H01L21/02554
Metal oxide (MO) semiconductor and thin-film transistor and application thereof
The present invention discloses a metal oxide (MO) semiconductor, which is implemented by respectively doping at least an oxide of rare earth element R and an oxide of rare earth element R′ into an indium-containing MO semiconductor to form an In.sub.xM.sub.yR.sub.nR′.sub.mO.sub.z semiconductor. According to the present invention, the extremely high oxygen bond breaking energy in the oxide of rare earth element R is used to effectively control the carrier concentration in the semiconductor, and a charge transportation center can be formed by using the characteristic that the radius of rare earth ions is equivalent to the radius of indium ions, so that the electrical stability of the semiconductor is improved. The present invention further provides a thin-film transistor based on the MO semiconductor and application thereof.
Oxide Semiconductor Sputtering Target And Method Of Fabricating Thin-Film Transistor Using Same
An oxide semiconductor sputtering target used in a sputtering process to deposit an active layer of a TFT. The oxide semiconductor sputtering target is formed from a material based on a composition of In, Sn, Ga, Zn, and O. The material contains gallium oxide, tin oxide, zinc oxide, and indium oxide. The In, Sn, Ga, and Zn contents are in ranges of 60% to 80%, 0.5% to 8%, 5% to 15%, and 10% to 30% by weight with respect to the weight of In+Sn+Ga+Zn, respectively. A method of fabricating a TFT includes depositing an active layer using the oxide semiconductor sputtering target. Such a TFT is used in a liquid crystal display (LCD), an organic light-emitting display, an electroluminescence display, and the like.
Methods for filling a gap feature on a substrate surface and related semiconductor structures
A method for filling a gap feature on a substrate surface is disclosed. The method may include: providing a substrate comprising a non-planar surface including one or more gap features; depositing a metal oxide film over a surface of the one or more gap features by a cyclical deposition process; contacting the metal oxide with an organic ligand vapor; and converting at least a portion of the metal oxide film to a porous material thereby filling the one or more gap features. Semiconductor structures including a metal-organic framework material formed by the methods of the disclosure are also disclosed.
TRANSISTOR, ELECTRONIC DEVICE, AND METHOD FOR MANUFACTURING TRANSISTOR
What is provided is a transistor including a gate electrode, a gate insulating film, a semiconductor film, a source electrode, and a drain electrode, in which the gate insulating film is a laminated film in which a SiO.sub.x film and a SiC.sub.yN.sub.z film are alternately formed, the total number of films constituting the laminated film is 3 or more and 18 or less, and the thickness of each film constituting the laminated film is 25 nm or more and 150 nm or less.
Semiconductor structure and method of forming semiconductor package
The present disclosure provides a semiconductor structure, including a capacitor. The capacitor includes a first electrode and a second electrode respectively electrically connected to a first conductor and a second conductor; and a first dielectric layer between the first electrode and the second electrode. In some embodiments, the first dielectric layer contacts with a sidewall surface of the first conductor. The semiconductor structure further includes a second dielectric layer over and adjacent to the capacitor. A method of forming the semiconductor package is also provided.
Leakage-free implantation-free ETSOI transistors
A semiconductor device includes an extremely thin semiconductor-on-insulator substrate (ETSOI) having a base substrate, a thin semiconductor layer and a buried dielectric therebetween. A device channel is formed in the thin semiconductor layer. Source and drain regions are formed at opposing positions relative to the device channel. The source and drain regions include an n-type material deposited on the buried dielectric within a thickness of the thin semiconductor layer. A gate structure is formed over the device channel.
Coating liquid for forming metal oxide film, oxide film, field-effect transistor, and method for producing the same
A coating liquid for forming a metal oxide film, the coating liquid including: a metal source, which is at least one selected from the group consisting of inorganic salts, oxides, hydroxides, metal complexes, and organic acid salts; at least one alkali selected from the group consisting of organic alkalis and inorganic alkalis; and a solvent.
METHOD FOR FORMING OXIDE SEMICONDUCTOR FILM, SEMICONDUCTOR DEVICE, AND METHOD FOR MANUFACTURING SEMICONDUCTOR DEVICE
The impurity concentration in the oxide semiconductor film is reduced, and a highly reliability can be obtained.
MANUFACTURING METHOD OF SEMICONDUCTOR DEVICE
To provide a method for manufacturing a semiconductor device including an oxide semiconductor film having conductivity, or a method for manufacturing a semiconductor device including an oxide semiconductor film having a light-transmitting property and conductivity. The method for manufacturing a semiconductor device includes the steps of forming an oxide semiconductor film over a first insulating film, performing first heat treatment in an atmosphere where oxygen contained in the oxide semiconductor film is released, and performing second heat treatment in a hydrogen-containing atmosphere, so that an oxide semiconductor film having conductivity is formed.
LOW DEFECT, HIGH MOBILITY THIN FILM TRANSISTORS WITH IN-SITU DOPED METAL OXIDE CHANNEL MATERIAL
Transistors with metal oxide channel material that is in-situ doped for desired charge carrier concentrations. The metal oxide channel material may be deposited by atomic layering of multiple constituent metals with an oxidation of each layer. Such an ALD process may be performed by cyclically depositing a precursor of one of the metals upon a substrate during a deposition phase, and oxidizing the absorbed precursor during an oxidation phase. For a quinary metal oxide, each of three metal precursors may be introduced and oxidized during the ALD process, and charge carrier concentrations may be modulated by further introducing a fourth metal precursor during the ALD process in a manner that disperses this dopant metal within the film at a significantly lower chemical concentration than the other metals.