H01L2224/84416

SEMICONDUCTOR DEVICE
20170250137 · 2017-08-31 ·

According to one embodiment, there is provided a semiconductor device including a first wiring, a semiconductor chip, a first bonding member, having a first melting temperature, located between the first wiring and the semiconductor chip, and a second wiring including a first connection unit and a second connection unit spaced from the first connection unit. A second bonding member having a second melting temperature higher than the first melting temperature is located between the semiconductor chip and the first connection unit. A third wiring is also provided, and a third bonding member having a third melting temperature lower than the second melting temperature is located between the second connection unit and the third wiring.

SEMICONDUCTOR DEVICE
20170250137 · 2017-08-31 ·

According to one embodiment, there is provided a semiconductor device including a first wiring, a semiconductor chip, a first bonding member, having a first melting temperature, located between the first wiring and the semiconductor chip, and a second wiring including a first connection unit and a second connection unit spaced from the first connection unit. A second bonding member having a second melting temperature higher than the first melting temperature is located between the semiconductor chip and the first connection unit. A third wiring is also provided, and a third bonding member having a third melting temperature lower than the second melting temperature is located between the second connection unit and the third wiring.

Metal paste for joints, assembly, production method for assembly, semiconductor device, and production method for semiconductor device

Provided is a metal paste for joints, containing: metal particles; and linear or branched monovalent aliphatic alcohol having 1 to 20 carbon atoms, in which the metal particles include sub-micro copper particles having a volume average particle diameter of 0.12 μm to 0.8 μM.

Metal paste for joints, assembly, production method for assembly, semiconductor device, and production method for semiconductor device

Provided is a metal paste for joints, containing: metal particles; and linear or branched monovalent aliphatic alcohol having 1 to 20 carbon atoms, in which the metal particles include sub-micro copper particles having a volume average particle diameter of 0.12 μm to 0.8 μM.

METAL PASTE FOR JOINTS, ASSEMBLY, PRODUCTION METHOD FOR ASSEMBLY, SEMICONDUCTOR DEVICE, AND PRODUCTION METHOD FOR SEMICONDUCTOR DEVICE

Provided is a metal paste for joints, containing: metal particles; and linear or branched monovalent aliphatic alcohol having 1 to 20 carbon atoms, in which the metal particles include sub-micro copper particles having a volume average particle diameter of 0.12 m to 0.8 M.

METAL PASTE FOR JOINTS, ASSEMBLY, PRODUCTION METHOD FOR ASSEMBLY, SEMICONDUCTOR DEVICE, AND PRODUCTION METHOD FOR SEMICONDUCTOR DEVICE

Provided is a metal paste for joints, containing: metal particles; and linear or branched monovalent aliphatic alcohol having 1 to 20 carbon atoms, in which the metal particles include sub-micro copper particles having a volume average particle diameter of 0.12 m to 0.8 M.

Copper paste for joining, method for producing joined body, and method for producing semiconductor device

Provided is copper paste for joining including metal particles, and a dispersion medium. The metal particles include sub-micro copper particles having a volume-average particle size of 0.12 m to 0.8 m, and micro copper particles having a volume-average particle size of 2 m to 50 m, a sum of the amount of the sub-micro copper particles contained and the amount of the micro copper particles contained is 80% by mass or greater on the basis of a total mass of the metal particles, and the amount of the sub-micro copper particles contained is 30% by mass to 90% by mass on the basis of a sum of a mass of the sub-micro copper particles and a mass of the micro copper particles.

Copper paste for joining, method for producing joined body, and method for producing semiconductor device

Provided is copper paste for joining including metal particles, and a dispersion medium. The metal particles include sub-micro copper particles having a volume-average particle size of 0.12 m to 0.8 m, and micro copper particles having a volume-average particle size of 2 m to 50 m, a sum of the amount of the sub-micro copper particles contained and the amount of the micro copper particles contained is 80% by mass or greater on the basis of a total mass of the metal particles, and the amount of the sub-micro copper particles contained is 30% by mass to 90% by mass on the basis of a sum of a mass of the sub-micro copper particles and a mass of the micro copper particles.

COPPER PASTE FOR JOINING, METHOD FOR PRODUCING JOINED BODY, AND METHOD FOR PRODUCING SEMICONDUCTOR DEVICE

Provided is copper paste for joining including metal particles, and a dispersion medium. The metal particles include sub-micro copper particles having a volume-average particle size of 0.12 m to 0.8 m, and micro copper particles having a volume-average particle size of 2 m to 50 m, a sum of the amount of the sub-micro copper particles contained and the amount of the micro copper particles contained is 80% by mass or greater on the basis of a total mass of the metal particles, and the amount of the sub-micro copper particles contained is 30% by mass to 90% by mass on the basis of a sum of a mass of the sub-micro copper particles and a mass of the micro copper particles.

COPPER PASTE FOR JOINING, METHOD FOR PRODUCING JOINED BODY, AND METHOD FOR PRODUCING SEMICONDUCTOR DEVICE

Provided is copper paste for joining including metal particles, and a dispersion medium. The metal particles include sub-micro copper particles having a volume-average particle size of 0.12 m to 0.8 m, and micro copper particles having a volume-average particle size of 2 m to 50 m, a sum of the amount of the sub-micro copper particles contained and the amount of the micro copper particles contained is 80% by mass or greater on the basis of a total mass of the metal particles, and the amount of the sub-micro copper particles contained is 30% by mass to 90% by mass on the basis of a sum of a mass of the sub-micro copper particles and a mass of the micro copper particles.