H01L21/31645

Enhanced thin film deposition

Methods of producing metal-containing thin films with low impurity contents on a substrate by atomic layer deposition (ALD) are provided. The methods preferably comprise contacting a substrate with alternating and sequential pulses of a metal source chemical, a second source chemical and a deposition enhancing agent. The deposition enhancing agent is preferably selected from the group consisting of hydrocarbons, hydrogen, hydrogen plasma, hydrogen radicals, silanes, germanium compounds, nitrogen compounds, and boron compounds. In some embodiments, the deposition-enhancing agent reacts with halide contaminants in the growing thin film, improving film properties.

High κ gate stack on III-V compound semiconductors

A method of forming a high k gate stack on a surface of a III-V compound semiconductor, such GaAs, is provided. The method includes subjecting a III-V compound semiconductor material to a precleaning process which removes native oxides from a surface of the III-V compound semiconductor material; forming a semiconductor, e.g., amorphous Si, layer in-situ on the cleaned surface of the III-V compound semiconductor material; and forming a dielectric material having a dielectric constant that is greater than silicon dioxide on the semiconducting layer. In some embodiments, the semiconducting layer is partially or completely converted into a layer including at least a surface layer that is comprised of AO.sub.xN.sub.y prior to forming the dielectric material. In accordance with the present invention, A is a semiconducting material, preferably Si, x is 0 to 1, y is 0 to 1 and x and y are both not zero.

Methods of forming a semiconductor device by thermally treating a cleaned surface of a semiconductor substrate in a non-oxidizing ambient

The present disclosure relates to methods for forming a high-k gate dielectric, the methods comprising the steps of providing a semiconductor substrate, cleaning the substrate, performing a thermal treatment, and performing a high-k dielectric material deposition, wherein said thermal treatment step is performed in a non-oxidizing ambient, leading to the formation of a thin interfacial layer between said semiconductor substrate and said high-k dielectric material and wherein the thickness of said thin interfacial layer is less than 10 Å.

Enhanced thin film deposition

Methods of producing metal-containing thin films with low impurity contents on a substrate by atomic layer deposition (ALD) are provided. The methods preferably comprise contacting a substrate with alternating and sequential pulses of a metal source chemical, a second source chemical and a deposition enhancing agent. The deposition enhancing agent is preferably selected from the group consisting of hydrocarbons, hydrogen, hydrogen plasma, hydrogen radicals, silanes, germanium compounds, nitrogen compounds, and boron compounds. In some embodiments, the deposition-enhancing agent reacts with halide contaminants in the growing thin film, improving film properties.

ENHANCED THIN FILM DEPOSITION
20190267231 · 2019-08-29 ·

Methods of producing metal-containing thin films with low impurity contents on a substrate by atomic layer deposition (ALD) are provided. The methods preferably comprise contacting a substrate with alternating and sequential pulses of a metal source chemical, a second source chemical and a deposition enhancing agent. The deposition enhancing agent is preferably selected from the group consisting of hydrocarbons, hydrogen, hydrogen plasma, hydrogen radicals, silanes, germanium compounds, nitrogen compounds, and boron compounds. In some embodiments, the deposition-enhancing agent reacts with halide contaminants in the growing thin film, improving film properties.

Enhanced thin film deposition

Methods of producing metal-containing thin films with low impurity contents on a substrate by atomic layer deposition (ALD) are provided. The methods preferably comprise contacting a substrate with alternating and sequential pulses of a metal source chemical, a second source chemical and a deposition enhancing agent. The deposition enhancing agent is preferably selected from the group consisting of hydrocarbons, hydrogen, hydrogen plasma, hydrogen radicals, silanes, germanium compounds, nitrogen compounds, and boron compounds. In some embodiments, the deposition-enhancing agent reacts with halide contaminants in the growing thin film, improving film properties.

Method of forming dielectric films, new precursors and their use in semiconductor manufacturing

Method of deposition on a substrate of a dielectric film by introducing into a reaction chamber a vapor of a precursor selected from the group consisting of Zr(MeCp)(NMe.sub.2).sub.3, Zr(EtCp)(NMe.sub.2).sub.3, ZrCp(NMe.sub.2).sub.3, Zr(MeCp)(NEtMe).sub.3, Zr(EtCp)(NEtMe).sub.3, ZrCp(NEtMe).sub.3, Zr(MeCp)(NEt.sub.2).sub.3, Zr(EtCp)(NEt.sub.2).sub.3, ZrCp(NEt.sub.2).sub.3, Zr(iPr.sub.2Cp)(NMe.sub.2).sub.3, Zr(tBu.sub.2Cp)(NMe.sub.2).sub.3, Hf(MeCp)(NMe.sub.2).sub.3, Hf(EtCp)(NMe.sub.2).sub.3, HfCp(NMe.sub.2).sub.3, Hf(MeCp)(NEtMe).sub.3, Hf(EtCp)(NEtMe).sub.3, HfCp(NEtMe).sub.3, Hf(MeCp)(NEt.sub.2).sub.3, Hf(EtCp)(NEt.sub.2).sub.3, HfCp(NEt.sub.2).sub.3, Hf(iPr.sub.2Cp)(NMe.sub.2).sub.3, Hf(tBu.sub.2Cp)(NMe.sub.2).sub.3, and mixtures thereof; and depositing the dielectric film on the substrate.

METHOD OF FORMING DIELECTRIC FILMS, NEW PRECURSORS AND THEIR USE IN SEMICONDUCTOR MANUFACTURING

Method of deposition on a substrate of a dielectric film by introducing into a reaction chamber a vapor of a precursor selected from the group consisting of Zr(MeCp)(NMe.sub.2).sub.3, Zr(EtCp)(NMe.sub.2).sub.3, ZrCp(NMe.sub.2).sub.3, Zr(MeCp)(NEtMe).sub.3, Zr(EtCp)(NEtMe).sub.3, ZrCp(NEtMe).sub.3, Zr(MeCp)(NEt.sub.2).sub.3, Zr(EtCp)(NEt.sub.2).sub.3, ZrCp(NEt.sub.2).sub.3, Zr(iPr.sub.2Cp)(NMe.sub.2).sub.3, Zr(tBu.sub.2Cp)(NMe.sub.2).sub.3, Hf(MeCp)(NMe.sub.2).sub.3, Hf(EtCp)(NMe.sub.2).sub.3, HfCp(NMe.sub.2).sub.3, Hf(MeCp)(NEtMe).sub.3, Hf(EtCp)(NEtMe).sub.3, HfCp(NEtMe).sub.3, Hf(MeCp)(NEt.sub.2).sub.3, Hf(EtCp)(NEt.sub.2).sub.3, HfCp(NEt.sub.2).sub.3, Hf(iPr.sub.2Cp)(NMe.sub.2).sub.3, Hf(tBu.sub.2Cp)(NMe.sub.2).sub.3, and mixtures thereof; and depositing the dielectric film on the substrate.

ENHANCED THIN FILM DEPOSITION
20180130666 · 2018-05-10 ·

Methods of producing metal-containing thin films with low impurity contents on a substrate by atomic layer deposition (ALD) are provided. The methods preferably comprise contacting a substrate with alternating and sequential pulses of a metal source chemical, a second source chemical and a deposition enhancing agent. The deposition enhancing agent is preferably selected from the group consisting of hydrocarbons, hydrogen, hydrogen plasma, hydrogen radicals, silanes, germanium compounds, nitrogen compounds, and boron compounds. In some embodiments, the deposition-enhancing agent reacts with halide contaminants in the growing thin film, improving film properties.

Method of manufacturing semiconductor device and substrate processing apparatus

Provided is a method of manufacturing a semiconductor device. The method includes: (a) forming an oxide film having a predetermined thickness on a substrate by alternately repeating: (a-1) forming a layer containing a predetermined element on the substrate by supplying a source gas containing the predetermined element into a process vessel accommodating the substrate and exhausting the source gas from the process vessel; and (a-2) changing the layer containing the predetermined element into an oxide layer by supplying an oxygen-containing gas and an hydrogen-containing gas into the process vessel, wherein inside of the process vessel is under a heated atmosphere having a pressure lower than an atmospheric pressure; and exhausting the oxygen-containing gas and the hydrogen-containing gas from the process vessel; and (b) modifying the oxide film formed on the substrate by supplying the oxygen-containing gas and the hydrogen-containing gas into the process vessel, wherein the inside of the process vessel is under the heated atmosphere having the pressure lower than the atmospheric pressure, and exhausting the oxygen-containing gas and the hydrogen-containing gas from the process vessel.