NICKEL-CHROMIUM-IRON ALLOYS WITH IMPROVED RESISTANCE TO STRESS CORROSION CRACKING IN NUCLEAR ENVIRONMENTS
20180010222 · 2018-01-11 ·

A Ni—Cr—Fe alloy with improved resistance to stress corrosion cracking in nuclear environments, the alloy comprising 23-28 wt % Cr, 25-35 wt % Ni, <0.03 wt % C, <0.70 wt % Si, <1.0 wt % Mn, <0.015 wt % S, >0.35 wt % Ti, 0.15-0.45 wt % Al, <0.75 wt % Cu, and balance Fe and incidental impurities. The alloy may be used in steam generator tubing of a nuclear reactor. A method of producing an article includes: providing the alloy as disclosed herein; forming the alloy into the article by cold working the alloy to 20%; and heat treating the article.

Collar supported pressure parts for heat recovery steam generators

Disclosed herein is a heat recovery steam generator system comprising a vestibule comprising a base plate, a roof and side walls; where the base plate is opposedly disposed to the roof; a heat exchanger space through which an exhaust gas stream is charged; where the vestibule is disposed atop a heat exchanger space; and where the vestibule comprises at least one header in fluid communication with a tube bundle; where a portion of the tube bundle is disposed in the heat exchanger space; and a support system for the tube bundle; where the support system comprises a strap that is reversibly attached to the base plate as well as to the roof of the vestibule or to a structural member in the vestibule; and where each tube of the tube bundle contacts a collar that rests on the base plate.

High-temperature reheater anti-friction device

The present invention relates to a high-temperature reheater anti-friction device for anti-friction of metal tubes on a heated surface of a high-temperature reheater adjacent to a soot blower, has a hole-type tube clamp arranged on a metal tube of a heated surface of a high-temperature reheater, an anti-friction box and an anti-friction cover. Compared with the prior art, the present invention has the advantages of reduced maintenance workload of the unit and prolonged service life of the metal tube.

Electroplating repair machine for tack expansion and seal welding region, electroplating repair system, and operating method

Disclosed are an electroplating repair apparatus, an electroplating repair system having the same, and an operating system thereof. The apparatus includes a probe body extending a predefined length in a structure corresponding to an inner diameter part of a tube, an electroplating electrode attached to and surrounding an outer circumferential surface of the probe body, a sealing member attached to opposite end sides of the probe body to seal a target portion to be electroplated, and a solution supply line supplying a solution to the target portion through the inside of the probe body, wherein the apparatus has a structure capable of wholly repairing the inside of the tube including a sealing welding part and an expanded part.

Method for removing large amounts of condensate from an underground vault steam system during startup
11035570 · 2021-06-15 · ·

A method for removing condensate from a steam line during a cold startup is provided, including introducing a dip tube in a substantially vertical orientation within a substantially vertical section of a steam line, wherein the dip tube includes a proximal end and a distil end, immersing the distil end within a volume of condensate, connecting the proximal end to a removal conduit external to the steam line, and removing at least a portion of the condensate through the removal conduit.

Method for operating a steam generation system
11029021 · 2021-06-08 · ·

A method is disclosed for anticipating operation characteristics of a steam generation system, the steam generation system comprising at least one boiler. The method comprises conducting a fuel analysis of a solid fuel and anticipating the at least one operation characteristic of the steam generation system at the time when a specific partial quantity of solid fuel is combusted in the furnace of a boiler of the steam generation system, and further determining at least one adapted setpoint of at least one operation parameter of the steam generation system dependent upon the fuel composition of any specific solid fuel partial quantity so as to counteract and/or remedy changes of the at least one operation characteristic which are caused by the fuel composition of the specific solid fuel partial quantity. The method may be employed to improve operation of a steam generating system when the fuel composition varies.

Heat transfer tube having superhydrophobic surface and method for manufacturing the same

The present disclosure relates to a heat transfer tube comprising nanostructures formed on the surface, and a method for manufacturing the same, and by forming nanostructures on a heat transfer tube surface, a superhydrophobic surface may be obtained under a high temperature environment as well. In addition, superhydrophobicity may be enhanced by further forming a hydrophobic coating layer on the nanostructure-formed heat transfer tube surface. By using a method of forming nanostructures by dipping the heat transfer tube surface, complex shapes may be coated, and therefore, a plurality of assembled heat transfer tubes may be coated, and damages occurring during a process of assembling the heat transfer tube after coating may be prevented.

Protective aluminum oxide surface coatings and low-temperature forming process for high-temperature applications

A method of both coating a substrate with aluminum oxide and infusing the substrate with elemental aluminum is disclosed. In one example, the method includes providing a metal powder/polymer binder slurry, the slurry having a solvent, an organic binder, metal granules and a seed element, wherein the metal granules include Al; dispersing the slurry upon a Cr-containing surface; after dispersing the slurry, exposing the slurry to air and maintaining the temperature of the slurry and substrate below 110 C. to remove at least a portion of the solvent from the slurry; and, in a combined step, both exposing the binder, metal granules and substrate to air and heating the remaining slurry and substrate at a temperature less than or equal to 1000 C. to both diffuse at least a portion of the metal of the metal granules into the substrate and coat the substrate with aluminum oxide.

METHOD FOR REMOVING LARGE AMOUNTS OF CONDENSATE FROM AN UNDERGROUND VAULT STEAM SYSTEM DURING STARTUP
20200056779 · 2020-02-20 ·

A method for removing condensate from a steam line during a cold startup is provided, including introducing a dip tube in a substantially vertical orientation within a substantially vertical section of a steam line, wherein the dip tube includes a proximal end and a distil end, immersing the distil end within a volume of condensate, connecting the proximal end to a removal conduit external to the steam line, and removing at least a portion of the condensate through the removal conduit.

APPARATUS FOR REMOVING LARGE AMOUNTS OF CONDENSATE FROM AN UNDERGROUND VAULT STEAM SYSTEM DURING STARTUP
20200056850 · 2020-02-20 ·

An apparatus for removing condensate from a steam line during a cold startup is provided, including a steam line with a first horizontal section, a vertical section, and a second horizontal section, the first horizontal section, the vertical section including a first centerline, the second horizontal section including, a first elbow, and a second elbow, the first elbow fluidically connected to the first horizontal section and the vertical section, and including an interior surface, the second elbow fluidically connected to the vertical section and the second horizontal section, a permanent flange on an exterior surface of the second elbow, penetrating the exterior surface, and aligned with the first centerline, and a dip tube, and a temporary flange configured to mate with the permanent flange, wherein a distil end of the dip tube is inserted into the permanent flange and positioned parallel to the first centerline.