Patent classifications
C23C14/352
OPTICAL DEVICE AND MANUFACTURING METHOD THEREFOR
An optical device includes, in sequence, a surface formed of a metal oxide, a samarium oxide-containing layer in contact with the surface formed of a metal oxide, and a magnesium fluoride-containing layer in contact with the samarium oxide-containing layer so as to suppress optical absorption resulting from high-rate sputter deposition of a magnesium fluoride-containing layer on a surface formed of a metal oxide.
METHOD OF DEPOSITING A MATERIAL
A method of manufacturing an electronic component including a substrate is provided. The method includes generating a plasma remote from a sputter target, generating sputtered material from the sputter target using the plasma, and depositing the sputtered material on a substrate as a crystalline layer.
COATINGS OF NON-PLANAR SUBSTRATES AND METHODS FOR THE PRODUCTION THEREOF
A coated article is described herein that may comprise a substrate and an optical coating. The substrate may have a major surface comprising a first portion and a second portion. A first direction that is normal to the first portion of the major surface may not be equal to a second direction that is normal to the second portion of the major surface. The optical coating may be disposed on at least the first portion and the second portion of the major surface. The coated article may exhibit at the first portion of the substrate and at the second portion of the substrate hardness of about 8 GPa or greater at an indentation depth of about 50 nm or greater as measured on the anti-reflective surface by a Berkovich Indenter Hardness Test.
COATED ARTICLES WITH OPTICAL COATINGS HAVING RESIDUAL COMPRESSIVE STRESS
Disclosed herein are coated articles which may include a substrate and an optical coating that includes one or more layers of deposited material. At least a portion of the optical coating may include a residual compressive stress of more than 100 MPa. The coated article may include a strain-to-failure of 0.4% or more as measured by a Ring-on-Ring Tensile Testing Procedure. The optical coating may include a maximum hardness of 8 GPa or more and an average photopic transmission of 50% or greater.
LOW-E MATERIAL COMPRISING A THICK LAYER BASED ON SILICON OXIDE
A material includes a transparent substrate coated with a stack including at least one functional metal layer based on silver and at least two dielectric coatings, each dielectric coating including at least one dielectric layer, in such a way that each functional metal layer is positioned between two dielectric coatings, wherein the stack includes a layer based on silicon oxide having a thickness of greater than or equal to 12 nm located directly in contact with the substrate.
Electrically and Magnetically Enhanced Ionized Physical Vapor Deposition Unbalanced Sputtering Source
An electrically and magnetically enhanced ionized physical vapor deposition (I-PVD) magnetron apparatus and method is provided for sputtering material from a cathode target on a substrate, and in particular, for sputtering ceramic and diamond-like coatings. The electrically and magnetically enhanced magnetron sputtering source has unbalanced magnetic fields that couple the cathode target and additional electrode together. The additional electrode is electrically isolated from ground and connected to a power supply that can generate positive, negative, or bipolar high frequency voltages, and is preferably a radio frequency (RF) power supply. RF discharge near the additional electrode increases plasma density and a degree of ionization of sputtered material atoms.
TiCN having reduced growth defects by means of HiPIMS
A method for applying a coating having at least one TiCN layer to a surface of a substrate to be coated by means of high power impulse magnetron sputtering (HIPIMS), wherein, to deposit the at least one TiCN layer, at least one Ti target is used as the Ti source for producing the TiCN layer, said target being sputtered in a reactive atmosphere by means of a HIPIMS process in a coating chamber, wherein the reactive atmosphere comprises at least one inert gas; preferably argon, and at least nitrogen gas as the reactive gas, wherein: the reactive atmosphere additionally contains, as a second reactive gas, a gas containing carbon, preferably CH4, used as the source of carbon to produce the TiCN layer wherein, while depositing the TiCN layer, a bipolar bias voltage is applied to the substrate to be coated, or at least one graphite target is used as the source of carbon for producing the TiCN layer, said target being used for sputtering in the coating chamber using a HIPIMS process with the reactive atmosphere having only nitrogen gas as the reactive gas, wherein the Ti targets are preferably operated by means of a first power supply device or a first power supply unit and the graphite targets are operated with pulsed power by means of a second power supply device or a second power supply unit.
Physical vapor deposition system and processes
A physical vapor deposition (PVD) chamber and a method of operation thereof are disclosed. Chambers and methods are described that provide a chamber comprising an upper shield with two holes that are positioned to permit alternate sputtering from two targets.
METHOD OF DEPOSITING MATERIAL ON A SUBSTRATE
A method of depositing a material on a substrate is provided. The method includes generating a plasma remote from one or more sputter targets suitable for plasma sputtering, wherein at least one distinct region of the one or more targets includes an alkali metal, alkaline earth metal, alkali metal containing compound, alkaline earth metal containing compound or a combination thereof; generating sputtered material from the target or targets using the plasma; and depositing the sputtered material on the substrate, the working distance between the target and the substrate being within +/−50% of the theoretical mean free path of the system.
STRUCTURAL COATING AND PREPARATION METHOD AND USE THEREOF
The present disclosure relates to a structural coating and preparation method and use thereof. The structural coating provided in the present disclosure includes a titanium transition layer and platinum-hafnium composite structure layers laminated in sequence on a surface of a substrate; the number of the platinum-hafnium composite structure layer is ≥3; the platinum-hafnium composite structure layer includes a hafnium layer and a platinum layer laminated in sequence.