° C. or higher, and a second layer which contains an adhesive resin. In a case of heating the protective film 100 having such a configuration, in a state of being interposed between two attaching substrates which are formed of polycarbonate, at 145° C. for 30 minutes, peeling off one attaching substrate on the side of the pressure sensitive adhesive layer at 25° C., and then viewing a surface of the one attaching substrate in a plan view, a residual ratio of an area where the pressure sensitive adhesive layer remains is 5% or less.

Protective film

A protective film of the present invention is used at the time of performing heat bending on the resin substrate, and includes a base material layer and a pressure sensitive adhesive layer adhered to a resin substrate, in which the base material layer includes a first layer which is positioned on an opposite side of the pressure sensitive adhesive layer and has a melting point of 150° C. or higher, and includes a second layer which is positioned on a pressure sensitive adhesive layer side and has a melting point of lower than 150° C., the pressure sensitive adhesive layer has a melting point of lower than 150° C., and MFR of a thermoplastic resin contained in the second layer, which is measured in conformity with JIS K7210, is in a range of 0.5 g/10 min to 4.0 g/10 min.

Protective film

A protective film of the present invention is used at the time of performing heat bending on the resin substrate, and includes a base material layer and a pressure sensitive adhesive layer adhered to a resin substrate, in which the base material layer includes a first layer which is positioned on an opposite side of the pressure sensitive adhesive layer and has a melting point of 150° C. or higher, and includes a second layer which is positioned on a pressure sensitive adhesive layer side and has a melting point of lower than 150° C., the pressure sensitive adhesive layer has a melting point of lower than 150° C., and MFR of a thermoplastic resin contained in the second layer, which is measured in conformity with JIS K7210, is in a range of 0.5 g/10 min to 4.0 g/10 min.

Protective film

A protective film of the present invention is used at the time of performing heat bending on the resin substrate, and includes a base material layer and a pressure sensitive adhesive layer adhered to a resin substrate, in which the base material layer includes a first layer which is positioned on an opposite side of the pressure sensitive adhesive layer and has a melting point of 150° C. or higher, and includes a second layer which is positioned on a pressure sensitive adhesive layer side and has a melting point of lower than 150° C., the pressure sensitive adhesive layer has a melting point of lower than 150° C., and MFR of a thermoplastic resin contained in the second layer, which is measured in conformity with JIS K7210, is in a range of 0.5 g/10 min to 4.0 g/10 min.

Waterproof corrugated paper, manufacturing method thereof, manufacturing apparatus thereof, and usage thereof

A waterproof corrugated paper includes at least one stone paper medium and at least one stone liner paper, wherein the at least one stone paper medium includes a first fluting surface. A stone glue is utilized to adhere the at least one stone liner paper and several wave crests of the first fluting surface. The stone glue includes a linear polyolefin plastic material and an inorganic material. The linear polyolefin plastic material is 30 wt %-70 wt % based on the stone glue, and the inorganic material is 30 wt %-70 wt % based on the stone glue. The waterproof corrugated paper provided by the present invention is waterproof and frost-resistant, which is adapted to package cooled or frozen food. A manufacturing method, a manufacturing apparatus, and a usage of the waterproof corrugated paper are also provided in the present invention.

Adhesive resin composition, film for fluorine resin adhesion, laminate, and method for producing laminate

The present invention provides an adhesive resin composition that is used for adhesion of a fluorine-based resin and is aimed at adhesion between fluorine-based resins or between a fluorine-based resin and a material other than a fluorine-based resin. More specifically, the present invention relates to an adhesive resin composition for use in adhesion of a fluorine-based resin, the composition including a polyethylene-based resin, an elastomer component, and a component having an epoxy group and a vinyl group, wherein a content of the polyethylene-based resin is 55 parts by mass or more and 90 parts by mass or less, a content of the elastomer component is 10 parts by mass or more and 45 parts by mass or less, the elastomer component and the component having an epoxy group and a vinyl group have a common repetition unit, and a content of the component having an epoxy group and a vinyl group based on a total amount of 100 parts by mass of the polyethylene-based resin and the elastomer component is 0.1 parts by mass or more and 1.5 parts by mass or less.