E01C7/267

SULPHUR ADDITIVE AND SULPHUR MODIFIED BITUMEN

The present disclosure discloses an additive for preparing modified bitumen comprising a) sulphur with a weight percentage in the range of 90-95% with respect to the additive; b) at least two H2S suppressants with a combined weight percentage in the range of 4-7% with respect to the additive; c) bitumen with a weight percentage in the range of 0.5-3% with respect to the additive; and d) at least one smell masking agent in the range of 0.05-1.0% with respect to the additive. The present disclosure provides a convenient process for the preparation of the additive. The present disclosure also reveals a sulphur modified bitumen and a process for preparing the sulphur modified bitumen.

HIGH-GRADE ASPHALT COMPOSITION HAVING WATERPROOF FUNCTION AND CONSTRUCTION METHOD USING THE SAME
20170226343 · 2017-08-10 ·

A high-grade asphalt composition includes 100 parts by weight of asphalt; 40-80 parts by weight of styrene-isoprene-styrene; 20-60 parts by weight of a polymer resin; 10-50 parts by weight of an anti-rutting agent; 2-15 parts by weight of a filler; 5-30 parts by weight of ceramic nanoparticles; 5-10 parts by weight of a binder; 3-15 parts by weight of an antioxidant; 1-10 parts by weight of a stabilizer; 5-20 parts by weight of a fiber; and 2-20 parts by weight of an adhesion promoter. A construction method is provided using the asphalt composition. The present asphalt composition is not easily rutted, aged and/or stripped. At the same time, the present asphalt can prevent water penetration and potholes, can reduce noise, and enable the roads to be paved at low costs.

MODIFIED BITUMEN COMPOSITION AND PROCESS OF PREPARATION THEREOF

The present disclosure relates to a modified bitumen composition comprising: (a) at least two refinery residues; and (b) a sulphur additive comprising: (i) sulphur; (ii) at least one H.sub.2S suppressant; (iii) at least one smell masking agent; and (iv) bitumen, wherein the sulphur and the at least one H.sub.2S suppressant is in the weight ratio range of 4:1 to 100:1. The present disclosure also discloses a process of preparing a modified bitumen composition and a process of preparing an asphalt pavement comprising a modified bitumen composition. Also provided herein use of a modified bitumen composition as an additive for waterproofing and road construction.

High-grade asphalt composition having waterproof function and construction method using the same
10392509 · 2019-08-27 · ·

A high-grade asphalt composition includes 100 parts by weight of asphalt; 40-80 parts by weight of styrene-isoprene-styrene; 20-60 parts by weight of a polymer resin; 10-50 parts by weight of an anti-rutting agent; 2-15 parts by weight of a filler; 5-30 parts by weight of ceramic nanoparticles; 5-10 parts by weight of a binder; 3-15 parts by weight of an antioxidant; 1-10 parts by weight of a stabilizer; 5-20 parts by weight of a fiber; and 2-20 parts by weight of an adhesion promoter. A construction method is provided using the asphalt composition. The present asphalt composition is not easily rutted, aged and/or stripped. At the same time, the present asphalt can prevent water penetration and potholes, can reduce noise, and enable the roads to be paved at low costs.

A SULPHUR ADDITIVE TO SUPPRESS HYDROGEN SULPHIDE EMISSIONS FROM SULPHUR EXTENDED ASPHALT

The present disclosure relates to a sulphur additive to suppress hydrogen sulphide emissions from Sulphur Extended Asphalt. The sulphur additive of the present disclosure comprises 5 sulphur in an amount ranging from 80 to 98 wt % and at least one aluminosilicate in an amount ranging from 2 to 20 wt %. The sulphur additive of the present disclosure suppresses the H2S emission up to acceptable safe limit during the preparation and application of the sulphur extended asphalt at elevated temperature.

Modified bitumen composition and process of preparation thereof

The present disclosure relates to a modified bitumen composition comprising: (a) at least two refinery residues; and (b) a sulphur additive comprising: (i) sulphur; (ii) at least one H.sub.2S suppressant; (iii) at least one smell masking agent; and (iv) bitumen, wherein the sulphur and the at least one H.sub.2S suppressant is in the weight ratio range of 4:1 to 100:1. The present disclosure also discloses a process of preparing a modified bitumen composition and a process of preparing an asphalt pavement comprising a modified bitumen composition. Also provided herein use of a modified bitumen composition as an additive for waterproofing and road construction.