CONDUCTIVE PILLAR, METHOD FOR MANUFACTURING THE SAME, AND METHOD FOR MANUFACTURING BONDED STRUCTURE
Provided is a method for manufacturing a conductive pillar capable of bonding a substrate and a bonding member with high bonding strength via a bonding layer without employing an electroplating method, and a method for manufacturing a bonded structure by employing this method. A method for manufacturing a conductive pillar 1 includes, in sequence, the steps of forming a resist layer 16 on a substrate 11 provided with an electrode pad 13, the resist layer 16 including an opening portion 16a on the electrode pad 13, forming a thin Cu film 17 by sputtering or evaporating Cu on a surface of the substrate 11 provided with the resist layer 16 including the opening portion 16a, filling the opening portion 16a with a fine particle copper paste 12c, and sintering the fine particle copper paste 12c by heating the substrate 11 filled with the fine particle copper paste 12c.
3D PRINTED INTERCONNECTS AND RESONATORS FOR SEMICONDUCTOR DEVICES
Techniques regarding forming flip chip interconnects are provided. For example, one or more embodiments described herein can comprise a three-dimensionally printed flip chip interconnect that includes an electrically conductive ink material that is compatible with a three-dimensional printing technology. The three-dimensionally printed flip chip interconnect can be located on a metal surface of a semiconductor chip.
3D PRINTED INTERCONNECTS AND RESONATORS FOR SEMICONDUCTOR DEVICES
Techniques regarding forming flip chip interconnects are provided. For example, one or more embodiments described herein can comprise a three-dimensionally printed flip chip interconnect that includes an electrically conductive ink material that is compatible with a three-dimensional printing technology. The three-dimensionally printed flip chip interconnect can be located on a metal surface of a semiconductor chip.
Heterogenous integration for RF, microwave and MM wave systems in photoactive glass substrates
The present invention includes a method for creating a system in a package with integrated lumped element devices and active devices on a single chip/substrate for heterogeneous integration system-on-chip (HiSoC) in photo-definable glass, comprising: masking a design layout comprising one or more electrical passive and active components on or in a photosensitive glass substrate; activating the photosensitive glass substrate, heating and cooling to make the crystalline material to form a glass-crystalline substrate; etching the glass-crystalline substrate; and depositing, growing, or selectively etching a seed layer on a surface of the glass-crystalline substrate on the surface of the photodefinable glass.
Zinc-cobalt barrier for interface in solder bond applications
A microelectronic device has bump bond structures on input/output (I/O) pads. The bump bond structures include copper-containing pillars, a barrier layer including cobalt and zinc on the copper-containing pillars, and tin-containing solder on the barrier layer. The barrier layer includes 0.1 weight percent to 50 weight percent cobalt and an amount of zinc equivalent to a layer of pure zinc 0.05 microns to 0.5 microns thick. A lead frame has a copper-containing member with a similar barrier layer in an area for a solder joint. Methods of forming the microelectronic device are disclosed.
Method of Manufacturing and Passivating a Die
In an embodiment, a method for manufacturing and passivating a die includes providing the die having an active frontside including a protrusion, the protrusion configured for electrically contacting the die, covering a portion of the protrusion by a passivation tape before applying a passivation layer, applying the passivation layer on all sides of the die including the frontside and its protrusion in one single process, except on the portion covered by the passivation tape and detaching the passivation tape from the covered portion of the protrusion after applying the passivation layer to expose the portion of the protrusion which forms an electrical contact area.
Method of Manufacturing and Passivating a Die
In an embodiment, a method for manufacturing and passivating a die includes providing the die having an active frontside including a protrusion, the protrusion configured for electrically contacting the die, covering a portion of the protrusion by a passivation tape before applying a passivation layer, applying the passivation layer on all sides of the die including the frontside and its protrusion in one single process, except on the portion covered by the passivation tape and detaching the passivation tape from the covered portion of the protrusion after applying the passivation layer to expose the portion of the protrusion which forms an electrical contact area.
Method of manufacturing circuit structure
Provided is a circuit structure including a substrate, a pad, a dielectric layer, a conductive layer, an adhesion layer, and a conductive bump. The pad is disposed on the substrate. The dielectric layer is disposed on the substrate and exposes a portion of the pad. The conductive layer contacts the pad and extends from the pad to cover a top surface of the dielectric layer. The adhesion layer is disposed between the dielectric layer and the conductive layer. The conductive bump extends in an upward manner from a top surface of the conductive layer. The conductive bump and the conductive layer are integrally formed. A method of manufacturing the circuit structure is also provided.
Method for producing joined body, and joining material
Provided is a method for producing a joined body, the method including a first step of preparing a laminated body which includes a first member having a metal pillar provided on a surface thereof, a second member having an electrode pad provided on a surface thereof, and a joining material provided between the metal pillar and the electrode pad and containing metal particles and an organic compound, and a second step of heating the laminated body to sinter the joining material at a predetermined sintering temperature, in which the joining material satisfies the condition of the following Formula (I):
(M.sub.1−M.sub.2)/M.sub.1×100≥1.0 (I)
[in Formula (I), M.sub.1 represents a mass of the joining material when a temperature of the joining material reaches the sintering temperature in the second step, and M.sub.2 represents a non-volatile content in the joining material.]
Method for producing joined body, and joining material
Provided is a method for producing a joined body, the method including a first step of preparing a laminated body which includes a first member having a metal pillar provided on a surface thereof, a second member having an electrode pad provided on a surface thereof, and a joining material provided between the metal pillar and the electrode pad and containing metal particles and an organic compound, and a second step of heating the laminated body to sinter the joining material at a predetermined sintering temperature, in which the joining material satisfies the condition of the following Formula (I):
(M.sub.1−M.sub.2)/M.sub.1×100≥1.0 (I)
[in Formula (I), M.sub.1 represents a mass of the joining material when a temperature of the joining material reaches the sintering temperature in the second step, and M.sub.2 represents a non-volatile content in the joining material.]