Patent classifications
H01L2224/8448
Metal paste for joints, assembly, production method for assembly, semiconductor device, and production method for semiconductor device
Provided is a metal paste for joints, containing: metal particles; and linear or branched monovalent aliphatic alcohol having 1 to 20 carbon atoms, in which the metal particles include sub-micro copper particles having a volume average particle diameter of 0.12 μm to 0.8 μM.
Metal paste for joints, assembly, production method for assembly, semiconductor device, and production method for semiconductor device
Provided is a metal paste for joints, containing: metal particles; and linear or branched monovalent aliphatic alcohol having 1 to 20 carbon atoms, in which the metal particles include sub-micro copper particles having a volume average particle diameter of 0.12 μm to 0.8 μM.
METAL PASTE FOR JOINTS, ASSEMBLY, PRODUCTION METHOD FOR ASSEMBLY, SEMICONDUCTOR DEVICE, AND PRODUCTION METHOD FOR SEMICONDUCTOR DEVICE
Provided is a metal paste for joints, containing: metal particles; and linear or branched monovalent aliphatic alcohol having 1 to 20 carbon atoms, in which the metal particles include sub-micro copper particles having a volume average particle diameter of 0.12 m to 0.8 M.
METAL PASTE FOR JOINTS, ASSEMBLY, PRODUCTION METHOD FOR ASSEMBLY, SEMICONDUCTOR DEVICE, AND PRODUCTION METHOD FOR SEMICONDUCTOR DEVICE
Provided is a metal paste for joints, containing: metal particles; and linear or branched monovalent aliphatic alcohol having 1 to 20 carbon atoms, in which the metal particles include sub-micro copper particles having a volume average particle diameter of 0.12 m to 0.8 M.
Copper paste for joining, method for producing joined body, and method for producing semiconductor device
Provided is copper paste for joining including metal particles, and a dispersion medium. The metal particles include sub-micro copper particles having a volume-average particle size of 0.12 m to 0.8 m, and micro copper particles having a volume-average particle size of 2 m to 50 m, a sum of the amount of the sub-micro copper particles contained and the amount of the micro copper particles contained is 80% by mass or greater on the basis of a total mass of the metal particles, and the amount of the sub-micro copper particles contained is 30% by mass to 90% by mass on the basis of a sum of a mass of the sub-micro copper particles and a mass of the micro copper particles.
Copper paste for joining, method for producing joined body, and method for producing semiconductor device
Provided is copper paste for joining including metal particles, and a dispersion medium. The metal particles include sub-micro copper particles having a volume-average particle size of 0.12 m to 0.8 m, and micro copper particles having a volume-average particle size of 2 m to 50 m, a sum of the amount of the sub-micro copper particles contained and the amount of the micro copper particles contained is 80% by mass or greater on the basis of a total mass of the metal particles, and the amount of the sub-micro copper particles contained is 30% by mass to 90% by mass on the basis of a sum of a mass of the sub-micro copper particles and a mass of the micro copper particles.
COPPER PASTE FOR JOINING, METHOD FOR PRODUCING JOINED BODY, AND METHOD FOR PRODUCING SEMICONDUCTOR DEVICE
Provided is copper paste for joining including metal particles, and a dispersion medium. The metal particles include sub-micro copper particles having a volume-average particle size of 0.12 m to 0.8 m, and micro copper particles having a volume-average particle size of 2 m to 50 m, a sum of the amount of the sub-micro copper particles contained and the amount of the micro copper particles contained is 80% by mass or greater on the basis of a total mass of the metal particles, and the amount of the sub-micro copper particles contained is 30% by mass to 90% by mass on the basis of a sum of a mass of the sub-micro copper particles and a mass of the micro copper particles.
COPPER PASTE FOR JOINING, METHOD FOR PRODUCING JOINED BODY, AND METHOD FOR PRODUCING SEMICONDUCTOR DEVICE
Provided is copper paste for joining including metal particles, and a dispersion medium. The metal particles include sub-micro copper particles having a volume-average particle size of 0.12 m to 0.8 m, and micro copper particles having a volume-average particle size of 2 m to 50 m, a sum of the amount of the sub-micro copper particles contained and the amount of the micro copper particles contained is 80% by mass or greater on the basis of a total mass of the metal particles, and the amount of the sub-micro copper particles contained is 30% by mass to 90% by mass on the basis of a sum of a mass of the sub-micro copper particles and a mass of the micro copper particles.