H01L2224/275

Anisotropically conductive moisture barrier films and electro-optic assemblies containing the same
11782322 · 2023-10-10 · ·

An electro-optic assembly includes a layer of electro-optic material configured to switch optical states upon application of an electric field and an anisotropically conductive layer having one or more moisture-resistive polymers and a conductive material, the moisture-resistive polymer having a WVTR less than 5 g/(m.sup.2*d).

Anisotropically conductive moisture barrier films and electro-optic assemblies containing the same
11782322 · 2023-10-10 · ·

An electro-optic assembly includes a layer of electro-optic material configured to switch optical states upon application of an electric field and an anisotropically conductive layer having one or more moisture-resistive polymers and a conductive material, the moisture-resistive polymer having a WVTR less than 5 g/(m.sup.2*d).

DIELECTRIC AND METALLIC NANOWIRE BOND LAYERS

In some examples, an electronic device comprises a first component having a surface, a second component having a surface, and a bond layer positioned between the surfaces of the first and second components to couple the first and second components to each other. The bond layer includes a set of metallic nanowires and a dielectric portion. The dielectric portion comprises a polymer matrix and dielectric nanoparticles.

COPPER PASTE FOR PRESSURELESS BONDING, BONDED BODY AND SEMICONDUCTOR DEVICE

A copper paste for pressureless bonding is a copper paste for pressureless bonding, containing: metal particles; and a dispersion medium, in which the metal particles include sub-micro copper particles having a volume average particle diameter of greater than or equal to 0.01 μm and less than or equal to 0.8 μm, and micro copper particles having a volume average particle diameter of greater than or equal to 2.0 μm and less than or equal to 50 μm, and the dispersion medium contains a solvent having a boiling point of higher than or equal to 300° C., and a content of the solvent having a boiling point of higher than or equal to 300° C. is greater than or equal to 2 mass % on the basis of a total mass of the copper paste for pressureless bonding.

COPPER PASTE FOR PRESSURELESS BONDING, BONDED BODY AND SEMICONDUCTOR DEVICE

A copper paste for pressureless bonding is a copper paste for pressureless bonding, containing: metal particles; and a dispersion medium, in which the metal particles include sub-micro copper particles having a volume average particle diameter of greater than or equal to 0.01 μm and less than or equal to 0.8 μm, and micro copper particles having a volume average particle diameter of greater than or equal to 2.0 μm and less than or equal to 50 μm, and the dispersion medium contains a solvent having a boiling point of higher than or equal to 300° C., and a content of the solvent having a boiling point of higher than or equal to 300° C. is greater than or equal to 2 mass % on the basis of a total mass of the copper paste for pressureless bonding.

Copper paste for pressureless bonding, bonded body and semiconductor device

A copper paste for pressureless bonding is a copper paste for pressureless bonding, containing: metal particles; and a dispersion medium, in which the metal particles include sub-micro copper particles having a volume average particle diameter of greater than or equal to 0.01 m and less than or equal to 0.8 m, and micro copper particles having a volume average particle diameter of greater than or equal to 2.0 m and less than or equal to 50 m, and the dispersion medium contains a solvent having a boiling point of higher than or equal to 300 C., and a content of the solvent having a boiling point of higher than or equal to 300 C. is greater than or equal to 2 mass % on the basis of a total mass of the copper paste for pressureless bonding.

Copper paste for pressureless bonding, bonded body and semiconductor device

A copper paste for pressureless bonding is a copper paste for pressureless bonding, containing: metal particles; and a dispersion medium, in which the metal particles include sub-micro copper particles having a volume average particle diameter of greater than or equal to 0.01 m and less than or equal to 0.8 m, and micro copper particles having a volume average particle diameter of greater than or equal to 2.0 m and less than or equal to 50 m, and the dispersion medium contains a solvent having a boiling point of higher than or equal to 300 C., and a content of the solvent having a boiling point of higher than or equal to 300 C. is greater than or equal to 2 mass % on the basis of a total mass of the copper paste for pressureless bonding.

DIELECTRIC AND METALLIC NANOWIRE BOND LAYERS

In some examples, an electronic device comprises a first component having a surface, a second component having a surface, and a bond layer positioned between the surfaces of the first and second components to couple the first and second components to each other. The bond layer includes a set of metallic nanowires and a dielectric portion. The dielectric portion comprises a polymer matrix and dielectric nanoparticles.

STRESS COMPENSATION FOR WAFER TO WAFER BONDING

Embodiments herein describe techniques for bonded wafers that includes a first wafer bonded with a second wafer, and a stress compensation layer in contact with the first wafer or the second wafer. The first wafer has a first stress level at a first location, and a second stress level different from the first stress level at a second location. The stress compensation layer includes a first material at a first location of the stress compensation layer that induces a third stress level at the first location of the first wafer, a second material different from the first material at a second location of the stress compensation layer that induces a fourth stress level different from the third stress level at the second location of the first wafer. Other embodiments may be described and/or claimed.

STRESS COMPENSATION FOR WAFER TO WAFER BONDING

Embodiments herein describe techniques for bonded wafers that includes a first wafer bonded with a second wafer, and a stress compensation layer in contact with the first wafer or the second wafer. The first wafer has a first stress level at a first location, and a second stress level different from the first stress level at a second location. The stress compensation layer includes a first material at a first location of the stress compensation layer that induces a third stress level at the first location of the first wafer, a second material different from the first material at a second location of the stress compensation layer that induces a fourth stress level different from the third stress level at the second location of the first wafer. Other embodiments may be described and/or claimed.